# US 2026/0304636 A1 · Forming a circuit bearing structure with low temperature and pressure during lamination cycle

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0304636 A1
- Document ID: US20260304636A1
- Status: Published application
- Kind: A1
- Application number: 19/478,808
- Filed: 2024-04-29
- Published: 2026-10-01
- Earliest claimed: 2023-04-28
- Assignees: LCP Medical Technologies, Inc.
- Applicants: Lcp Medical Technologies, LLC
- Inventors: James Rathburn
- Web page: https://patentgrep.com/patent/US20260304636A1

## CPC

- H05K 3/0064: {onto a polymeric substrate}
- H05K 1/0313: {Organic insulating material}
- H05K 3/06: the conductive material being removed chemically or electrolytically, e.g. by photo-etch process {(semi-additive methods H05K3/108)}
- H05K 3/4602: {characterized by a special circuit board as base or central core whereon additional circuit layers are built or additional circuit boards are laminated}
- H05K 3/4626: {characterised by the insulating layers or materials (H05K3/4688 takes precedence)}
- H05K 2201/0141: Liquid crystal polymer [LCP]
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

Embodiments for a method of forming a circuit bearing structure are provided. The method includes pre-tacking one or more dielectric bonding sheets to a second substrate including a layer of liquid crystal polymer (LCP). The second substrate is then stacked on a first substrate to form a stack-up. The first substrate includes a layer of LCP and has circuit features standing proud on a first surface thereof. The one or more dielectric bonding sheets are disposed between the second substrate and the first substrate over the circuit features. The stack-up is then laminated with pressure lower than 300 pounds per square inch (psi) and temperature lower than 250 degrees Celsius for at least 90 percent of the time of lamination to cure the one or more dielectric bonding sheets and bond the first substrate to the second substrate.

## Claims

### Claim 1

A method of forming a circuit bearing structure, the method comprising:
providing a first substrate having a first dielectric layer defining a first surface and first circuit features standing proud on the first surface, wherein the first dielectric layer is composed of liquid crystal polymer (LCP);
providing a second substrate having a second dielectric layer, the second dielectric layer composed of LCP;
pre-tacking a first one or more dielectric bonding sheets to the second substrate;
stacking the second substrate on the first substrate to form a first stack-up, such that the first one or more dielectric bonding sheets are disposed between the second substrate and the first substrate and on the first surface of the first substrate over the first circuit features on the first surface; and
laminating the first stack-up with pressure lower than 300 pounds per square inch (psi) and temperature lower than 250 degrees Celsius for at least 90 percent of the time of lamination to cure the first one or more dielectric bonding sheets and bond the first substrate to the second substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein laminating the stack-up forms a third substrate, the method comprising:
forming second circuit features in or on an exposed surface of the second dielectric layer;
providing a fourth substrate having a third dielectric layer, the third dielectric layer composed of LCP;
pre-tacking a second one or more dielectric bonding sheets to the third substrate;
stacking the fourth substrate on the third substrate to form a second stack-up, such that the second one or more dielectric bonding sheets are disposed between the third substrate and the fourth substrate and on the exposed surface of the second dielectric layer of the third substrate over the second circuit features in or on the exposed surface; and
laminating the second stack-up with pressure lower than 300 pounds per square inch (psi) and temperature lower than 250 degrees Celsius for at least 90 percent of the time of lamination to cure the second one or more dielectric bonding sheets and bond the fourth substrate to the third substrate.

### Claim 3 (depends on 1)

The method of claim 1, comprising:
providing a third substrate having a third dielectric layer, the third dielectric layer composed of LCP;
pre-tacking a second one or more dielectric bonding sheets to the third substrate;
wherein stacking including stacking the third substrate on the first substrate along with the second substrate to form the first stack-up, such that the second one or more dielectric bonding sheets are disposed between the third substrate and the first substrate and on a surface of the first substrate opposite the first surface; and
laminating the first stack-up with pressure lower than 300 pounds per square inch (psi) and temperature lower than 250 degrees Celsius for at least 90 percent of the time of lamination to cure the first and second one or more dielectric bonding sheets and bond together the first, second, and third substrates.

### Claim 4 (depends on 1)

The method of claim 1, comprising:
forming second circuit features in or on an exposed surface of the second dielectric layer;
providing a third substrate having a third dielectric layer, the third dielectric layer composed of LCP;
pre-tacking a second one or more dielectric bonding sheets to the third substrate;
wherein stacking including stacking the third substrate on the second substrate after stacking the second substrate on the first substrate to form the first stack-up which includes the first, second, and third substrates, wherein the first one or more dielectric bonding sheets are disposed between the second substrate and the first substrate and on the first surface of the first substrate, wherein the second one or more dielectric bonding sheets are disposed between the third substrate and the fourth substrate and on the exposed surface of the second dielectric layer of the second substrate over the second circuit features in or on the exposed surface; and
laminating the first stack-up with pressure lower than 300 pounds per square inch (psi) and temperature lower than 250 degrees Celsius for at least 90 percent of the time of lamination to cure the first and second one or more dielectric bonding sheets and bond together the first, second, and third substrates.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first dielectric layer is less than 200 microns thick and the one or more dielectric bonding layers are collectively less than 200 microns thick.

### Claim 6

A method of forming a circuit bearing structure, the method comprising:
providing a first substrate having a first dielectric layer defining a first surface and first circuit features standing proud on the first surface, wherein the first dielectric layer is composed of liquid crystal polymer (LCP);
stacking one or more dielectric bonding sheets on the first surface of the first substrate over the first circuit features on the first surface;
laminating the one or more bonding sheets to the substrate with pressure lower than 300 pounds per square inch (psi) and temperature lower than 250 degrees Celsius for at least 90 percent of the time of lamination to cure the one or more dielectric bonding sheets and bond the one or more dielectric bonding sheets to the first substrate, wherein laminating forms a second substrate having a layer of cured bonding sheets, wherein the layer of cured bonding sheets has an exposed surface; and
forming second circuit features in or on the exposed surface of the layer of cured bonding sheets.

### Claim 7 (depends on 6)