# US 2026/0307056 A1 · Catalyst for methane reforming and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0307056 A1
- Document ID: US20260307056A1
- Status: Published application
- Kind: A1
- Application number: 19/478,903
- Filed: 2024-04-02
- Published: 2026-10-08
- Earliest claimed: 2023-04-28
- Assignees: Hanwha Solutions Corporation; Korea Advanced Institute of Science and Technology
- Applicants: Hanwha Solutions Corporation; Korea Advanced Institute of Science and Technology
- Inventors: Junemin BAE; Jeong Hwan CHUN; Minkee CHOI; Yeongmin KIM
- Web page: https://patentgrep.com/patent/US20260307056A1

## CPC

- B01J 23/78: with alkali- or alkaline earth metals
- B01J 35/394: {Metal dispersion value, e.g. percentage or fraction}
- B01J 35/613: {10-100 m2/g}
- B01J 37/10: in the presence of water, e.g. steam
- C01B 3/40: characterised by the catalyst
- C01B 2203/0238: the reforming step being a carbon dioxide reforming step
- C01B 2203/1058: Nickel catalysts
- C01B 2203/1082: Composition of support materials
- C01B 2203/1241: Natural gas or methane
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

The present invention relates to catalyst for a methane reforming reaction and a manufacturing method thereof. More particularly, the objective of the present invention is to provide a highly dispersed nickel catalyst with secured structural stability that may be used in a methane reforming reaction using carbon dioxide, and a manufacturing method thereof, wherein the nickel is highly dispersed and has excellent structural stability during the methane reforming reaction, thereby providing a nickel catalyst that exhibits excellent catalytic performance in a methane reforming reaction using carbon dioxide.

## Claims

### Claim 1

A catalyst for methane reforming comprising nickel (Ni), boron (B), and magnesium (Mg),
and a B content is more than 1 mol parts and less than 35 mol parts based on 100 mol parts of Mg.

### Claim 2 (depends on 1)

The catalyst of claim 1, wherein:
the Mg in the catalyst for methane reforming is present in a form of MgO as a support.

### Claim 3 (depends on 1)

The catalyst of claim 1, wherein:
a Ni content is 2 parts by weight to 10 parts by weight based on 100 parts by weight of the catalyst for methane reforming.

### Claim 4 (depends on 1)

The catalyst of claim 1, wherein:
the catalyst for methane reforming has a BET specific surface area of 10 m2/g to 50 m2/g measured by a nitrogen adsorption method.

### Claim 5 (depends on 1)

The catalyst of claim 1, wherein:
the catalyst for methane reforming has a lattice constant of MgO of 4.1 Å to 4.2 Å as measured by X-ray diffraction analysis.

### Claim 6 (depends on 1)

The catalyst of claim 1, wherein:
wherein the catalyst for methane reforming comprises a Ni—B intermetallic compound structure having a size of 5 nm to 17 nm after 48 hours of methane reforming reaction.

### Claim 7 (depends on 1)

The catalyst of claim 1, wherein:
the catalyst is used for a methane reforming reaction using carbon dioxide.

### Claim 8

A manufacturing method of a catalyst for methane reforming, comprising:
preparing an aqueous solution mixture by mixing MgO, a nickel (Ni) precursor, and boron (B) precursor (step 1);
hydrothermally synthesizing the mixture of step 1 (step 2); and
drying and sintering the hydrothermally synthesized composition of step 2 (step 3);
wherein in step 1, the B precursor is mixed in an amount such that an B content is more than 1 mol parts and less than 35 mol parts based on 100 mol parts of Mg.

### Claim 9 (depends on 8)

The manufacturing method of claim 8, wherein:
in step 1, the Ni precursor is mixed in an amount such that a Ni content is 2 parts of weight to 10 parts of weight based on 100 parts by weight of the catalyst for methane reforming.

### Claim 10 (depends on 8)

The manufacturing method of claim 8, wherein:
the B precursor of step 1 is at least one selected from the group consisting of H3BO3, BI3, BN, BF3, BCl3, B2O3, CB4, BF3·2H2O, BBr3, and LiBH4.

### Claim 11 (depends on 8)

The manufacturing method of claim 8, wherein:
the Ni precursor of step 1 is at least one selected from the group consisting of Ni(CH3COO)2·4H2O), NiCl2, NiCl2·6H2O, Ni(N3)2, NiSO4, (NH4)2Ni(SO4)2·6H2O, NiBr2, NiCO3, NiF2, NiI2, NiC2O4·2H2O and Ni(ClO4)2·6H2O.

### Claim 12 (depends on 8)

The manufacturing method of claim 8, wherein:
the hydrothermal synthesis of step 2 is performed at a temperature of 100° C. to 300° C. for 12 hours to 48 hours.

### Claim 13 (depends on 8)

The manufacturing method of claim 8, wherein:
wherein the drying of step 3 is performed at 50° C. to 150° C. for 2 hours to 24 hours.

### Claim 14 (depends on 8)

The manufacturing method of claim 8, wherein:
wherein the sintering of step 3 is performed at 600° C. to 1000° C. for 2 hours to 6 hours.