# US 2026/0297411 A1 · Thermally conductive silicone composition and production method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0297411 A1
- Document ID: US20260297411A1
- Status: Published application
- Kind: A1
- Application number: 18/996,604
- Filed: 2023-07-11
- Published: 2026-10-01
- Earliest claimed: 2022-07-29
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Mitsuhiro IWATA; Yuji TABATA
- Web page: https://patentgrep.com/patent/US20260297411A1

## CPC

- C09K 5/14: Solid materials, e.g. powdery or granular
- C08K 3/22: of metals
- C08K 3/28: Nitrogen-containing compounds
- C08K 5/5419: containing at least one Si—C bond
- C08L 83/06: containing silicon bound to oxygen-containing groups (C08L83/12 takes precedence)
- C08K 2003/2296: {of zinc}
- C08K 2003/282: {Binary compounds of nitrogen with aluminium}
- C08K 2201/001: Conductive additives
- C08K 2201/005: Additives being defined by their particle size in general
- C08K 2201/006: Additives being defined by their surface area
- C08K 2201/011: Nanostructured additives
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- H10W 40/242: {comprising thermal conductors between chips and the and the arrangements for cooling, e.g. compliant heat-spreaders}
- H10W 40/251: {Organics}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

This thermally conductive silicone composition contains: (A) an organopolysiloxane having a kinematic viscosity of 10-10,000 mm2/s: (B) an organopolysiloxane having a kinematic viscosity of 10-100,000 mm2/s; (C) an aluminum nitride powder which has an oxygen content of 0.5 mass % or less, a BET specific surface area of 1.0 m2/g or less, an average particle diameter of 3-40 μm, and a proportion of coarse particles having particle diameters of 44-105 μm in a volume-based laser diffraction type particle size distribution of 10.0 mass % or less relative to component (C) as a whole; and (D) an irregularly shaped zinc oxide powder at a quantity whereby the blending ratio of component (C) and component (D) is 5.0:5.0 to 9.5:0.5 in terms of mass ratio and the total amount of powders of components (C) and (D) is 70-85 vol % of the composition as a whole. The thermally conductive silicone composition maintains fluidity, exhibits good handleability, exhibits excellent heat dissipation performance, and exhibits excellent durability and reliability under conditions of high temperature and conditions of high temperature and high humidity.

## Claims

### Claim 1

A heat conductive silicone composition comprising
(A) 5 to 100 parts by weight of an organopolysiloxane represented by the general formula (1):
wherein R1 is independently a substituted or unsubstituted monovalent hydrocarbon group, R2 is independently an alkyl, alkoxyalkyl, alkenyl or acyl group, a is an integer of 5 to 100, and b is an integer of 1 to 3, and having a kinematic viscosity at 25° C. of 10 to 10,000 mm2/s,
(B) 0 to 95 parts by weight of an organopolysiloxane represented by the average compositional formula (2):
wherein R3 is independently a C1-C18 substituted or unsubstituted monovalent hydrocarbon group and c is a number of 1.8 to 2.2, and having a kinematic viscosity at 25° C. of 10 to 100,000 mm2/s, the total amount of components (A) and (B) being 100 parts by weight,
(C) an aluminum nitride powder having an oxygen content of up to 0.5% by weight, a BET specific surface area of up to 1.0 m2/g, and an average particle size of 3 to 40 μm, in which the proportion of coarse particles with a particle size of 44 to 105 μm in a volume basis laser diffraction type particle size distribution is up to 10.0% by weight based on overall component (C), and
(D) an irregular shape zinc oxide powder having an average particle size of 0.01 μm to less than 3.0 μm in which the proportion of coarse particles with a sieve particle size of 25 to 45 μm is up to 0.2% by weight based on overall component (D),
components (C) and (D) being blended in a weight ratio of from 5.0:5.0 to 9.5:0.5, the total amount of powder components (C) and (D) being 70 to 85% by volume of the overall composition,
the silicone composition having a thermal conductivity of 4.0 to 9.2 W/m·K as measured by the hot disk method according to ISO 22007-2 and a viscosity at 25° C. of 5 to 800 Pa·s as measured by a spiral viscometer with rotor A at a rotational speed 10 rpm.

### Claim 2 (depends on 1)

The silicone composition of claim 1 wherein component (C) is an aluminum nitride powder of rounded shape.

### Claim 3 (depends on 1)

The silicone composition of claim 1, further comprising (E) a volatile solvent for dispersing or dissolving components (A) and (B), in an amount of up to 100 parts by weight per 100 parts by weight of components (A) and (B) in total.

### Claim 4 (depends on 1)

The silicone composition of claim 1, further comprising (F) 0.1 to 50 parts by weight of an alkoxysilane represented by the general formula (3):
wherein R4 is independently a C9-C15 alkyl group, R5 is independently a C1-C8 substituted or unsubstituted monovalent hydrocarbon group, R6 is independently a C1-C6 alkyl group, d is an integer of 1 to 3, e is an integer of 0 to 2, and d+e is an integer of 1 to 3, with which components (C) and (D) are surface-treated.

### Claim 5 (depends on 1)

The silicone composition of claim 1 which has a viscosity at 25° C. of up to 1,000 Pa-s as measured by a spiral viscometer at a rotational speed of 10 rpm after it is degraded by heating at 200° C. for 100 hours.

### Claim 6 (depends on 1)

The silicone composition of claim 1 which has a thermal resistance at 25° C. of up to 15 mm2-K/W as measured by the laser flash method after it is allowed to stand in a 130° C./85% RH atmosphere for 96 hours.

### Claim 7 (depends on 1)

The silicone composition of claim 1, having a volume resistivity of at least 109 Ω·cm.

### Claim 8 (depends on 1)

A method of preparing the heat conductive silicone composition of claim 1, comprising the step of mixing components (A) to (D).