# US 2026/0305272 A1 · Silicon-on-insulator substrate including trap-rich layer and methods for making thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0305272 A1
- Document ID: US20260305272A1
- Status: Published application
- Kind: A1
- Application number: 19/539,751
- Filed: 2026-02-13
- Published: 2026-10-01
- Earliest claimed: 2019-10-07
- Assignees: Addison Crockett
- Inventors: Ron Bowman; Mark Franklin
- Web page: https://patentgrep.com/patent/US20260305272A1

## CPC

- H10P 90/1916: {with separation or delamination along an ion implanted layer, e.g. Smart-cut}
- H10D 86/201: {the substrates comprising an insulating layer on a semiconductor body, e.g. SOI (H10D86/40 take precedence)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A silicon-on-insulator substrate includes: (1) a high-resistivity base layer including silicon and a trap-rich region including arsenic diffused within a first side of the high-resistivity base layer, wherein the trap-rich region has a thickness that is in a range of 1 to 10 microns and a trap density that is in a range of 0.8*1010 cm2 eV−1 to 1.2*1010 cm2 eV−1, wherein the high-resistivity base layer has resistivity in a range of 50 to 100 ohm-meters and a thickness in a range of 500 to 700 microns; (2) a silicon dioxide layer positioned on the first side of the high-resistivity base layer and having a thickness that is in a range of 1000 to 5000 angstroms; and (3) a transfer layer positioned on the silicon dioxide layer, wherein the transfer layer comprises a silicon wafer having a thickness that is a range of 500 to 5000 angstroms.

## Claims

### Claim 1

A silicon-on-insulator substrate, comprising:
a layered structure including, in layered order:
(1) a high-resistivity base layer having a first side and a second side opposite the first side,
wherein the high-resistivity base layer comprises
(a) silicon, and
(b) a trap-rich region comprising arsenic diffused within the first side of the high-resistivity base layer, wherein the trap-rich region has
(i) a thickness that is in a range of 1 to 10 microns, and
(ii) a trap density that is in a range of 0.8*1010 cm2 eV−1 to 1.2*1010 cm2 eV−1,
wherein the high-resistivity base layer has
(a) a resistivity in a range of from 50 to 100 ohm-meters, and
(b) a thickness in a range of from 500 to 700 microns;
(2) a silicon dioxide layer positioned on the first side of the high-resistivity base layer,
wherein the silicon dioxide layer has a thickness that is in a range of from 1000 to 5000 angstroms; and
(3) a transfer layer positioned on the silicon dioxide layer,
wherein the transfer layer comprises a silicon wafer, and
wherein the transfer layer has a thickness that is a range of from 500 to angstroms.

### Claim 2 (depends on 1)

The silicon-on-insulator substrate of claim 1, wherein the trap-rich region has a trap density that is in a range of 1010 cm2 eV−1 to 1.2*1010 cm2 eV−1.

### Claim 3 (depends on 1)

The silicon-on-insulator substrate of claim 1, wherein the trap-rich region comprises arsenic interspersed within a crystalline structure of the silicon of the high-resistivity base layer.

### Claim 4 (depends on 1)

The silicon-on-insulator substrate of claim 1, wherein the trap-rich region has a thickness that is in a range of from 4 microns to 7 microns.

### Claim 5 (depends on 1)

The silicon-on-insulator substrate of claim 1, wherein the high-resistivity base layer has a thickness that is in a range of from 550 to 650 microns.

### Claim 6 (depends on 1)

The silicon-on-insulator substrate of claim 1, wherein the silicon dioxide layer has a thickness that is in a range of from 2000 to 4000 angstroms.

### Claim 7 (depends on 1)

The silicon-on-insulator substrate of claim 1, wherein the transfer layer has a thickness that is in a range of from 2000 to 3500 angstroms.

### Claim 8

A method, comprising:
providing a first silicon wafer having a first side and a second side;
applying an arsenic solution to the first side of the first silicon wafer,
wherein the solution is a liquid colloidal solution;
maintaining the first silicon wafer with the arsenic solution on the first side at a controlled temperature for a controlled period of time to result in the arsenic diffused into the first side of the first silicon wafer to produce a trap-rich region,
wherein the controlled time period is in a range of from 5 hours to 20 hours,
wherein the controlled temperature is in a range of from 700 to 1200 degrees Celsius,
wherein a thickness of the trap-rich region is in a range of from 1 to 10 microns, and
wherein the trap-rich region has a trap density that is in a range of 0.8*1010 cm2 eV 1.2*1010 cm2 eV−1;
depositing a silicon dioxide layer on the first side of the first silicon wafer using a high density plasma chemical vapor deposition (HDPCVD) process,
wherein the HDPCVD process uses an inductively-coupled plasma source,
wherein the inductively-coupled plasma source is operated at a power that is in a range of from 65 watts to 225 watts,
wherein the HDPCVD process uses a flow of oxygen gas, a flow of silane gas, and a flow of argon gas,
wherein a flow rate of the flow of oxygen gas is in a range of from 20 to 35 sccm,
wherein a flow rate of the flow of silane gas is in a range of 20 to 35 sccm,
wherein a flow rate of the flow of argon gas in a range of from 20 to 35 sccm,
wherein the HDPCVD process is performed at a pressure that is in a range of from 5 millitorr to 20 millitorr,
wherein the HDPCVD process is performed using a bias power that is in a range of from 0 to 100 watts,
wherein the HDPCVD process is performed with the first silicon wafer held at a temperature that is in a range of from 100 to 250 degrees Celsius,
wherein a deposition rate of the silicon dioxide layer is in a range of from 900 to 1100 angstroms per minute, and
wherein a thickness of the silicon dioxide layer is in a range of from 1500 to 5000 angstroms;
providing a second silicon wafer having a first side and a second side opposite the first side of the second silicon wafer;
introducing a hydrogen implant into the second silicon wafer so as to define a cleave plane,
wherein a thickness of a portion of the second silicon wafer between the first side of the second silicon wafer and the cleave plane is in a range of from 500 to 5000 angstroms; activating the silicon dioxide layer,
wherein the activating step comprises low-pressure plasma-activated bonding at a pressure in a range of from 0.1 to 100 Pa;
contacting the first side of the second silicon wafer to the activated silicon dioxide layer, thereby producing a combined wafer;
annealing the combined wafer,
wherein the annealing is performed at a temperature in a range of from 200 to 400 degrees Celsius for a duration in a range of from one hour to eight hours;
applying a tension to the combined wafer in a direction so as to urge the first silicon wafer and the second silicon wafer apart from one another; and
striking an edge of the second silicon wafer so as to cleave the second silicon wafer at the cleave plane, thereby producing a silicon-on-insulator substrate.

### Claim 9 (depends on 8)

The method of claim 8, wherein the step of applying the arsenic solution to the first side of the first silicon wafer comprises spin-coating the arsenic solution onto the first side of the first silicon wafer.

### Claim 10 (depends on 8)

The method of claim 8, wherein the liquid colloidal solution comprises arsenic-doped glass.

### Claim 11 (depends on 8)

The method of claim 8, wherein the flow rate of the flow of oxygen gas, the flow rate of the flow of silane gas, and the flow rate of the flow of argon gas are the same as one another.

### Claim 12 (depends on 8)

The method of claim 8, wherein the flow rate of the flow of oxygen gas, the flow rate of the flow of silane gas, and the flow rate of the flow of argon gas are selected to control a refractive index of the silicon dioxide layer.

### Claim 13 (depends on 8)

The method of claim 8, wherein the controlled time period is selected to control a charge dissipation of the trap-rich layer.

### Claim 14 (depends on 8)

The method of claim 8, wherein the trap-rich region has a trap density that is in a range of 1010 cm2 eV−1 to 1.2*1010 cm2 eV−1.

### Claim 15 (depends on 8)

The method of claim 8, wherein the step of maintaining the first silicon wafer with the arsenic solution on the first side at a controlled temperature for a controlled period of time produces the arsenic interspersed within a crystalline structure of the silicon of the high-resistivity base layer.

### Claim 16 (depends on 8)

The method of claim 8, wherein the step of maintaining the first silicon wafer with the arsenic solution on the first side at a controlled temperature for a controlled period of time produces the trap-rich region having a thickness that is in a range of from 4 microns to 7 microns.

### Claim 17 (depends on 8)

The method of claim 8, wherein the high-resistivity base layer has a thickness that is in a range of from 550 to 650 microns.

### Claim 18 (depends on 8)

The method of claim 8, wherein the silicon dioxide layer has a thickness that is in a range of from 2000 to 4000 angstroms.

### Claim 19 (depends on 1)

The silicon-on-insulator substrate of claim 1, wherein the thickness of the portion of the second silicon wafer between the first side of the second silicon wafer and the cleave plane is in a range of from 2000 to 3500 angstroms.