# US 2026/0293766 A1 · Method for forming conductive bumps by performing a reflow process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0293766 A1
- Document ID: US20260293766A1
- Status: Published application
- Kind: A1
- Application number: 19/685,028
- Filed: 2026-05-21
- Published: 2026-09-24
- Earliest claimed: 2023-03-13
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chao-Wei Chiu; Wei-Yu Chen; Chih-Chiang Tsao; Hao-Jan Pei; Hsiu-Jen Lin; Ching-Hua Hsieh
- Web page: https://patentgrep.com/patent/US20260293766A1

## CPC

- H10W 90/00: Package configurations
- H10W 20/0698: {Local interconnections}
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/072: {of bump connectors}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/90: Bond pads, in general
- H10W 74/01: Manufacture or treatment
- H10W 74/117: {the substrate having spherical bumps for external connection}
- H10W 70/60: Insulating or insulated package substrates; Interposers; Redistribution layers (leadframes H10W70/40)
- H10W 72/07255: {changes in materials}
- H10W 72/251: {Materials}
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 90/721: {of bump connectors}
- H10W 90/722: {between stacked chips}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

An electronic apparatus including a package substrate and a structure disposed on and electrically connected to the package substrate through conductive bumps is provided. The material of the conductive bumps includes a bismuth (Bi) containing alloy or an indium (In) containing alloy. In some embodiments, the bismuth (Bi) containing alloy includes Sn-Ag-Cu-Bi alloy. In some embodiments, a concentration of bismuth (Bi) contained in the Sn-Ag-Cu-Bi alloy ranges from about 1wt% to about 10wt%. Methods for forming the Sn-Ag-Cu-Bi alloy are also provided.

## Claims

### Claim 1

A method, comprising:
providing a substrate comprising alloy patterns comprising Sn and Cu;
providing a structure comprising alloy patterns comprising Sn and Ag and alloy patterns comprising Sn and X on the alloy patterns comprising Sn and Ag, wherein X represents bismuth or indium;
performing a first thermal process to bond the alloy patterns comprising Sn and X and the alloy patterns comprising Sn and Cu under a first temperature, wherein the alloy patterns comprising Sn and Ag, the alloy patterns comprising Sn and X and the alloy patterns comprising Sn and Cu remain solid state during the first thermal process; and
performing a second thermal process under a second temperature to convert the alloy patterns comprising Sn and Cu, the alloy patterns comprising Sn and Ag and the alloy patterns comprising Sn and X into conductive bumps, wherein the second temperature is higher than the first temperature.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein during the first thermal process, an intermetallic compound (IMC) layer is generated between the alloy patterns comprising Sn and X and the alloy patterns comprising Sn and Cu.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the alloy patterns comprising Sn and Cu are liquid state, the alloy patterns comprising Sn and X are solid state, and the alloy patterns comprising Sn and Ag are solid state when performing the second thermal process.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the alloy patterns comprising Sn and Cu, the alloy patterns comprising Sn and X and the alloy patterns comprising Sn and Ag are solid state when performing the second thermal process.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the alloy patterns comprising Sn and Cu, the alloy patterns comprising Sn and X and the alloy patterns comprising Sn and Ag are liquid state when performing the second thermal process.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein a material of the conductive bumps comprises Sn-Ag-Cu-X alloy, and a concentration of X contained in the Sn-Ag-Cu-X alloy ranges from about 1wt% to about 10wt%.

### Claim 7

A method, comprising:
forming alloy patterns comprising Sn and X on a first structure, wherein X represents bismuth or indium;
forming alloy patterns comprising Sn and Ag on a second structure;
performing a first thermal process to bond the alloy patterns comprising Sn and X and the alloy patterns comprising Sn and Ag, wherein the alloy patterns comprising Sn and X and the alloy patterns comprising Sn and Ag remain solid state during the first thermal process; and
after performing the first thermal process, performing a second thermal process to convert the alloy patterns comprising Sn and X and the alloy patterns comprising Sn and Ag into conductive bumps, wherein a first process temperature of the first thermal process is lower than a second process temperature of the second thermal process.

### Claim 8 (depends on 7)

The method as claimed in claim 7, wherein during the first thermal process, an intermetallic compound (IMC) layer is generated between the alloy patterns comprising Sn and X and the alloy patterns comprising Sn and Ag.

### Claim 9 (depends on 7)

The method as claimed in claim 7, wherein the alloy patterns comprising Sn and X are solid state, and the alloy patterns comprising Sn and Ag are liquid state when performing the second thermal process.

### Claim 10 (depends on 7)

The method as claimed in claim 7, wherein the alloy patterns comprising Sn and X are liquid state, and the alloy patterns comprising Sn and Ag are liquid state when performing the second thermal process.

### Claim 11 (depends on 7)

The method as claimed in claim 7, wherein the alloy patterns comprising Sn and X are solid state, and the alloy patterns comprising Sn and Ag are solid state when performing the second thermal process.

### Claim 12

A method, comprising:
forming Sn-Cu alloy patterns on a first structure;
forming Sn-Ag alloy patterns on a second structure;
forming Sn-X alloy patterns between the Sn-Cu alloy patterns and the Sn-Ag alloy patterns, wherein X represents bismuth or indium;
pre-heating the Sn-Ag alloy patterns, the Sn-X alloy patterns and the Sn-Cu alloy patterns, wherein the Sn-X alloy patterns remain solid state during pre-heating the Sn-Ag alloy patterns, the Sn-X alloy patterns and the Sn-Cu alloy patterns; and
after pre-heating the Sn-Ag alloy patterns, the Sn-X alloy patterns and the Sn-Cu alloy patterns, reflowing the Sn-Ag alloy patterns, the Sn-X alloy patterns and the Sn-Cu alloy patterns to form solder joints between the first structure and the second structure.

### Claim 13 (depends on 12)

The method as claimed in claim 12, wherein the Sn-Ag alloy patterns, the Sn-X alloy patterns and the Sn-Cu alloy patterns remain solid state during pre-heating the Sn-Ag alloy patterns, the Sn-X alloy patterns and the Sn-Cu alloy patterns.

### Claim 14 (depends on 12)

The method as claimed in claim 12, wherein the Sn-Cu alloy patterns are liquid state, the Sn-X alloy patterns are solid state, and the Sn-Ag alloy patterns are solid state when reflowing the Sn-Ag alloy patterns, the Sn-X alloy patterns and the Sn-Cu alloy patterns.

### Claim 15 (depends on 12)

The method as claimed in claim 12, wherein the Sn-Cu alloy patterns, the Sn-X alloy patterns and the Sn-Ag alloy patterns are solid state when reflowing the Sn-Ag alloy patterns, the Sn-X alloy patterns and the Sn-Cu alloy patterns.

### Claim 16 (depends on 12)

The method as claimed in claim 12, wherein the Sn-Cu alloy patterns, the Sn-X alloy patterns and the Sn-Ag alloy patterns are liquid state when reflowing the Sn-Ag alloy patterns, the Sn-X alloy patterns and the Sn-Cu alloy patterns.

### Claim 17 (depends on 12)

The method as claimed in claim 12, wherein a material of the conductive bumps comprises Sn-Ag-Cu-X alloy, and a concentration of X contained in the Sn-Ag-Cu-X alloy ranges from about 1wt% to about 10wt%.

### Claim 18 (depends on 12)

The method as claimed in claim 12, wherein a concentration of silver (Ag) contained in the Sn-Ag alloy patterns ranges from about 1.0wt% to about 2.5wt%, and a thickness of the Sn-Ag alloy pattern ranges from about 20 micrometers to about 25 micrometers.

### Claim 19 (depends on 12)

The method as claimed in claim 12, wherein a concentration of bismuth (Bi) contained in the Sn-Bi alloy patterns ranges from about 40wt% to about 58wt%, and a thickness of the Sn-Bi alloy patterns ranges from about 10 micrometers to about 15 micrometers.

### Claim 20 (depends on 12)

The method as claimed in claim 12, wherein a concentration of copper (Cu) contained in the Sn-Cu alloy patterns ranges from about 0.4wt% to about 1.1wt%, and a thickness of the Sn-Cu alloy patterns ranges from about 35 micrometers to about 45 micrometers.