# US 2026/0308292 A1 · High dart impact and tear films from titanium based prepolymer catalyzed polyethylenes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0308292 A1
- Document ID: US20260308292A1
- Status: Published application
- Kind: A1
- Application number: 19/172,314
- Filed: 2025-04-07
- Published: 2026-10-08
- Earliest claimed: 2025-04-07
- Assignees: Formosa Plastics Corporation, U.S.A.
- Applicants: Formosa Plastics Corporation, USA
- Inventors: Guangxu XU; Zhiming WANG
- Web page: https://patentgrep.com/patent/US20260308292A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- B29C 39/003: {characterised by the choice of material}
- B29C 49/0005: {characterised by the material}
- B29C 49/04: Extrusion blow-moulding
- C08F 2/34: Polymerisation in gaseous state
- C08F 4/022: {Magnesium halide as support anhydrous or hydrated or complexed by means of a Lewis base for Ziegler-type catalysts}
- C08F 4/64: Titanium, zirconium, hafnium or compounds thereof
- B29K 2023/08: {Copolymers of ethylene (B29K2023/16 takes precedence)}
- B29K 2995/0081: Tear strength
- B29K 2995/0089: Impact strength or toughness
- B29L 2007/008: {Wide strips, e.g. films, webs}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A polyethylene film with enhanced physical and mechanical properties, along with a method for its production, is presented. Notably, the film exhibits a 2% secant modulus exceeding 20,000 psi, dart impact resistance greater than 500 g/mil, and machine direction (MD) tear strength above 500 g/mil. The production method involves reacting ethylene with a comonomer in the presence of a Ziegler-Natta (titanium) base prepolymer at temperatures ranging from 75° C. to 95° C. The process operates under an ethylene partial pressure between 90 psia and 125 psia, with a comonomer-to-ethylene ratio of 0.08 to 0.15, enabling the formation of an ethylene-based polymer without the need for additional cocatalysts or antistatic agents in the gas phase polymerization process.

## Claims

### Claim 1

A method for producing a polyethylene film, comprising:
reacting ethylene with a comonomer in the presence of a titanium-based prepolymer at temperatures ranging from about 75° C. to about 95° C., an ethylene partial pressure between about 90 psia and about 125 psia, and a comonomer-to-ethylene ratio of 0.08 to 0.15 to produce an ethylene-based polymer; and
extruding the ethylene-based polymer at conditions sufficient to produce the polyethylene film;
wherein the polyethylene film comprises a 2% secant modulus exceeding about 20,000 psi, a dart impact resistance greater than about 500 g/mil, and a machine direction (MD) tear strength greater than about 500 g/mil.

### Claim 2 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer is produced without additional cocatalysts or antistatic agents.

### Claim 3 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer is produced in a gas phase polymerization process.

### Claim 4 (depends on 1)

The method of claim 1, wherein the extruding step comprises blow film extrusion.

### Claim 5 (depends on 1)

The method of claim 1, wherein the extruding step comprises cast film extrusion.

### Claim 6 (depends on 1)

The method of claim 1, wherein the comonomer comprises 1-hexene.

### Claim 7 (depends on 1)

The method of claim 1, wherein the titanium-based prepolymer comprises particles having a particle size distribution span ((d90−d10)/d50) of below about 1.5.

### Claim 8 (depends on 1)

The method of claim 1, wherein the titanium-based prepolymer comprises a supported Ziegler-Natta catalyst precursor comprising titanium, magnesium, silicon, halogen, and a nitrogen-based electron donor.

### Claim 9 (depends on 1)

The method of claim 1, wherein the titanium-based prepolymer comprises an activator or cocatalyst comprising alkylaluminum.

### Claim 10 (depends on 1)

The method of claim 1, wherein the titanium-based prepolymer comprises ethylene or one or more alpha-olefins in the range of 10 g to about 500 g per mmol titanium.

### Claim 11 (depends on 8)

The method of claim 8, wherein nitrogen-based electron donor is selected from pyridine, 2-methylpyridine, 4-methylpyridine, 2-ethylpyridine, 4-ethylpyridine, 4-tert-butylpyridine, 2-[methylamino]methyl]pyridine, 2,6-dimethylpyridine, 2,6-diisopropylpyridine, 2,6-di-tert-butylpyridine, 2-phenyl-6-propyl-pyridine, 2-methyl-6-phenyl-pyridine, 2, 6-trimethylsilyl-pyridine, 2,6-dimethoxypyridine, 2,6-bis(chloromethyl)-pyridine, 2,2′:6′,2′-terpyridine, 4′-(4-methylphenyl)-2,2′:6′,2″-terpyridine, and 6,6′-dimethyl-2,2′-dipyridyl.

### Claim 12 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer comprises a 35° C. soluble fraction comprising about 15 wt. % to about 35 wt. % of the total resin mass, with a low density below about 0.890, a molecular weight (Mw) greater than about 80,000), and a narrow molecular weight distribution.

### Claim 13 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer, when eluted across temperatures ranging from about 25° C. to about 110° C., exhibits a consistently high molecular weight across all fractions.

### Claim 14 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer exhibits a uniform distribution of short-chain branching across its molecular weight distribution in both the 35° C. soluble and 35° C. insoluble fractions, with an even distribution of comonomers along the polyethylene chains and a distinct absence of low molecular weight species.

### Claim 15 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer exhibits a chemical sequence distribution in both the 35° C. soluble and 35° C. insoluble fractions that follows Bernoullian statistics.

### Claim 16 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer has a Composition Distribution Breadth Index (CDBI) ranging from about 20% to about 35%, and a Solubility Distribution Breadth Index (SDBI) ranging from about 23° C. to about 30° C.

### Claim 17 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer has a Composition Distribution Breadth Index (CDBI) ranging from about 20% to about 30%, and a Solubility Distribution Breadth Index (SDBI) ranging from about 23° C. to about 29° C.

### Claim 18 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer has a molecular weight distribution (Mw/Mn) ranging from about 3.4 to about 3.8, a Mz/Mw ratio ranging from about 2.5 to about 3.8, and a melt flow ratio (MFR), defined as the ratio of I21 to I2, ranging from about 24 to about 28.

### Claim 19 (depends on 1)

The method of claim 1, wherein the ethylene-based polymer has a melting point (Tm) ranging from about 124° C. to about 126° C. and a virgin powder density ranging from about 0.860 to about 0.930.