# US 2026/0302439 A1 · All solid secondary battery, all solid secondary battery structure and preparation method for all solid secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0302439 A1
- Document ID: US20260302439A1
- Status: Published application
- Kind: A1
- Application number: 19/691,835
- Filed: 2026-05-29
- Published: 2026-10-01
- Earliest claimed: 2021-07-30
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Jeonghoon KIM; Jongdae KIM; Mansoo SHIN; Ikhwan CHO; Youngseok JEONG; Daesik OH
- Web page: https://patentgrep.com/patent/US20260302439A1

## CPC

- H01M 50/124: having a layered structure
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/364: {as mixtures}
- H01M 4/366: {as layered products}
- H01M 4/405: {Alloys based on lithium}
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 10/0562: Solid materials
- H01M 50/119: Metals
- H01M 50/121: Organic material
- H01M 50/133: Thickness
- H01M 50/136: Flexibility or foldability
- H01M 50/204: Racks, modules or packs for multiple batteries or multiple cells
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0068: inorganic
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

An all solid secondary battery, an all solid secondary battery structure, and a method of manufacturing the all solid secondary battery, wherein the all solid secondary battery includes a stack including a positive electrode layer, a negative electrode layer, and a solid electrolyte layer disposed between the positive electrode layer and the negative electrode layer, wherein the positive electrode layer includes a positive electrode current collector and a positive electrode active material layer disposed on one surface or opposite surfaces of the positive electrode current collector, the negative electrode layer includes a negative electrode current collector and a first negative electrode active material layer disposed on the negative electrode current collector, and the first negative electrode active material layer does not contain a solid electrolyte or an amount of the solid electrolyte contained in the first negative electrode active material layer is 3 wt % or less of the total weight of the first negative electrode active material layer; and an exterior casing material for accommodating and sealing the stack, wherein the exterior casing material includes a first exterior casing material disposed on a first surface of the stack adjacent to the negative electrode layer, and a second exterior casing material disposed on the second surface of the stack opposing the first surface, and the first exterior casing material includes a cushioning layer.

## Claims

### Claim 1

An all solid secondary battery, comprising:
a stack including a positive electrode layer, a negative electrode layer, and a solid electrolyte layer disposed between the positive electrode layer and the negative electrode layer; and
an exterior casing material accommodating and sealing the stack,
wherein:
the positive electrode layer includes a positive electrode current collector and a positive electrode active material layer disposed on the positive electrode current collector,
the negative electrode layer includes a negative electrode current collector and a first negative electrode active material layer disposed on the negative electrode current collector,
the exterior casing material includes:
a first exterior casing material disposed on a first surface of the stack adjacent to the negative electrode layer, and
a second exterior casing material disposed on the second surface of the stack opposing the first surface,
the first exterior casing material includes a cushioning layer,
the cushioning layer has a stress relaxation rate of 3% to 25%, the stress relaxation rate being represented by Equation 2,
Stress
⁢
relaxation
⁢
rate
=
[
(
S
⁢
1
-
S
⁢
2
)
/
S
⁢
1
]
×
10.
Equation
⁢
2
SI indicates a first stress measured when a first point is reached by compression by 50% of an initial thickness and then a second point is reached from the first point by additional compression by 13.33% of the initial thickness, and
S2 indicates a second stress measured after 60 seconds lapse from a time of measuring the first stress.

### Claim 2 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein the cushioning layer has a compression elastic modulus of 0.1 MPa to 100 MPa.

### Claim 3 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein the cushioning layer has a deformation rate of 50% to 95% at a load of 10 MPa.

### Claim 4 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein the cushioning layer has a 50% compression force deflection (CFD) according to ASTM D3574 of 0.25 MPa to 0.55 MPa.

### Claim 5 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein the first negative electrode active material layer does not contain a solid electrolyte.

### Claim 6 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein an amount of the solid electrolyte contained in the first negative electrode active material layer is 3 wt % or less of the total weight of the first negative electrode active material layer.

### Claim 7 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein a thickness of the first exterior casing material is 1 μm to 5000 μm, and a thickness of the cushioning layer is 1 μm to 1000 μm.

### Claim 8 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein:
the first exterior casing material further includes at least one selected from a metal layer and a polymer layer,
the polymer layer includes a polymer, and
the polymer has a gas permeability of 10 cc·20·μm/m2·24 h·atm or less.

### Claim 9 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein the second exterior casing material includes at least one selected from a cushioning layer, a metal layer, and a polymer layer.

### Claim 10 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein:
the exterior casing material includes a sealing portion disposed along outer edges of the first exterior casing material and the second exterior casing material, and
the sealing portion further includes either an adhesive layer disposed between the first exterior casing material and the second exterior casing material, or a fusion portion in which the first exterior casing material and the second exterior casing material are fused to each other.

### Claim 11 (depends on 1)

The all solid secondary battery as claimed in claim 1, further comprising an inactive member surrounding a side surface of the positive electrode layer.

### Claim 12 (depends on 11)

The all solid secondary battery as claimed in claim 11, wherein:
the positive electrode layer includes a first positive electrode active material layer and a second positive electrode active material layer respectively disposed on opposite surfaces of the positive electrode current collector,
the solid electrolyte layer includes a first solid electrolyte layer and a second solid electrolyte layer which are in contact with the first positive electrode active material layer and the second positive electrode active material layer, respectively,
the negative electrode layer includes a first negative electrode layer and a second negative electrode layer which are in contact with the first solid electrolyte layer and the second solid electrolyte layer, respectively, and
the inactive member surrounds a side surface of the positive electrode layer, is between the first solid electrolyte layer and the second solid electrolyte layer facing each other, and is separated from the first negative electrode layer and the second negative electrode layer.

### Claim 13 (depends on 11)

The all solid secondary battery as claimed in claim 11, wherein:
the inactive member is a flame retardant inactive member, and the flame retardant inactive member includes a matrix and a filler,
the matrix includes a base material and a reinforcing material.

### Claim 14 (depends on 13)

The all solid secondary battery as claimed in claim 13, wherein:
the base material includes a first fibrous material, the first fibrous material is an insulating material, and the first fibrous material includes at least one selected from pulp fibers, insulating polymer fibers, and ion conductive polymer fibers,
the reinforcing material includes a second fibrous material, the second fibrous material is a flame retardant material, and the second fibrous material includes at least one selected from glass fibers and ceramic fibers.

### Claim 15 (depends on 13)

The all solid secondary battery as claimed in claim 13, wherein:
the filler is a moisture getter, and the filler contains a metal hydroxide, and
the metal hydroxide is at least one selected from Mg(OH)2, Fe(OH)3, Sb(OH)3, Sn(OH)4, TI(OH)3, Zr(OH)4, and Al(OH)3.

### Claim 16 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein:
the solid electrolyte includes a sulfide-based solid electrolyte, the sulfide-based solid electrolyte is one or more selected from Li2S—P2S5, Li2S—P2S5—LiX where X is a halogen element, Li2S—P2S5—Li2O, Li2S—P2S5—Li2O—LiI, Li2S—SiS2, Li2S—SiS2—LiI, Li2S—SiS2—LiBr, Li2S—SiS2—LiCl, Li2S—SiS2—B2S3—LiI, Li2S—SiS2—P2S5—LiI, Li2S—B2S3, Li2S—P2S5—ZmSn where m and n are each a positive number, and Z is one of Ge, Zn, or Ga, Li2S—GeS2, Li2S—SiS2—Li3PO4, Li2S—SiS2-LipMOq, p and q are each a positive number, M is one of P, Si, Ge, B, Al, Ga, In, Li7-xPS6-xClx where 0≤x≤2, Li7-xPS6-xBrx where 0≤x≤2, and Li7-xPS6-xIx where 0≤x≤2,
the sulfide-based solid electrolyte is an Argyrodite-type solid electrolyte including one or more selected from among Li6PS5Cl, Li6PS5Br, and Li6PS5I, and
a density of the Argyrodite-type solid electrolyte is 1.5 g/cc to 2.0 g/cc.

### Claim 17 (depends on 1)

The all solid secondary battery as claimed in claim 1, wherein:
the first negative electrode active material layer includes a first negative electrode active material and a binder,
the first negative electrode active material has a particle shape, and an average particle diameter of the first negative electrode active material is 4 μm or less,
the first negative electrode active material includes at least one selected from a carbon-based negative electrode active material and a metal or metalloid negative electrode active material,
the carbon-based negative electrode active material includes amorphous carbon,
the metal or metalloid negative electrode active material includes at least one selected from the group consisting of gold (Au), platinum (Pt), palladium (Pd), silicon (Si), silver (Ag), aluminum (Al), bismuth (Bi), tin (Sn), and zinc (Zn),
the first negative electrode active material includes a mixture of first particles consisting of amorphous carbon and second particles consisting of metal or metalloid, and
an amount of the second particles is 8 wt % to 60 wt % based on a total weight of the mixture.

### Claim 18 (depends on 1)

The all solid secondary battery as claimed in claim 1, further comprising a second negative electrode active material layer between the negative electrode current collector and the first negative electrode active material layer or between the solid electrolyte layer and the first negative electrode active material layer,
wherein the second negative electrode active material layer is a metal layer including lithium or a lithium alloy.

### Claim 19 (depends on 1)

An all solid secondary battery structure, comprising:
an all solid secondary battery stack including a plurality of all solid secondary batteries stacked in one direction, each of the all solid secondary batteries being the all solid secondary battery of claim 1, and
an end plate disposed on one surface or opposite surfaces of the stack.

### Claim 20

An all solid secondary battery, comprising:
a stack including a positive electrode layer, a negative electrode layer, and a solid electrolyte layer disposed between the positive electrode layer and the negative electrode layer; and
an exterior casing material accommodating and sealing the stack,
wherein:
the positive electrode layer includes a positive electrode current collector and a positive electrode active material layer disposed on one surface or opposite surfaces of the positive electrode current collector,
the negative electrode layer includes a negative electrode current collector and a first negative electrode active material layer disposed on the negative electrode current collector,
the exterior casing material includes:
a first exterior casing material disposed on a first surface of the stack adjacent to the negative electrode layer, and
a second exterior casing material disposed on the second surface of the stack opposing the first surface,
the first exterior casing material includes a cushioning layer,
the cushioning layer has a compression recovery ratio in a thickness direction of 65% to 99%, the compression recovery ratio in the thickness direction being represented by Equation 3,
Compression
⁢
recovery
⁢
ratio
=
AA
⁢
2
/
AA
⁢
1
×
100
⁢
C
.
Equation
⁢
3
AA1 is a third stress measured at a first point which is reached by compression by 50% of an initial thickness, and
AA2 is a fourth stress measured when a second point is reached by additional compression by 13.33% of the initial thickness from the first point, and then, after 60 seconds lapse at the second point, the first point is reached back by a relaxation from the second point.