# US 2026/0305177 A1 · Lead zirconate titanate (pzt) solution phase diagram and crystal growth near thermodynamic equilibrium

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0305177 A1
- Document ID: US20260305177A1
- Status: Published application
- Kind: A1
- Application number: 19/480,405
- Filed: 2024-05-10
- Published: 2026-10-01
- Earliest claimed: 2023-05-10
- Assignees: Quest Integrity USA, LLC
- Applicants: Quest Integrity USA, LLC
- Inventors: Vincent Fratello; Song Won Ko
- Web page: https://patentgrep.com/patent/US20260305177A1

## CPC

- H10N 30/8554: {Lead-zirconium titanate [PZT] based}
- C30B 7/08: by cooling of the solution
- H10N 30/095: by melting
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

To grow a lead zirconate titanate (PZT) crystal from a system in thermodynamic equilibrium, thermodynamic equilibrium was established, which had not been done previously. Solvent phase diagrams were measured, and the results fit to a model that allows extrapolation to a variety of solvent systems and solute concentrations. Innovative phosphate solvents were developed. In an embodiment, the present disclosure provides methods for growing PZT single crystals from a single-phase solution near the thermodynamic equilibrium with a very low undercooling wherein the solution is in thermodynamic equilibrium with the growing crystal of composition PbZrXTi(1-X)O3 at a saturation temperature TS. In an embodiment, the present disclosure provides methods for achieving a two-phase liquid-solid system in thermodynamic equilibrium wherein the solution is in equilibrium with solid PbZrXTi(1-X)O3 at a temperature T and methods to grow PbZrXTi(1-x)O3 single crystals of the desired composition X from such a system.

## Claims

### Claim 1

(canceled)

### Claim 2

A system comprising:
a solid comprising lead zirconate titanate (PZT) PbZrXTi(1-x)O3 in thermodynamic equilibrium with a high-temperature solution,
wherein
the high-temperature solution is in a state of saturation at a saturation temperature TS,
X in the solid is in a range of 0.30 and 0.65,
an average temperature of the high-temperature solution is constant to within ±3° C.,
a ratio XL=[Zr]L/([Ti]L+[Zr]L) in the high-temperature solution is in a range of 0.06 and 0.15,
the high-temperature solution comprises lead oxide, zirconium oxide (ZrO2), and titanium oxide (TiO2), and
the high-temperature solution does not comprise a fluoride or chloride constituent.

### Claim 3

(canceled)

### Claim 4 (depends on 1)

The system of claim 1, wherein a solvent composition of the high-temperature solution comprises lead oxide and a Lewis acid or Lewis base component selected from the group consisting of B2O3, P2O5, V2O5, MoO3, Li2O, Na2O, K2O, or a combination thereof.

### Claim 5

(canceled)

### Claim 6 (depends on 4)

The system of claim 4, wherein the solvent composition is selected from PbO, Pb3O4, PbO—B2O3, Pb3O4—B2O3, PbO—Li2O, Pb3O4—Li2O, PbO—Li2O—B2O3, Pb3O4—Li2O—B2O3, PbO—Li2O—MoO3, Pb3O4—Li2O—MoO3, PbO—Pb2P2O7, and PbO—PbLiPO4.

### Claim 7

(canceled)

### Claim 8 (depends on 1)

The system of claim 1, wherein the saturation temperature TS is in a range of about 950° C. to about 1150° C.

### Claim 9 (depends on 1)

The system of claim 1, wherein the system is contained in an inert crucible with low solubility in the high-temperature solution at the saturation temperature Ts.

### Claim 10

(canceled)

### Claim 11 (depends on 1)

The system of claim 1, wherein the PbZrXTi(1-X)O3 solid comprises a higher density than the high-temperature solution.

### Claim 12 (depends on 1)

The system of claim 1, wherein the saturation temperature TS is a function of [TiO2]L.

### Claim 13 (depends on 1)

The system of claim 1, wherein the saturation temperature TS is constant, wherein the solidus composition X in the solid PbZrXTi(1-x)O3 is a function of [TiO2]L.

### Claim 14

(canceled)

### Claim 15 (depends on 2)

A method of growing a PbZrXTi(1-x)O3 crystal from the system of claim 2 by isothermal liquid phase transport in a temperature gradient in the high-temperature solution, the method comprising:
a. mixing powders comprising the composition of the two-phase system of claim 2 to form a charge, wherein the composition comprises a sum of the solid comprising an amount of excess PbZrXTi(1-x)O3 components [ZrO2]s, [TiO2]s, and [PbO]s in proportions to form a solid of composition PbZrXTi(1-x)O3 and a liquid composition that is in thermodynamic equilibrium with the solid at a temperature TS;
b. bringing the charge to equilibrium at TS by:
i. heating the charge in a crucible in a vertical furnace to a temperature greater than the saturation temperature TS of the entire charge including the excess PZT; mixing the fully melted system for a time sufficient to achieve thermodynamic equilibrium with all components in solution; and cooling with stirring to an average melt temperature of TS to allow precipitation of the excess PZT to provide a melted two-phase system; or
ii. heating the charge in a crucible in a vertical furnace to an average melt temperature of TS to provide a melted two-phase system; and mixing the melted two-phase system for a time sufficient to achieve thermodynamic equilibrium;
c. establishing a temperature gradient between the system and a growing region;
d. introducing a seed in the growing region;
e. holding the average temperature constant to within ±3° C. during a growing period to provide a grown crystal; and
f. separating the grown crystal from the liquid.

### Claim 16

(canceled)

### Claim 17

(canceled)

### Claim 18 (depends on 15)

The method of growing a PbZrXTi(1-x)O3 crystal according to claim 15, wherein a temperature gradient between a nutrient solid phase and a growing crystal is less than 10° C.

### Claim at position 19

19-23. (canceled)

### Claim 24 (depends on 1, 15)

The method of growing a PbZrXTi(1-x)O3 crystal according to claim 15, wherein the seed comprises platinum, a platinum alloy, gold, a gold alloy, a perovskite comprising an average lattice parameter of 4.07±0.01 at room temperature, or PbZrXTi(1-x)O3 wherein X is the same as in claim 1 within ±0.1.

### Claim at position 21

25-27. (canceled)

### Claim 28 (depends on 15)

The method of growing a PbZrXTi(1-x)O3 crystal according to claim 15, wherein a dopant is incorporated into the solution and the crystal.

### Claim 29 (depends on 28)

The method of claim 28, wherein the dopant is selected from iron, manganese, niobium, or a rare earth.

### Claim 30 (depends on 15)

The method of claim 15, wherein a resultant PbZrXTi(1-x)O3 single crystal of mass greater than 10 g.

### Claim 31 (depends on 30)

The method of claim 30, wherein X is uniform within ±0.02.

### Claim 32 (depends on 15)

A piezoelectric device comprising a PZT single crystal formed according to claim 15.

### Claim 33 (depends on 32)

The piezoelectric device of claim 32, wherein the piezoelectric device is selected from the group consisting of a transducer, a receiver, a sensor, and an actuator.

### Claim 34 (depends on 4)

The system of claim 4, where the Lewis acid or Lewis base is in a cation fraction range of 0 and 0.2.

### Claim 35 (depends on 15)

The method of growing a PbZrXTi(1-x)O3 crystal according to claim 15 wherein a growth technique is selected from:
top seeded solution growth;
isothermal liquid phase transport in a temperature gradient in the high-temperature solution using a cold finger;
traveling heater method; and
traveling solvent floating zone method.