# US 2026/0307055 A1 · Copper silicate-based catalyst and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0307055 A1
- Document ID: US20260307055A1
- Status: Published application
- Kind: A1
- Application number: 19/164,451
- Filed: 2025-01-22
- Published: 2026-10-08
- Earliest claimed: 2024-01-23
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Myungji SUH; Tae Yun KIM; Sungshik EOM
- Web page: https://patentgrep.com/patent/US20260307055A1

## CPC

- B01J 23/72: Copper
- B01J 21/08: Silica
- B01J 35/55: Cylinders or rings
- B01J 35/77: Compounds characterised by their crystallite size
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 37/038: {to form slurries or suspensions, e.g. a washcoat}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- C07C 29/141: with hydrogen or hydrogen-containing gases
- C07C 31/20: Dihydroxylic alcohols
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

A copper silicate-based catalyst according to an exemplary embodiment of the present application contains copper and silica, wherein the weight ratio of Cu:Si in the copper silicate-based catalyst is 30:70 to 70:30, and the Cu 2p binding energy of the copper silicate-based catalyst determined by XPS (X-ray photoelectron spectroscopy) analysis is 932 eV to 934 eV.

## Claims

### Claim 1

A copper silicate-based catalyst comprising copper and silica, wherein
a weight ratio of Cu:Si in the copper silicate-based catalyst is 30:70 to 70:30, and
a Cu 2p binding energy of the copper silicate-based catalyst determined by XPS (X-ray photoelectron spectroscopy) analysis is 932 eV to 934 eV.

### Claim 2 (depends on 1)

The copper silicate-based catalyst according to claim 1, wherein a Cu dispersibility of the copper silicate-based catalyst determined by N2O pulse chemisorption analysis is 0.5% to 3%, and a Cu cubic crystallite size is 200 nm or smaller.

### Claim 3 (depends on 1)

The copper silicate-based catalyst according to claim 1, wherein, upon NH3-TPD (temperature-programmed desorption) analysis of the copper silicate-based catalyst, peaks are present in a weak acid site region of 100° C. or higher and lower than 400° C. and a strong acid site region of 400° C. or higher and 700° C. or lower, and a total acid amount is 0.03 mmol to 2.0 mmol.

### Claim 4 (depends on 1)

The copper silicate-based catalyst according to claim 1, wherein the copper silicate-based catalyst has a crushing strength of 40 N or higher.

### Claim 5 (depends on 1)

The copper silicate-based catalyst according to claim 1, wherein the copper silicate-based catalyst is a catalyst extrusion-molded into a cylindrical shape with a diameter of 2 mm to 6 mm and a height of 2 mm to 10 mm.

### Claim 6 (depends on 1)

The copper silicate-based catalyst according to claim 1, wherein the copper silicate-based catalyst is for preparation of neopentyl glycol.

### Claim 7 (depends on 1)

A method for preparing the copper silicate-based catalyst according to claim 1, comprising:
a step of preparing a coprecipitated slurry by adding a silica sol and an alkaline precipitant to an aqueous solution comprising a copper precursor;
a step of aging the coprecipitated slurry at 80° C. to 90° C. for 3 hours or longer, and then obtaining a dried product by filtering and drying the same;
a step of mixing the dried product with a fiber-based binder and an organic compound, and then preparing a catalyst precursor by molding the same; and
a step of drying the catalyst precursor, and then sintering the same at 400° C. to 650° C., wherein
a content of the fiber-based binder is 0.1 wt % or more and less than 15 wt % based on a total weight of the dried product.

### Claim 8 (depends on 7)

The method for preparing the copper silicate-based catalyst according to claim 7, wherein the alkaline precipitant comprises one or more of NH4OH, (NH4)2CO3, NH4HCO3, CH4N2O, NaOH and Na2CO3.

### Claim 9 (depends on 7)

The method for preparing the copper silicate-based catalyst according to claim 7, wherein a content of the organic compound is 0.1 wt % to 50 wt % based on the total weight of the dried product.

### Claim 10 (depends on 7)

The method for preparing the copper silicate-based catalyst according to claim 7, wherein the fiber-based binder comprises one or more of glass fiber, carbon fiber, aramid fiber, alumina fiber, aluminum silicate fiber, silicon carbide fiber and boron fiber.

### Claim 11 (depends on 7)

The method for preparing the copper silicate-based catalyst according to claim 7, wherein the organic compound comprises one or more of polyvinyl alcohol, isopropyl alcohol, ethanol, polyacrylate, polyethylene glycol, glycerin, starch, dextrin, wax, methyl cellulose, carboxymethyl cellulose, hydroxypropyl methyl cellulose, paraffin, lignosulfonate, stearic acid and palmitic acid.

### Claim 12 (depends on 1)

A method for preparing neopentyl glycol, comprising a step of conducting hydrogenation reaction by adding a hydroxypivaldehyde (HPA) solution and hydrogen to a hydrogenation reactor, wherein
the hydrogenation reactor comprises the copper silicate-based catalyst according to claim 1.