# US 2026/0302342 A1 · Core-shell/glassy solid-state electrolyte, and preparation method therefor and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0302342 A1
- Document ID: US20260302342A1
- Status: Published application
- Kind: A1
- Application number: 19/489,896
- Filed: 2024-05-14
- Published: 2026-10-01
- Earliest claimed: 2023-06-05
- Assignees: Liongo (Changzhou) New Energy Co., Ltd.
- Applicants: Liongo (Changzhou) New Energy Co., Ltd.
- Inventors: Yanfeng LI; Lifei LI; Cheng JIN; Kui ZOU; Chengqi ZHU; Weimin DI
- Web page: https://patentgrep.com/patent/US20260302342A1

## CPC

- H01M 10/0562: Solid materials
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2300/0071: Oxides
- H01M 2300/0094: in the form of layered products, e.g. coatings
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

A composite material includes LiAlPO4(OH)xF1-x and Al(H2PO4)3 compounded on the surface of the LiAlPO4(OH)xF1-x, where 0≤x≤1. A corresponding core-shell/glassy solid-state electrolyte material is also prepared. The composite solid electrolyte has good ionic conductivity, good flexibility, a stable composite structure and thermal stability, such that when being applied to positive electrode coating, the composite solid electrolyte can slow down reduction in the capacity of a positive electrode by a coating layer, effectively remove alkaline residual lithium left on the surface in the preparation process of a positive electrode material, and convert the residual lithium into Li3PO4 favorable for ionic conductivity of the coating layer and AlPO4 capable of protecting the positive electrode.

## Claims

### Claim 1

A composite material, comprising LiAlPO4(OH)xF1-x and Al(H2PO4)3 compounded on a surface of the LiAlPO4(OH)xF1-x, wherein
0
≤
x
≤
1
.

### Claim 2 (depends on 1)

The composite material according to claim 1, wherein the composite material has a core-shell structure, wherein
the LiAlPO4(OH)xF1-x is a core, and the Al(H2PO4)3 is a shell layer;
a thickness of the shell layer is 10 nm-50 nm;
a particle size of the composite material is 80 nm-600 nm; and
a mass ratio of the LiAlPO4(OH)xF1-x to the Al(H2PO4)3 is (30-65):(0.5-3).

### Claim 3

(canceled)

### Claim 4

(canceled)

### Claim 5 (depends on 1)

A core-shell glassy solid-state electrolyte material, calculated based on raw materials, comprising Li3AlF6 and a composite material comprising the composite material according to claim 1 and compounded in the Li3AlF6.

### Claim 6 (depends on 5)

The core-shell glassy solid-state electrolyte material according to claim 5, wherein the Li3AlF6 is a matrix material in the core-shell glassy solid-state electrolyte material;
the composite material compounded in the Li3AlF6 is dispersed in the Li3AlF6;
a mass ratio of the Li3AlF6 to the LiAlPO4(OH)xF1-x in the composite material is (5-30):(30-65); and
the core-shell glassy solid-state electrolyte material comprises a core-shell glassy solid-state electrolyte material for a lithium-ion battery.

### Claim 7 (depends on 6)

The core-shell glassy solid-state electrolyte material according to claim 6, wherein the raw materials further comprise SiO2 or/and Al2O3, wherein
the SiO2 or/and the Al2O3 is dispersed in the Li3AlF6;
a mass ratio of the SiO2 or/and the Al2O3 to the Li3AlF6 is (0.03-0.3):(5-30); and
the lithium-ion battery comprises a coating material for a positive electrode material of the lithium-ion battery.

### Claim 8 (depends on 5)

A preparation method for the core-shell glassy solid-state electrolyte material according to claim 5, comprising steps of:
1) mixing a LiAlPO4(OH)xF1-x slurry with the Al(H2PO4)3 to obtain a slurry, wherein
0
≤
x
≤
1
;
premixing LiF and AlF3, followed by a first sintering to obtain a glassy Li3AlF6 material, and then milling the glassy Li3AlF6 material to obtain a glassy Li3AlF6 powder; and
2) remixing the glassy Li3AlF6 powder, the slurry, and an SiO2 powder or/and an Al2O3 powder, to obtain a mixed slurry; and then subjecting the mixed slurry to vacuum drying to obtain the core-shell glassy solid-state electrolyte material.

### Claim 9 (depends on 8)

The preparation method according to claim 8, wherein the LiAlPO4(OH)xF1-x slurry is obtained by milling the LiAlPO4(OH)xF1-x, wherein
a method for milling the LiAlPO4(OH)xF1-x comprises wet milling;
a rotational speed of milling the LiAlPO4(OH)xF1-x is 500 r/min-2500 r/min; and
a duration of milling the LiAlPO4(OH)xF1-x is 2 h-10 h.

### Claim 10 (depends on 8)

The preparation method according to claim 8, wherein a duration of the mixing is 30 min-600 min;
a molar ratio of the LiF to the AlF3 is (3.0-3.3):1;
a method of the premixing comprises planetary ball mill mixing;
a duration of the premixing is 4 h-12 h; and
a rotational speed of the premixing is 200 r/min-500 r/min.

### Claim 11 (depends on 8)

The preparation method according to claim 8, after the premixing, further comprising a step of drying, wherein
a temperature of the drying is 80° C.-200° C.;
a duration of the drying is 2 h-24 h;
a temperature of the first sintering is 600° C.-950° C.; and
a duration of the first sintering is 5 min-180 min.

### Claim 12 (depends on 8)

The preparation method according to claim 8, after the first sintering, further comprising a step of quenching, wherein
a method of the quenching comprises water quenching or liquid nitrogen cooling; and
a particle size of the glassy Li3AlF6 powder is 100 nm-400 nm.

### Claim 13 (depends on 8)

The preparation method according to claim 8, wherein the remixing is first mixing the glassy Li3AlF6 powder and the slurry, and then further mixing with the SiO2 powder or/and the Al2O3 powder, wherein
a duration of the first mixing is 30 min-300 min;
a duration of the further mixing is 2 h-24 h;
a temperature of the vacuum drying is 100° C.-300° C.; and
a duration of the vacuum drying is 3 h-48 h.

### Claim 14

(canceled)

### Claim 15

(canceled)

### Claim 16 (depends on 5)

A coated positive electrode material for a lithium-ion battery, comprising a positive electrode material and a core-shell glassy solid-state electrolyte material comprising the core-shell glassy solid-state electrolyte material according to claim 5 and coated on the positive electrode material.

### Claim 17 (depends on 16)

The coated positive electrode material for the lithium-ion battery according to claim 16, wherein a mass ratio of the positive electrode material to the core-shell glassy solid-state electrolyte material is 1:(0.02-0.15); and
a coating layer thickness of the core-shell glassy solid-state electrolyte material is 0.6 μm-1.2 μm.

### Claim 18 (depends on 5)

A preparation method for a coated positive electrode material for a lithium-ion battery, comprising steps of:
mixing a positive electrode material, a milled core-shell glassy solid-state electrolyte material, and a solvent, followed by a second sintering, to obtain the coated positive electrode material coated with a core-shell glassy solid-state electrolyte material comprising the core-shell glassy solid-state electrolyte material according to claim 5.

### Claim 19 (depends on 18)

The preparation method according to claim 18, wherein the milled core-shell glassy solid-state electrolyte material has a powder particle size D50 of 0.4 μm-1.0 μm;
steps of the mixing are: first subjecting the positive electrode material and the solvent to ultrasonic stirring and dispersion, and then adding the milled core-shell glassy solid-state electrolyte material, followed by stirring and mixing;
the solvent comprises anhydrous ethanol and/or N-methylpyrrolidone;
a duration of the ultrasonic stirring and dispersion is 20 min-120 min; and
a duration of the stirring and mixing is 2 h-24 h.

### Claim 20 (depends on 18)

The preparation method according to claim 18, after the mixing, further comprising a step of drying, wherein
a temperature of the drying is 80° C.-200° C.;
a duration of the drying is 2 h-12 h;
a temperature of the second sintering is 200° C.-400° C.; and
a holding duration of the second sintering is 2 h-12 h.