# US 2026/0295559 A1 · Moisture absorption film layered product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0295559 A1
- Document ID: US20260295559A1
- Status: Published application
- Kind: A1
- Application number: 19/572,208
- Filed: 2026-03-19
- Published: 2026-10-01
- Earliest claimed: 2025-03-27
- Assignees: Nippon Steel Chemical & Material Co., Ltd.; Mazda Motor Corporation
- Applicants: NIPPON STEEL Chemical & Material Co., Ltd.; Mazda Motor Corporation
- Inventors: Takashi Saito; Tetsuya Maeda; Tetsuya Sugimoto
- Web page: https://patentgrep.com/patent/US20260295559A1

## CPC

- B01J 20/261: {obtained by reactions only involving carbon to carbon unsaturated bonds (macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds per se C08F)}
- B01J 20/3204: {Inorganic carriers, supports or substrates}
- B01J 20/3214: {characterised by the method for obtaining this coating or impregnating}
- B01J 20/327: {Polymers obtained by reactions involving only carbon to carbon unsaturated bonds}
- B01J 20/3276: {Copolymers}
- B01J 20/3297: {Coatings in the shape of a sheet}
- C03C 17/32: with synthetic or natural resins (C03C17/30 takes precedence)
- C03C 2218/116: by spin-coating, centrifugation
- C03C 2218/32: After-treatment
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Provided is a moisture absorption film layered product that can be photocured in a short time by using ultraviolet ray and that has both defogging properties and scratch resistance. A moisture absorption film layered product, including a moisture absorption film formed on an at least partial surface of a substrate, wherein the moisture absorption film is formed by curing a photocurable resin composition including at least a trifunctional or more (meth)acryl monomer (A) having no ethylene-oxide-modified (meth)acryloyl group, a trifunctional or more (meth)acryl monomer (B) having at least three ethylene-oxide-modified (meth)acryloyl groups, a hydroxyalkyl (meth)acrylate (C), and a photo-initiator as essential components, relative to 100 parts by weight of a total of (A), (B), and (C), a content of (A) is 1 to 20 parts by weight, a content of (B) is 30 to 59 parts by weight, and a content of (C) is 40 to 69 parts by weight.

## Claims

### Claim 1

A moisture absorption film layered product, comprising a moisture absorption film formed on an at least partial surface of a substrate, wherein the moisture absorption film is formed by curing a photocurable resin composition comprising at least
a trifunctional or more (meth)acryl monomer (A) having no ethylene-oxide-modified (meth)acryloyl group,
a trifunctional or more (meth)acryl monomer (B) having at least three ethylene-oxide-modified (meth)acryloyl groups,
a hydroxyalkyl (meth)acrylate (C), and
a photo-initiator as essential components,
relative to 100 parts by weight of a total of the (A), the (B), and the (C),
a content of the (A) is 1 to 20 parts by weight,
a content of the (B) is 30 to 59 parts by weight, and
a content of the (C) is 40 to 69 parts by weight,
the moisture absorption film has a water absorption rate of 10 w % or more and 30 w % or less, and the moisture absorption film of the moisture absorption film layered product has a haze changing value ΔH before and after a Taber abrasion test of 4 or less.

### Claim 2 (depends on 1)

The moisture absorption film layered product according to claim 1, wherein the photocurable resin composition further comprises a hindered-amine light stabilizer (D) having a (meth)acryl group within a range of 0.1 to 7.0 parts by weight relative to 100 parts by weight of the total of the (A), the (B), and the (C).

### Claim 3 (depends on 1)

The moisture absorption film layered product according to claim 1, wherein the photocurable resin composition further comprises an ultraviolet ray absorbent and/or a light stabilizer.

### Claim 4 (depends on 1)

The moisture absorption film layered product according to claim 1, wherein the moisture absorption film layered product is used as a window member for a vehicle.

### Claim 5 (depends on 1)

A method of manufacturing the moisture absorption film layered product according to claim 1, the method comprising:
a step 1 of applying a photocurable resin composition on a substrate; and
a step 2 of irradiating the applied photocurable resin composition with active energy ray for curing the photocurable resin composition to form the moisture absorption film.

### Claim 6 (depends on 5)

The method of manufacturing the moisture absorption film layered product according to claim 5, wherein, in the step 2, the active energy ray has an illuminance within a wavelength region of 320 to 390 nm of 200 to 900 mW/cm2 and an integrated light quantity of 1000 to 8000 mJ/cm2.

### Claim 7

A photocurable resin composition, comprising at least:
a trifunctional or more (meth)acryl monomer (A) having no ethylene-oxide-modified (meth)acryloyl group;
a trifunctional or more (meth)acryl monomer (B) having at least three ethylene-oxide-modified (meth)acryloyl groups;
a hydroxyalkyl (meth)acrylate (C); and
a photo-initiator as essential components,
relative to 100 parts by weight of a total of the (A), the (B), and the (C),
a content of the (A) is 1 to 20 parts by weight,
a content of the (B) is 30 to 59 parts by weight, and
a content of the (C) is 40 to 69 parts by weight,
a moisture absorption film has a water absorption rate of 10 w % or more and 30 w % or less, the moisture absorption film being produced by irradiating the photocurable resin composition with active energy ray under conditions of an illuminance within a wavelength region of 320 to 390 nm of 200 to 900 mW/cm2 and an integrated light quantity of 1000 to 8000 mJ/cm2, and
the moisture absorption film produced on glass so as to have a thickness of 5 μm or more and 25 μm or less has a haze changing value ΔH before and after a Taber abrasion test of 4 or less.

### Claim 8 (depends on 7)

The photocurable resin composition according to claim 7, further comprising a hindered-amine light stabilizer (D) having a (meth)acryl group within a range of 0.1 to 7.0 parts by weight relative to 100 parts by weight of the total of the (A), the (B), and the (C).