# US 2026/0302093 A1 · Manufacturing method of supercapacitor electrode material and supercapacitor electrode using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0302093 A1
- Document ID: US20260302093A1
- Status: Published application
- Kind: A1
- Application number: 19/190,908
- Filed: 2025-04-28
- Published: 2026-10-01
- Earliest claimed: 2025-03-25
- Assignees: CPC Corporation, Taiwan
- Applicants: Cpc Corporation, Taiwan
- Inventors: Cheng-Wei HUANG; Tzu-Hsien HSIEH; Yu-Hsien LIAO; Yang-Chuang CHANG
- Web page: https://patentgrep.com/patent/US20260302093A1

## CPC

- H01G 11/32: Carbon-based
- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- H01G 11/86: specially adapted for electrodes (carbonisation or activation of carbon for the manufacture of electrodes H01G11/34)
- C01P 2006/40: Electric properties
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Disclosed is a manufacturing method of a supercapacitor electrode material, comprising a material preparation step of mixing sodium lignosulfonate, a surfactant and an activator to obtain a biomass material; a heat treatment step of performing on the biomass material a heat treatment at 300° C. for 1 hour in an oxygen-free atmosphere, followed by a heat treatment at 900° C. for 8 hours in an oxygen-free atmosphere to obtain a carbonized material; and a washing step of acid washing the carbonized material with hydrochloric acid to adjust pH to 0.5, followed by water washing to adjust the pH to above 6, thereby obtaining a biomass porous carbon material as the supercapacitor electrode material.

## Claims

### Claim 1

A manufacturing method of a supercapacitor electrode material, comprising:
a material preparation step of mixing sodium ligninsulfonate, a surfactant and an activator to obtain a biomass material;
a heat treatment step of performing on the biomass material a heat treatment at 300° C. for 1 hour in an oxygen-free atmosphere, followed by a heat treatment at 900° C. for 8 hours in an oxygen-free atmosphere to obtain a carbonized material; and
a washing step of acid washing the carbonized material with hydrochloric acid to adjust pH to 0.5, followed by water washing to adjust the pH to above 6, thereby obtaining a biomass porous carbon material as the supercapacitor electrode material.

### Claim 2 (depends on 1)

The manufacturing method as claimed in claim 1, further comprising, before the washing step, a crushing step of crushing the carbonized material.

### Claim 3 (depends on 1)

The manufacturing method as claimed in claim 1, further comprising, after the washing step, a second heat treatment step of performing on the biomass mixture a heat treatment at 300° C. for 1 hour in an oxygen-free atmosphere, followed by a heat treatment at 900° C. for 8 hours in an oxygen-free atmosphere.

### Claim 4 (depends on 1)

The manufacturing method as claimed in claim 1, wherein in the material preparation step, the weight of the activator accounts for 1 to 15% of the weight of the sodium ligninsulfonate.

### Claim 5 (depends on 1)

The manufacturing method as claimed in claim 1, wherein in the raw-material preparation step, the weight of the surfactant accounts for 50 to 200% of the total weight of the sodium ligninsulfonate and the activator.

### Claim 6 (depends on 1)

A supercapacitor electrode, wherein:
as an active material of the super capacitor electrode, the biomass porous carbon material prepared by the manufacturing method as claimed in claim 1 is used,
as a conductive agent of the super capacitor electrode, at least one selected from the group consisting of carbon black, graphite, graphene, carbon nanotubes and carbon nanofibers is used, and
as an adhesive of the supercapacitor electrode, at least one selected from the group consisting of methyl methacrylate, carboxymethyl cellulose, styrene-butadiene rubber and polyvinylidene fluoride is used.

### Claim 7 (depends on 6)

The supercapacitor electrode as claimed in claim 6, wherein the weight of the conductive agent accounts for 1 to 10% of the weight of the active material.

### Claim 8 (depends on 6)

The supercapacitor electrode as claimed in claim 6, wherein the weight of the adhesive accounts for 1 to 10% of the weight of the active material.

### Claim 9 (depends on 2)

A supercapacitor electrode, wherein:
as an active material of the super capacitor electrode, the biomass porous carbon material prepared by the manufacturing method as claimed in claim 2 is used,
as a conductive agent of the super capacitor electrode, at least one selected from the group consisting of carbon black, graphite, graphene, carbon nanotubes and carbon nanofibers is used, and
as an adhesive of the supercapacitor electrode, at least one selected from the group consisting of methyl methacrylate, carboxymethyl cellulose, styrene-butadiene rubber and polyvinylidene fluoride is used.

### Claim 10 (depends on 9)

The supercapacitor electrode as claimed in claim 9, wherein the weight of the conductive agent accounts for 1 to 10% of the weight of the active material.

### Claim 11 (depends on 9)

The supercapacitor electrode as claimed in claim 9, wherein the weight of the adhesive accounts for 1 to 10% of the weight of the active material.

### Claim 12 (depends on 3)

A supercapacitor electrode, wherein:
as an active material of the super capacitor electrode, the biomass porous carbon material prepared by the manufacturing method as claimed in claim 3 is used,
as a conductive agent of the super capacitor electrode, at least one selected from the group consisting of carbon black, graphite, graphene, carbon nanotubes and carbon nanofibers is used, and
as an adhesive of the supercapacitor electrode, at least one selected from the group consisting of methyl methacrylate, carboxymethyl cellulose, styrene-butadiene rubber and polyvinylidene fluoride is used.

### Claim 13 (depends on 12)

The supercapacitor electrode as claimed in claim 12, wherein the weight of the conductive agent accounts for 1 to 10% of the weight of the active material.

### Claim 14 (depends on 12)

The supercapacitor electrode as claimed in claim 12, wherein the weight of the adhesive accounts for 1 to 10% of the weight of the active material.

### Claim 15 (depends on 4)

A supercapacitor electrode, wherein:
as an active material of the super capacitor electrode, the biomass porous carbon material prepared by the manufacturing method as claimed in claim 4 is used,
as a conductive agent of the super capacitor electrode, at least one selected from the group consisting of carbon black, graphite, graphene, carbon nanotubes and carbon nanofibers is used, and
as an adhesive of the supercapacitor electrode, at least one selected from the group consisting of methyl methacrylate, carboxymethyl cellulose, styrene-butadiene rubber and polyvinylidene fluoride is used.

### Claim 16 (depends on 15)

The supercapacitor electrode as claimed in claim 15, wherein the weight of the conductive agent accounts for 1 to 10% of the weight of the active material.

### Claim 17 (depends on 15)

The supercapacitor electrode as claimed in claim 15, wherein the weight of the adhesive accounts for 1 to 10% of the weight of the active material.

### Claim 18 (depends on 5)

A supercapacitor electrode, wherein:
as an active material of the super capacitor electrode, the biomass porous carbon material prepared by the manufacturing method as claimed in claim 5 is used,
as a conductive agent of the super capacitor electrode, at least one selected from the group consisting of carbon black, graphite, graphene, carbon nanotubes and carbon nanofibers is used, and
as an adhesive of the supercapacitor electrode, at least one selected from the group consisting of methyl methacrylate, carboxymethyl cellulose, styrene-butadiene rubber and polyvinylidene fluoride is used.

### Claim 19 (depends on 18)

The supercapacitor electrode as claimed in claim 18, wherein the weight of the conductive agent accounts for 1 to 10% of the weight of the active material.

### Claim 20 (depends on 18)

The supercapacitor electrode as claimed in claim 18, wherein the weight of the adhesive accounts for 1 to 10% of the weight of the active material.