# US 2026/0307057 A1 · Coral-reef-like bifunctional catalyst for biomass gasification to produce green hydrogen with simultaneous decarbonization, and preparation method and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0307057 A1
- Document ID: US20260307057A1
- Status: Published application
- Kind: A1
- Application number: 19/655,747
- Filed: 2026-04-23
- Published: 2026-10-08
- Earliest claimed: 2025-04-03
- Assignees: Southeast University
- Applicants: Southeast University
- Inventors: Huiyan ZHANG; Qiuxiang LU; Yinhai SU; Rui XIAO
- Web page: https://patentgrep.com/patent/US20260307057A1

## CPC

- B01J 23/78: with alkali- or alkaline earth metals
- B01J 21/10: Magnesium; Oxides or hydroxides thereof
- B01J 23/94: of catalysts comprising metals, oxides or hydroxides of the iron group metals or copper
- B01J 37/0036: {Grinding}
- B01J 37/0201: {Impregnation}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 38/02: Heat treatment
- C10J 3/02: Fixed-bed gasification of lump fuel
- C10J 2300/092: Wood, cellulose
- C10J 2300/0976: as steam
- C10J 2300/0986: Catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10J: PRODUCTION OF PRODUCER GAS, WATER-GAS, SYNTHESIS GAS FROM SOLID CARBONACEOUS MATERIAL, OR MIXTURES CONTAINING THESE GASES (synthesis gas from liquid or gaseous hydrocarbons C01B; underground gasification of minerals E21B43/295); CARBURETTING AIR OR OTHER GASES

## Abstract

A coral-reef-like bifunctional catalyst for biomass gasification to co-produce green hydrogen and achieve decarbonization. Active metal site regulation optimizes the matching between active phases and supports to enhance catalytic activity and stability. The unique coral-reef-like structure builds a confined space for bond cleavage and CO2 conversion. Dual active sites respectively drive directional bond cleavage for high-purity green hydrogen production and in-situ CO2 adsorption and conversion. The catalyst exhibits excellent cyclic stability and couples multiple reaction pathways, realizing efficient preparation of high H2/CO (3.8) syngas and possessing promising application potential.

## Claims

### Claim 1

A preparation method of a coral-reef-like bifunctional catalyst for biomass gasification to produce green hydrogen with simultaneous decarbonization, comprising the following steps:
S1, an aluminum oxide support goes through acid leaching, calcination, and grinding to produce an activated aluminum oxide support; magnesium oxide is calcined and ground to produce an activated magnesium oxide;
S2, the activated aluminum oxide support and the activated magnesium oxide are mixed to produce a composite support;
S3, the composite support is mixed fully with an active phase precursor of iron and an active phase precursor of nickel in water and then dried, calcined, and ground to produce the coral-reef-like bifunctional catalyst.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein in the step S1, the aluminum oxide support is γ-Al2O3; the acid leaching uses a nitric acid solution with a concentration of 0.1 to 2 mol/L and an acid leaching time is 2 to 4 h; a calcination temperature of the aluminum oxide support is 600 to 900° C., and a time is 2 to 4 h; the calcination is carried out in an inert atmosphere.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein in the step S1, a calcination temperature of the magnesium oxide is 700 to 900° C. and a time is 1.5 to 3.5 h; the calcination is carried out in an inert atmosphere.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein in the step S2, in the composite support, a weight ratio of the activated aluminum oxide support to the activated magnesium oxide is 1:4 to 4:1.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein in the step S3, the active phase precursor of iron comprises a soluble iron salt and the active phase precursor of nickel comprises a soluble nickel salt.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein in the step S3, in the active phase precursor of iron and the active phase precursor of nickel, a molar ratio of iron element to nickel element is 1:3 to 3:1.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein in the step S3, the mixing is carried out at a stirring speed of 600 to 900 r/min under a mixing temperature of 60 to 100° C. for a time of 2 to 3 h; the calcination is carried out in an inert atmosphere at a calcination temperature of 700 to 900° C. for a time of 3 to 4 h.

### Claim 8 (depends on 1)

A coral-reef-like bifunctional catalyst for biomass gasification to produce green hydrogen with simultaneous decarbonization, prepared by the preparation method according to claim 1, wherein the coral-reef-like bifunctional catalyst comprises a γ-Al2O3 support with regular tetrahedron structure and an active MgO support for decarbonization; active metals iron and nickel are anchored to oxygen vacancies of the γ-Al2O3 support and loading of the active metals iron and nickel relative to a total weight of the catalyst is 8 wt. % to 10 wt. %.

### Claim 9 (depends on 8)

An application of the coral-reef-like bifunctional catalyst according to claim 8 in preparation of a bio-based hydrogen-rich synthesis gas, wherein a dried biomass feedstock is mixed with the coral-reef-like bifunctional catalyst at a ratio, and pyrolysis reaction is performed with water as gasifying agent to prepare the hydrogen-rich synthesis gas; in the hydrogen-rich synthesis gas, a molar ratio of H2 to CO is 2 to 4.

### Claim 10 (depends on 9)

The application according to claim 9, wherein a deactivated catalyst after use goes through combustion treatment at a combustion treatment temperature of 600 to 800° C. for a time of 30 to 80 min to produce a regenerated catalyst.

### Claim 11 (depends on 8)

The coral-reef-like bifunctional catalyst according to claim 8, wherein in the step S1 of the preparation method, the aluminum oxide support is γ-Al2O3; the acid leaching uses a nitric acid solution with a concentration of 0.1 to 2 mol/L and an acid leaching time is 2 to 4 h; a calcination temperature of the aluminum oxide support is 600 to 900° C., and a time is 2 to 4 h; the calcination is carried out in an inert atmosphere.

### Claim 12 (depends on 8)

The coral-reef-like bifunctional catalyst according to claim 8, wherein in the step S1 of the preparation method, a calcination temperature of the magnesium oxide is 700 to 900° C. and a time is 1.5 to 3.5 h; the calcination is carried out in an inert atmosphere.

### Claim 13 (depends on 8)

The coral-reef-like bifunctional catalyst according to claim 8, wherein in the step S2 of the preparation method, in the composite support, a weight ratio of the activated aluminum oxide support to the activated magnesium oxide is 1:4 to 4:1.

### Claim 14 (depends on 8)

The coral-reef-like bifunctional catalyst according to claim 8, wherein in the step S3 of the preparation method, the active phase precursor of iron comprises a soluble iron salt and the active phase precursor of nickel comprises a soluble nickel salt.

### Claim 15 (depends on 8)

The coral-reef-like bifunctional catalyst according to claim 8, wherein in the step S3 of the preparation method, in the active phase precursor of iron and the active phase precursor of nickel, a molar ratio of iron element to nickel element is 1:3 to 3:1.

### Claim 16 (depends on 8)

The coral-reef-like bifunctional catalyst according to claim 8, wherein in the step S3 of the preparation method, the mixing is carried out at a stirring speed of 600 to 900 r/min under a mixing temperature of 60 to 100° C. for a time of 2 to 3 h; the calcination is carried out in an inert atmosphere at a calcination temperature of 700 to 900° C. for a time of 3 to 4 h.

### Claim 17 (depends on 9)

The application according to claim 9, wherein in the step S1 of the preparation method, the aluminum oxide support is γ-Al2O3; the acid leaching uses a nitric acid solution with a concentration of 0.1 to 2 mol/L and an acid leaching time is 2 to 4 h; a calcination temperature of the aluminum oxide support is 600 to 900° C., and a time is 2 to 4 h; the calcination is carried out in an inert atmosphere.

### Claim 18 (depends on 9)

The application according to claim 9, wherein in the step S1 of the preparation method, a calcination temperature of the magnesium oxide is 700 to 900° C. and a time is 1.5 to 3.5 h; the calcination is carried out in an inert atmosphere.

### Claim 19 (depends on 9)

The application according to claim 9, wherein in the step S2 of the preparation method, in the composite support, a weight ratio of the activated aluminum oxide support to the activated magnesium oxide is 1:4 to 4:1.

### Claim 20 (depends on 9)

The application according to claim 9, wherein in the step S3 of the preparation method, the active phase precursor of iron comprises a soluble iron salt and the active phase precursor of nickel comprises a soluble nickel salt.