# US 2026/0297231 A1 · Polymer, electrolyte composition, and battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0297231 A1
- Document ID: US20260297231A1
- Status: Published application
- Kind: A1
- Application number: 19/480,584
- Filed: 2024-05-02
- Published: 2026-10-01
- Earliest claimed: 2023-05-08
- Assignees: Sumitomo Chemical Company, Limited; Kyoto University
- Applicants: Sumitomo Chemical Company, Limited; Kyoto University
- Inventors: Hideto NAKAJIMA; Makoto OUCHI
- Web page: https://patentgrep.com/patent/US20260297231A1

## CPC

- C08F 220/04: Acids; Metal salts or ammonium salts thereof
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present disclosure provides a polymer including a structural unit (A) represented by formula (A) and a structural unit (B) represented by formula (B), wherein when solid 13C NMR measurement of the polymer is performed at 25° C., a half width of a peak derived from carbonyl carbon of a —COOA group (A is an alkali metal element) is 1380 Hz or less. (In formula (A), R1 is a —COOA group or a monovalent organic group having a —COOA group; R2 to R4 are each independently a hydrogen atom or a monovalent substituent, or one of R2 and R3 forms a ring together with R4.) (In formula (B), R5 is a hydrogen atom or a monovalent substituent; R6 to R8 are each independently a hydrogen atom or a monovalent substituent, or one of R6 and R7 forms a ring together with R8.)

## Claims

### Claim 1

A polymer comprising:
a structural unit (A) represented by the following formula (A); and
a structural unit (B) represented by the following formula (B),
wherein the polymer satisfies at least one of the following (1) to (3):
(1) when solid 13C NMR measurement of the polymer is performed at 25° C., a half width of a peak derived from carbonyl carbon of a —COOA group (A is an alkali metal element) is 1380 Hz or less;
(2) when 13C NMR measurement of the polymer is performed in deuterated methanol at 55° C., a half width of a peak derived from carbonyl carbon of the —COOA group is 80 Hz or less; and
(3) when 13C NMR measurement of the polymer is performed in deuterated methanol at 55° C., a ratio of peak height to half width of a peak derived from carbonyl carbon of the —COOA group is 0.4×10−4 abn/Hz or more.
(In formula (A), R1 is a —COOA group or a monovalent organic group having a —COOA group; R2 to R4 are each independently a hydrogen atom or a monovalent substituent, or one of R2 and R3 is a hydrogen atom or a monovalent substituent and the other forms a ring together with R4; and * represents a bonding site of the structural unit (A) with another structural unit.)
(In formula (B), R5 is a hydrogen atom or a monovalent substituent; R6 to R8 are each independently a hydrogen atom or a monovalent substituent, or one of R6 and R7 is a hydrogen atom or a monovalent substituent and the other forms a ring together with R8; and * represents a bonding site of the structural unit (B) with another structural unit.)

### Claim 2 (depends on 1)

The polymer according to claim 1, wherein A comprises at least one of sodium and lithium.

### Claim 3 (depends on 1)

An electrolyte composition comprising the polymer according to claim 1.

### Claim 4 (depends on 3)

The electrolyte composition according to claim 3, further comprising a plasticizer,
wherein the plasticizer comprises at least one selected from the group consisting of carbonate-based solvents, ether-based solvents, fluorine-based solvents, and phosphate ester-based solvents.

### Claim 5 (depends on 3)

The electrolyte composition according to claim 3, further comprising an anion receptor.

### Claim 6 (depends on 3)

The electrolyte composition according to claim 3, further comprising an alkali metal salt.

### Claim 7

A polymer obtained by polymerizing a monomer mixture comprising a monomer (A) having a —COOA group (A is an alkali metal element) and a monomer (B) other than the monomer (A), wherein a reactivity ratio r1 of the monomer (A) and a reactivity ratio r2 of the monomer (B) in a polymerization reaction of the monomer (A) and the monomer (B) are both 0.5 or less.

### Claim 8 (depends on 3)

A battery comprising the electrolyte composition according to claim 3.

### Claim 9 (depends on 2)

An electrolyte composition comprising the polymer according to claim 2.