# US 2026/0297729 A1 · Method of forming a structure using selective deposition on a metal surface

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0297729 A1
- Document ID: US20260297729A1
- Status: Published application
- Kind: A1
- Application number: 19/629,057
- Filed: 2026-03-26
- Published: 2026-10-01
- Earliest claimed: 2025-03-31
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: YoungChol Byun; Sang Ho Yu; Chad Russell Lunceford; Richard Nile; Jonathan Bakke; Kranthi Kumar Vaidyula; Holger Saare; Sukanya Datta; Aditya Deshpande
- Web page: https://patentgrep.com/patent/US20260297729A1

## CPC

- C23C 16/0272: {Deposition of sub-layers, e.g. to promote the adhesion of the main coating}
- C23C 16/04: Coating on selected surface areas, e.g. using masks
- C23C 16/4408: {by purging residual gases from the reaction chamber or gas lines}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Methods for forming a structure with selective deposition on a metal surface are disclosed. An exemplary method includes providing a substrate in a reaction chamber, optionally performing a pre-treatment process on the metal surface, performing a growth promotion treatment, and depositing a film on or overlying the metal surface. An exemplary growth promotion treatment includes pulsing a boron-containing precursor and performing a purge.

## Claims

### Claim 1

A method for forming a structure, the method comprising:
providing a substrate in a reaction chamber, wherein the substrate comprises a metal surface on at least part of a surface of the substrate;
performing a growth promotion treatment, wherein the growth promotion treatment comprises pulsing a boron-containing precursor to the reaction chamber and performing a purge; and
selectively depositing a film on the metal surface, wherein depositing the film comprises providing a halide precursor to the reaction chamber.

### Claim 2 (depends on 1)

The method of claim 1, wherein the metal surface comprises one or more of copper, cobalt, nickel, zinc, ruthenium, or molybdenum.

### Claim 3 (depends on 1)

The method of claim 1, wherein the metal surface is metallic.

### Claim 4 (depends on 1)

The method of claim 1, wherein the boron-containing precursor comprises one or more of borane, diborane, triborane, triethylborane, trimethylborane, borazine, and borazane.

### Claim 5 (depends on 1)

The method of claim 1, further comprising performing a pre-treatment process before performing the growth promotion treatment, wherein the pre-treatment process comprises generating a hydrogen plasma.

### Claim 6 (depends on 1)

The method of claim 1, further comprising forming a growth promotion layer on the metal surface, wherein forming the growth promotion layer comprises pulsing the boron-containing precursor.

### Claim 7 (depends on 6)

The method of claim 6, wherein the growth promotion layer has a thickness of between about 20 Angstroms and 50 Angstroms.

### Claim 8 (depends on 1)

The method of claim 1, wherein the growth promotion treatment comprises repeating the steps of pulsing the boron-containing precursor to the reaction chamber and performing the purge a plurality of times.

### Claim 9 (depends on 1)

The method of claim 1, wherein a temperature of the reaction chamber during the method is 400° C. or less.

### Claim 10 (depends on 1)

The method of claim 1, wherein the film is metallic.

### Claim 11 (depends on 10)

The method of claim 10, wherein depositing the film comprises providing a reducing reactant to the reaction chamber.

### Claim 12 (depends on 1)

The method of claim 1, wherein a pulse of the boron-containing precursor is between about 0.2 and 5 seconds.

### Claim 13 (depends on 1)

The method of claim 1, wherein a pressure in the reaction chamber is between about 1 to about 50 Torr.

### Claim 14 (depends on 1)

The method of claim 1, wherein the surface of the substrate comprises one or more features comprising a bottom and one or more sidewalls, wherein the metal surface is disposed on the bottom of the one or more features.

### Claim 15 (depends on 14)

The method of claim 14, wherein the one or more sidewalls comprise a low-k material.

### Claim 16 (depends on 15)

The method of claim 15, wherein the growth promotion treatment comprises forming a growth promotion layer selectively on the metal surface, wherein forming the growth promotion layer comprises pulsing the boron-containing precursor.

### Claim 17 (depends on 6)

The method of claim 6, wherein providing the halide precursor removes at least part of the growth promotion layer.

### Claim 18 (depends on 14)

The method of claim 14, wherein the one or more features comprise an aspect ratio greater than 10.

### Claim 19 (depends on 1)

The method of claim 1, wherein a temperature of the reaction chamber during the growth promotion treatment is 325° C. or less.

### Claim 20

A method for depositing a film on a metal layer, the method comprising
providing a substrate in a reaction chamber, wherein the substrate comprises the metal layer on a surface of the substrate,
depositing a growth promotion layer directly on the metal layer, wherein depositing the growth promotion layer comprises pulsing a boron-containing precursor to the reaction chamber and performing a purge,
depositing the film directly on the growth promotion layer.