# US 2026/0308722 A1 · High-strength and high-impact toughness near-beta titanium alloy, and preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0308722 A1
- Document ID: US20260308722A1
- Status: Published application
- Kind: A1
- Application number: 19/455,080
- Filed: 2026-01-21
- Published: 2026-10-08
- Earliest claimed: 2025-01-21
- Assignees: Central South University
- Applicants: Central South University
- Inventors: Libin LIU; Kaige WANG; Ligang ZHANG; Yueyan TIAN
- Web page: https://patentgrep.com/patent/US20260308722A1

## CPC

- C22C 14/00: Alloys based on titanium
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22F 1/183: {of titanium or alloys based thereon}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

Provided are a high-strength and high-impact toughness near-β titanium alloy, and a preparation method and use thereof, belonging to the technical field of titanium alloy. The high-strength and high-impact toughness near-β titanium alloy provided includes chemical elements as follows: in percentage by mass, 3.2-4.5% of Mo, 2.5-4% of Cr, 0.5-1.8% of Fe, and 0.5-3% of Al, with a balance being Ti and unavoidable impurities, a component ratio of which satisfies 9<[Mo]eq<11; where the high-strength and high-impact toughness near-β titanium alloy has a metallographic structure including a coarse α-lamellar structure and a fine α-lamellar structure.

## Claims

### Claim 1

A high-strength and high-impact toughness near-β titanium alloy, comprising chemical elements as follows: in percentage by mass, 3.2-4.5% of Mo, 2.5-4% of Cr, 0.5-1.8% of Fe, and 0.5-3% of Al, with a balance being Ti and unavoidable impurities, wherein
a molybdenum equivalent of the high-strength and high-impact toughness near-β titanium alloy is denoted as [Mo]eq, and the [Mo]eq satisfies 9<[Mo]eq<11;
the [Mo]eq is obtained according to equation I:
[
Mo
]
e
⁢
q
=
1
[
Mo
]
+
1.6
[
Cr
]
+
2
⁢
.90
[
Fe
]
-
1
[
A
⁢
l
]
,
equation
⁢
I
where [Mo], [Cr], [Fe], and [Al] in the equation I respectively represent a mass percentage of each element in the high-strength and high-impact toughness near-β titanium alloy; and
the high-strength and high-impact toughness near-β titanium alloy has a metallographic structure comprising a coarse α-lamellar structure and a fine α-lamellar structure.

### Claim 2 (depends on 1)

The high-strength and high-impact toughness near-β titanium alloy of claim 1, wherein the high-strength and high-impact toughness near-β titanium alloy comprises chemical elements as follows: in percentage by mass, 3.58% of Mo, 2.97% of Cr, 1.06% of Fe, and 1.06% of Al, with the balance being Ti and the unavoidable impurities.

### Claim 3 (depends on 1)

The high-strength and high-impact toughness near-β titanium alloy of claim 1, wherein the high-strength and high-impact toughness near-β titanium alloy comprises chemical elements as follows: in percentage by mass, 3.50% of Mo, 2.97% of Cr, 0.98% of Fe, and 2.01% of Al, with the balance being Ti and the unavoidable impurities.

### Claim 4 (depends on 1)

The high-strength and high-impact toughness near-β titanium alloy of claim 1, wherein the high-strength and high-impact toughness near-β titanium alloy exhibits a tensile strength of greater than 1000 MPa, a yield strength of greater than 900 MPa, an elongation at break of greater than 12%, and an impact toughness of greater than 50 J/cm2.

### Claim 5 (depends on 1)

The high-strength and high-impact toughness near-β titanium alloy of claim 1, wherein the high-strength and high-impact toughness near-β titanium alloy comprises chemical elements as follows: in percentage by mass, 3.5%-4% of Mo, 2.8%-3% of Cr, 0.8%-1.2% of Fe, and 1%-2.1% of Al, with the balance being Ti and the unavoidable impurities.

### Claim 6 (depends on 1)

The high-strength and high-impact toughness near-β titanium alloy of claim 1, wherein the coarse α-lamellar structure has a width of 0.6-1.9 μm, and the fine α-lamellar structure has a width of 0.12-0.35 μm.

### Claim 7 (depends on 1)

A method for preparing the high-strength and high-impact toughness near-β titanium alloy of claim 1, comprising the steps of:
smelting raw materials according to a chemical element composition of the high-strength and high-impact toughness near-β titanium alloy of claim 1 to obtain a titanium alloy ingot;
subjecting the titanium alloy ingot to a heat deformation process to obtain a titanium alloy billet; and
subjecting the titanium alloy billet to heat treatment to obtain the high-strength and high-impact toughness near-β titanium alloy, wherein the heat treatment comprises a first heat preservation, a first cooling, a second heat preservation, and a second cooling performed in sequence, wherein
the first heat preservation is carried out at a temperature of 800-900° C. for 1-4 h; the first cooling is carried out by cooling in a furnace from a temperature for the first heat preservation to a temperature for the second heat preservation; the second heat preservation is carried out at a temperature of 500-600° C. for 4-8 h; and the second cooling is carried out by air cooling.

### Claim 8 (depends on 7)

The method of claim 7, wherein the smelting is performed by vacuum arc smelting, the smelting is performed at a temperature of 2000-2500° C., and the smelting is carried out for 2-6 times.

### Claim 9 (depends on 7)

The method of claim 7, wherein the heat deformation process comprises cogging and hot rolling performed in sequence.

### Claim 10 (depends on 9)

The method of claim 9, wherein the cogging is carried out at a temperature of 1000-1200° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein the hot rolling is carried out at a temperature of 900-1000° C., with a pass deformation of 5-10% and a cumulative deformation of greater than 50%.

### Claim 12 (depends on 7)

The method of claim 7, wherein the high-strength and high-impact toughness near-β titanium alloy comprises chemical elements as follows: in percentage by mass, 3.5%-4% of Mo, 2.8%-3% of Cr, 0.8%-1.2% of Fe, and 1%-2.1% of Al, with the balance being Ti and the unavoidable impurities.

### Claim 13 (depends on 7)

The method of claim 7, wherein the high-strength and high-impact toughness near-β titanium alloy exhibits a tensile strength of greater than 1000 MPa, a yield strength of greater than 900 MPa, an elongation at break of greater than 12%, and an impact toughness of greater than 50 J/cm2.