# US 2026/0302347 A1 · Electrolyte membrane and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0302347 A1
- Document ID: US20260302347A1
- Status: Published application
- Kind: A1
- Application number: 19/566,788
- Filed: 2026-03-13
- Published: 2026-10-01
- Earliest claimed: 2025-03-31
- Assignees: Hon Hai Precision Industry Co., Ltd.; SolidEdge Solution Inc.
- Applicants: Hon Hai Precision Industry Co., Ltd.; SolidEdge Solution Inc.
- Inventors: JING-KAI KAO; TSENG-LUNG CHANG
- Web page: https://patentgrep.com/patent/US20260302347A1

## CPC

- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- H01M 2300/0082: Organic polymers
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

The present invention relates to an electrolyte membrane and a preparation method thereof. The preparation method includes the following steps: mixing a first polymer, an ionic liquid, and an organic solvent to obtain a first solution; adding a solid electrolyte to the first solution to obtain a slurry A; mixing second polymers having different weight average molecular weights to obtain a polymer mixture, and mixing the polymer mixture, the ionic liquid, and the organic solvent to obtain a colloidal liquid B; mixing the slurry A and the colloidal liquid B to obtain an intermediate colloid C; mixing a lithium salt and the ionic liquid with the organic solvent to obtain a composite solution; mixing the intermediate colloid C with the composite solution and stirring to obtain a composite; applying the composite onto a substrate and drying the composite.

## Claims

### Claim 1

A preparation method of an electrolyte membrane, comprising:
mixing a first polymer, an ionic liquid, and an organic solvent to obtain a first solution;
adding solid electrolyte to the first solution to obtain a slurry A;
mixing at least one type of second polymers to obtain a polymer mixture, wherein a weight-average molecular weight of each of the at least one type of second polymers is different from each other; mixing the polymer mixture, the ionic liquid, and the organic solvent to obtain colloid liquid B;
dividing the slurry A into partial batches and adding each of the partial batches of the slurry A to the colloid liquid B to obtain an intermediate colloid C; wherein a mixture of the slurry A and the colloid liquid B is stirred for a period of time after each of the partial batches of the slurry A is added to the colloid liquid B, and a pH of the mixture of the slurry A and the colloid liquid B is maintained to be 6.8 to 7.5;
mixing lithium salt and the ionic liquid with the organic solvent to obtain a composite solution;
mixing the intermediate colloid C with the composite solution to obtain a composite; and
applying the composite onto a substrate and drying the composite to form the electrolyte membrane.

### Claim 2 (depends on 1)

The preparation method of claim 1, wherein the first polymer is selected from a group consisting of polyvinylidene fluoride, poly(vinylidene fluoride-co-hexafluoropropylene), polyvinyl alcohol, polylactic acid, polyethylene glycol, polymethyl methacrylate, propylene glycol methyl ether acetate, and polyacrylic acid, and any combination thereof.

### Claim 3 (depends on 2)

The preparation method of claim 2, wherein the first polymer is a mixture of the polyvinylidene fluoride and the polymethyl methacrylate.

### Claim 4 (depends on 1)

The preparation method of claim 1, wherein the organic solvent is selected from a group consisting of N,N-dimethylacetamide, N-methyl-2-pyrrolidone, and N,N-dimethylformamide, and any combination thereof.

### Claim 5 (depends on 1)

The preparation method of claim 1, wherein the solid electrolyte comprises a material selected from a group consisting of lanthanum zirconium oxide, tantalum-doped lithium lanthanum zirconium oxide, and lithium aluminum titanium phosphate, and any combination thereof.

### Claim 6 (depends on 1)

The preparation method of claim 1, wherein a mass ratio of the solid electrolyte to the first solution is 1% to 20%.

### Claim 7 (depends on 1)

The preparation method of claim 1, wherein the at least one type of second polymers are selected from a group consisting of types of polyvinylidene fluoride, types of polyacrylonitrile, and types of polyethylene oxide.

### Claim 8 (depends on 7)

The preparation method of claim 7, wherein the at least one type of second polymers is a mixture of four types of polyvinylidene fluorides, the four types of polyvinylidene fluorides have molecular weights of 2 million, 1.5 million, 1.3 million, and 1 million, respectively, and are in a mass ratio of (1%~5%):(5%~10%):(60%~90%):(10%~20%).

### Claim 9 (depends on 1)

The preparation method of claim 1, wherein the polymer mixture is further mixed with N,N-dimethylacetamide containing 0.1 wt. % ionic liquid at a mass ratio ranging from 0.2 to 0.35.

### Claim 10 (depends on 1)

The preparation method of claim 1, wherein the slurry A and the colloid liquid B are mixed at a mass ratio of 0.8~1.65.

### Claim 11 (depends on 1)

The preparation method of claim 1, wherein the ionic liquid comprises 1-ethyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide.

### Claim 12 (depends on 1)

The preparation method of claim 1, wherein mixing the lithium salt and the ionic liquid with the organic solvent further comprises controlling a mass of the lithium salt greater than a mass of the ionic liquid, and a total mass of the lithium salt and the ionic liquid less than 30% of a mass of the electrolyte membrane.

### Claim 13 (depends on 1)

The preparation method of claim 1, wherein the lithium salt is selected from a group consisting of lithium fluoride, lithium bis(fluorosulfonyl)imide, lithium bis(trifluoromethanesulfonyl)imide, lithium bis(perfluoroethanesulfonyl)imide, and lithium bis(oxalato)borate, and any combination thereof.

### Claim 14 (depends on 1)

The preparation method of claim 1, wherein the composite is applied onto the substrate by spin coating or spray coating.

### Claim 15 (depends on 14)

The preparation method of claim 14, wherein the composite is coated onto the substrate by blade coating, and a blade gap is in a range of 200 μm to 500 μm.

### Claim 16 (depends on 15)

The preparation method of claim 15, further comprising providing the substrate having a water contact angle of 70° to 120° and a thickness of 50 μm to 150 μm.

### Claim 17 (depends on 1)

The preparation method of claim 1, wherein drying the composite to form the electrolyte membrane comprises drying the composite in a first drying stage, a second drying stage, and a third drying stage sequentially, wherein a heating temperature of the first drying stage is controlled in a range of 80° C. to 110° C., a heating temperature of the second drying stage is controlled in a range of 130° C. to 150° C., and a heating temperature of the third drying stage is controlled in a range of 150° C. to 180° C.

### Claim 18 (depends on 1)

The preparation method of claim 1, further comprising:
applying a release film onto a surface of the electrolyte membrane away from the substrate.

### Claim 19 (depends on 18)

The preparation method of claim 18, further comprising proving the release film having a water contact angle of 70° to 120° and a thickness of 10 μm to 80 μm.

### Claim 20

An electrolyte membrane prepared by:
mixing a first polymer, an ionic liquid, and an organic solvent to obtain a first solution;
adding solid electrolyte to the first solution to obtain a slurry A;
mixing at least one type of second polymers to obtain a polymer mixture, wherein a weight-average molecular weight of each of the at least one type of second polymers is different from each other; mixing the polymer mixture, the ionic liquid, and the organic solvent to obtain colloid liquid B;
dividing the slurry A into partial batches and adding each of the partial batches of the slurry A to the colloid liquid B to obtain an intermediate colloid C; wherein a mixture of the slurry A and the colloid liquid B is stirred for a period of time after each of the partial batches of the slurry A is added to the colloid liquid B, and a pH of the mixture of the slurry A and the colloid liquid B is maintained to be 6.8 to 7.5;
mixing lithium salt and the ionic liquid with the organic solvent to obtain a composite solution;
mixing the intermediate colloid C with the composite solution to obtain a composite; and
applying the composite onto a substrate and drying the composite to form the electrolyte membrane.