# US 2026/0296888 A1 · Manufacturing method for lithium phosphate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0296888 A1
- Document ID: US20260296888A1
- Status: Published application
- Kind: A1
- Application number: 19/483,346
- Filed: 2024-12-10
- Published: 2026-10-01
- Earliest claimed: 2023-12-15
- Assignees: Posco Holdings Inc.; Research Institute of Industrial Science & Technology
- Applicants: Posco Holdings Inc.; Research Institute of Industrial Science & Technology
- Inventors: Woonkyoung PARK; Jae Sin PARK; Hee-Soo KANG; Heok YANG
- Web page: https://patentgrep.com/patent/US20260296888A1

## CPC

- C01B 25/305: {Preparation from phosphorus-containing compounds by alkaline treatment}
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A manufacturing method of lithium phosphate includes: introducing a lithium-containing solution into a reactor; introducing an alkaline material and a phosphorus supplying material into the reactor; stirring the lithium-containing solution into which the alkaline material and the phosphorus supplying material are introduced to grow lithium phosphate nucleus particles and obtain a lithium phosphate slurry; and separating the slurry into solid and liquid to obtain the lithium phosphate, in which one of the alkaline material and the phosphorus supplying material is introduced into an upper portion of the reactor, and the other is introduced into a lower portion of the reactor.

## Claims

### Claim 1

A manufacturing method of lithium phosphate, comprising:
introducing a lithium-containing solution into a reactor;
introducing an alkaline material and a phosphorus supplying material into the reactor;
stirring the lithium-containing solution into which the alkaline material and the phosphorus supplying material are introduced to grow lithium phosphate nucleus particles and obtain a lithium phosphate slurry; and
separating the slurry into solid and liquid to obtain the lithium phosphate,
wherein one of the alkaline material and the phosphorus supplying material is introduced into an upper portion of the reactor, and the other is introduced into a lower portion of the reactor.

### Claim 2 (depends on 1)

The manufacturing method of claim 1, wherein:
in the introducing of the alkaline material and the phosphorus supplying material into the reactor,
the alkaline material and the phosphorus supplying material are introduced at the same time.

### Claim 3 (depends on 1)

The manufacturing method of claim 1, wherein:
the alkaline material and the phosphorus supplying material are introduced at a distance of 40 to 100% relative to a height of the reactor.

### Claim 4 (depends on 3)

The manufacturing method of claim 3, wherein:
the alkaline material and the phosphorus supplying material are introduced at a distance of 60 to 100% relative to the height of the reactor.

### Claim 5 (depends on 1)

The manufacturing method of claim 1, wherein:
the alkaline material and the phosphorus supplying material are introduced at a distance of 0 to 100% relative to a width of the reactor.

### Claim 6 (depends on 1)

The manufacturing method of claim 1, wherein:
the alkaline material is introduced into the upper portion of the reactor, and the phosphorus supplying material is introduced into the lower portion of the reactor.

### Claim 7 (depends on 1)

The manufacturing method of claim 1, wherein:
in the stirring of the lithium-containing solution into which the alkaline material and the phosphorus supplying material are introduced to grow the lithium phosphate nucleus particles and obtain the lithium phosphate slurry, the stirring is performed at 30 to 500 RPM.

### Claim 8 (depends on 1)

The manufacturing method of claim 1, wherein:
the stirring of the lithium-containing solution into which the alkaline material and the phosphorus supplying material are introduced to grow the lithium phosphate nucleus particles and obtain the lithium phosphate slurry, includes forming a pH gradient in the reactor;

### Claim 9 (depends on 1)

The manufacturing method of claim 1, wherein:
an introduction time of the alkaline material and the phosphorus supplying material is 10 to 120 minutes.

### Claim 10 (depends on 1)

The manufacturing method of claim 1, wherein:
the stirring of the lithium-containing solution into which the alkaline material and the phosphorus supplying material are introduced to grow the lithium phosphate nucleus particles and obtain the lithium phosphate slurry is performed at a temperature of 0 to 90° C.

### Claim 11 (depends on 1)

The manufacturing method of claim 1, wherein:
the separating of the slurry into the solid and liquid to obtain the lithium phosphate includes:
obtaining a cake containing lithium phosphate particles by separating the slurry into the solid and liquid; and
washing the cake containing the lithium phosphate particles.

### Claim 12 (depends on 11)

The manufacturing method of claim 11, wherein:
the washing is performed at a temperature of 10 to 90° C.

### Claim 13 (depends on 11)

The manufacturing method of claim 11, wherein:
the washing is performed using 100 to 600 parts by weight of washing water based on 100 parts by weight of the entire cake containing the lithium phosphate particles.

### Claim 14 (depends on 1)

The manufacturing method of claim 1, wherein:
the lithium-containing solution is saline water.

### Claim 15 (depends on 1)

The manufacturing method of claim 1, wherein:
the alkaline material includes at least one selected from the group consisting of NaOH, KOH, and LiOH.

### Claim 16 (depends on 1)

The manufacturing method of claim 1, wherein:
the phosphorus supplying material is at least one selected from the group consisting of phosphoric acid, phosphate, and phosphoric acid aqueous solution.