# US 2026/0308061 A1 · Method for producing geopolymer material from silicate- and aluminate-rich waste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0308061 A1
- Document ID: US20260308061A1
- Status: Published application
- Kind: A1
- Application number: 19/171,212
- Filed: 2025-04-05
- Published: 2026-10-08
- Earliest claimed: 2025-04-05
- Inventors: Hau Trung Tran; Nghia Trung Tran
- Web page: https://patentgrep.com/patent/US20260308061A1

## CPC

- C04B 28/006: {containing mineral polymers, e.g. geopolymers of the Davidovits type}
- C04B 12/005: {Geopolymer cements, e.g. reaction products of aluminosilicates with alkali metal hydroxides or silicates}
- C04B 18/08: Flue dust {, i.e. fly ash}
- C04B 18/101: {Burned rice husks or other burned vegetable material}
- C04B 18/141: {Slags}
- C04B 18/165: Ceramic waste
- C04B 2111/00017: {Aspects relating to the protection of the environment}
- C04B 2201/52: High compression strength concretes, i.e. with a compression strength higher than about 55 N/mm2, e.g. reactive powder concrete [RPC]
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A method for producing geopolymer materials from silicate- and aluminate-rich wastes is disclosed. The process includes preparing a dry mixture of industrial and/or agricultural waste, adding an alkaline activator, forming a geopolymer slurry, shaping by casting, pressing, extrusion, or pelletizing, and curing at 60° C. to 250° C. The resulting geopolymer exhibits high compressive strength, low permeability, chemical durability, and potential for CO2 capture and heavy metal immobilization. The product is suitable for use as aggregate, concrete, or precast components in construction and environmental applications.

## Claims

### Claim 1

A method for producing a geopolymer material from silicate- and aluminate-rich waste materials, the method comprising:
(a) preparing a dry mixture comprising:
(i) from 30% to 99% by dry weight of silicate- and aluminate-rich waste materials;
(ii) from 1% to 10% by dry weight of an alkaline activator; and
(iii) the remainder of the dry mixture comprising supplemental materials rich in silica (SiO2) and alumina (Al2O3);
(b) adding from 5% to 60% water by total weight of the geopolymer mixture, wherein:
(i) for shaping by pressing, extrusion, rolling, centrifugal casting, or pelletizing, the water content ranges from 5% to 25%; and
(ii) for shaping by casting, the water content is up to 60%;
(c) dissolving the alkaline activator in water to form an alkaline activator solution;
(d) blending the alkaline activator solution with the dry mixture to form a geopolymer slurry;
(e) shaping the geopolymer slurry using at least one method selected from the group consisting of casting, pressing, extrusion, rolling, centrifugal casting, vibration, and vibro-compaction; and
(f) curing the shaped material by drying at a temperature ranging from 60° C. to 250° C. to complete geopolymerization.

### Claim 2 (depends on 1)

The method of claim 1, wherein the waste materials are selected from the group consisting of: incinerator fly ash, coal fly ash, metallurgical slag, cement kiln dust, rice husk ash, fired clay, biomass ash, ceramic waste, glass waste, mining sludge, and peat ash.

### Claim 3 (depends on 1)

The method of claim 1, wherein supplemental materials are selected from: crushed sand, glass powder, aluminum powder, rice husk ash, metakaolin, red mud, finely ground bauxite ore, basalt dust, and granite powder.

### Claim 4 (depends on 1)

The method of claim 1, wherein the alkaline activator comprises NaOH, KOH, Na2SiO3, K2SiO3, or combinations thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the waste may be used singly or in blends to optimize the SiO2/Al2O3 molar ratio.

### Claim 6 (depends on 1)

The method of claim 1, wherein the slurry is pre-compacted into pellets prior to shaping to improve density and formability.

### Claim 7 (depends on 1)

The method of claim 1, wherein the SiO2/Al2O3 molar ratio is adjusted between 1.5 and 5 for optimal geopolymerization.

### Claim 8 (depends on 1)

The method of claim 1, further comprising adding additives selected from pozzolans, plasticizers, waterproofing agents, strength enhancers, and reinforcing fibers.

### Claim 9 (depends on 1)

The method of claim 1, wherein the slurry is preheated to 60° C.-150° C. before shaping.

### Claim 10 (depends on 1)

The method of claim 1, wherein drying is conducted using electric, gas, infrared, vacuum, autoclave, microwave, solar, or hybrid systems.

### Claim 11 (depends on 1)

The method of claim 1, wherein the resulting geopolymer material absorbs and retains CO2, enhancing strength and lowering emissions.

### Claim 12 (depends on 1)

The method of claim 1, wherein the product is chemically resistant and suitable for marine, civil, and industrial applications.

### Claim 13 (depends on 1)

The method of claim 1, wherein up to 15% BaSO4 is added to enhance radiation shielding for nuclear plants, hospitals, and laboratories.

### Claim 14 (depends on 1)

The method of claim 1, wherein the geopolymer product replaces conventional aggregate in Portland cement concrete.

### Claim 15 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14)

The method according to any one of claims 1 to 14, wherein the final product exhibits properties and functionalities comparable to those of conventional Portland cement concrete.