# US 2026/0308070 A1 · Sintering additives for improved microstructure control

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0308070 A1
- Document ID: US20260308070A1
- Status: Published application
- Kind: A1
- Application number: 19/640,778
- Filed: 2026-04-07
- Published: 2026-10-08
- Earliest claimed: 2025-04-07
- Assignees: UT-Battelle, LLC
- Applicants: UT-Battelle, LLC
- Inventors: Christopher A. HOBBS; James M. KURLEY, III; Rodney D. HUNT
- Web page: https://patentgrep.com/patent/US20260308070A1

## CPC

- C04B 35/5156: {based on rare earth compounds}
- C04B 35/624: Sol-gel processing
- C04B 35/6303: {Inorganic additives}
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- G21C 3/58: Solid reactor fuel {Pellets made of fissile material}
- C04B 2235/32: Metal oxides, mixed metal oxides, or oxide-forming salts thereof, e.g. carbonates, nitrates, (oxy)hydroxides, chlorides
- C04B 2235/3852: Nitrides, e.g. oxynitrides, carbonitrides, oxycarbonitrides, lithium nitride, magnesium nitride
- C04B 2235/443: Nitrates or nitrites
- C04B 2235/444: Halide containing anions, e.g. bromide, iodate, chlorite
- C04B 2235/528: Spheres
- C04B 2235/6567: Treatment time
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- G21C: NUCLEAR REACTORS (fusion reactors, hybrid fission-fusion reactors G21B; nuclear explosives G21J)

## Abstract

A precursor composition, fuel kernel, coated fuel particle, and method for producing uranium nitride nuclear fuel kernels are provided. The precursor composition includes uranyl nitrate, a carbon source, and a sintering additive comprising a salt having an additive cation and an additive anion, where the additive cation includes zirconium, hafnium, gadolinium, or combinations thereof. The precursor composition may be used in a sol-gel process to form gelled microspheres. The microspheres are heated in a nitrogen-containing atmosphere to convert the microspheres to uranium nitride kernels. The kernels may exhibit high density and may be incorporated into coated fuel particles including one or more coating layers. Methods include preparing a uranyl nitrate solution, preparing a feedstock including hexamethylenetetramine, urea, and a carbon source, gelation, and carbothermic reduction-nitridation.

## Claims

### Claim 1

A precursor composition for forming uranium nitride nuclear fuel, the precursor composition comprising:
a uranium source;
a carbon source; and
a sintering additive selected from the group consisting of:
(i) a metal oxide selected from the group consisting of zirconium dioxide, hafnium oxide, gadolinium oxide, and combinations thereof;
(ii) a salt including an additive cation and an additive anion;
wherein the additive cation is selected from the group consisting of zirconium, hafnium, gadolinium, and combinations thereof; and
(iii) combinations of (i) and (ii).

### Claim 2 (depends on 1)

The precursor composition of claim 1,
wherein the sintering additive is a salt, and the additive cation is selected from the group consisting of zirconium, hafnium, and combinations thereof.

### Claim 3 (depends on 2)

The precursor composition of claim 2,
wherein the additive cation is zirconium.

### Claim 4 (depends on 2)

The precursor composition of claim 2,
wherein the additive cation is hafnium.

### Claim 5 (depends on 1)

The precursor composition of claim 1,
wherein the uranium source is selected from the group consisting of uranyl nitrate, uranyl chloride, uranium dioxide, and combinations thereof.

### Claim 6 (depends on 1)

The precursor composition of claim 1,
wherein the uranium source is uranyl nitrate, and the uranyl nitrate is present in an aqueous nitric acid solution.

### Claim 7 (depends on 1)

The precursor composition of claim 1,
wherein the carbon source is provided in a solution comprising hexamethylenetetramine, urea, and distributed carbon.

### Claim 8 (depends on 1)

The precursor composition of claim 1,
wherein the sintering additive is a salt, and the additive cation is present in an amount of 0.5 atomic % to 5 atomic % relative to uranium.

### Claim 9 (depends on 1)

The precursor composition of claim 1,
wherein the carbon source is present in an amount providing a carbon-to-uranium ratio of 1:1 to 3:1.

### Claim 10 (depends on 1)

A uranium nitride nuclear fuel kernel prepared from the precursor composition of claim 1 by carbothermic reduction-nitridation.

### Claim 11 (depends on 10)

The uranium nitride nuclear fuel kernel of claim 10,
wherein the nuclear fuel kernel has a density of at least 12 g/cm3.

### Claim 12 (depends on 10)

A nuclear fuel particle comprising:
the nuclear fuel kernel of claim 10; and
one or more coating layers surrounding the kernel.

### Claim 13

A method of preparing a uranium nitride nuclear fuel kernel, the method comprising:
preparing a uranium source;
preparing a feedstock comprising hexamethylenetetramine, urea, and a carbon source;
combining a sintering additive and the uranium source to form an additive solution;
combining the additive solution and the feedstock to form a gelation broth;
forming droplets of the gelation broth;
gelling the droplets of the gelation broth to form gelled microspheres;
heating the gelled microspheres in a nitrogen-containing atmosphere to convert the gelled microspheres to uranium nitride nuclear fuel;
wherein the sintering additive is selected from the group consisting of:
(i) a metal oxide selected from the group consisting of zirconium dioxide, hafnium oxide, gadolinium oxide, and combinations thereof;
(ii) a salt including an additive cation and an additive anion, wherein the additive cation is selected from the group consisting of zirconium, hafnium, gadolinium, and combinations thereof; and
(iii) combinations of (i) and (ii).

### Claim 14 (depends on 13)

The method of claim 13,
wherein the sintering additive is the salt, and the additive cation is selected from the group consisting of zirconium, hafnium, and combinations thereof.

### Claim 15 (depends on 13)

The method of claim 13,
wherein the sintering additive is the salt, and the additive cation is zirconium.

### Claim 16 (depends on 13)

The method of claim 13,
wherein the sintering additive is the salt, and the additive cation is hafnium.

### Claim 17 (depends on 13)

The method of claim 13,
wherein gelling the droplets of the gelation broth comprises combining the droplets and heated silicone oil.

### Claim 18 (depends on 13)

The method of claim 13,
wherein heating the gelled microspheres is conducted at a temperature between 1400° C. and 2200° C.

### Claim 19 (depends on 13)

The method of claim 13,
wherein heating the gelled microspheres is conducted for 7 to 13 hours.

### Claim 20 (depends on 13)

The method of claim 13, further comprising:
heating the uranium nitride nuclear fuel kernel in argon for 1 hour to 5 hours.