# US 2026/0282854 A1 · Method for filling gap

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0282854 A1
- Document ID: US20260282854A1
- Status: Published application
- Kind: A1
- Application number: 19/666,535
- Filed: 2026-05-04
- Published: 2026-09-17
- Earliest claimed: 2023-09-11
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Po-Hsien CHENG; Tai-Chun HUANG; Chung-Ting KO; Chia-Yu FANG; Sung-En LIN; Yu-Yun PENG
- Web page: https://patentgrep.com/patent/US20260282854A1

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6536: {by exposure to radiation, e.g. visible light}
- H10P 14/6546: {to change the surface groups of the insulating materials}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for filling a gap includes: filling a dielectric layer in the gap so that a seam is formed in the dielectric layer, the dielectric layer including two surface portions at two opposite sides of the seam, respectively; introducing a surface modification agent into the seam such that each of the two surface portions has first functional groups and second functional groups; forming a stress layer on the dielectric layer to cover the seam, the stress layer including a material different from that of the dielectric layer; and applying an energy field to permit the two surface portions to bond with each other through reaction between the first functional groups and the second functional groups.

## Claims

### Claim 1

A method for manufacturing a semiconductor structure, comprising:
forming a gap which extends from an upper surface of a base structure into an interior of the base structure;
depositing a dielectric layer in the gap so that a seam is formed in the dielectric layer, the dielectric layer including two surface portions at two opposite sides of the seam, respectively;
depositing a stress layer on the dielectric layer to cover the seam, the stress layer including a material different from a material of the dielectric layer; and
applying an electromagnetic field with a predetermined frequency to heat the two surface portions such that the two surface portions are bonded to each other.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein prior to depositing the stress layer, the seam has a width between the two surface portions which ranges from 5 Å to 1 nm.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the stress layer and the dielectric layer have different coefficients of thermal expansion such that a stress is generated between the stress layer and the dielectric layer.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the dielectric layer includes silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbide, silicon carbon nitride, silicon oxycarbon nitride, boron nitride, metal oxide, metal nitride, metal oxynitride, metal oxycarbide, metal carbon nitride, metal oxycarbon nitride, or combinations thereof.

### Claim 5 (depends on 4)

The method as claimed in claim 4, wherein the stress layer includes amorphous silicon, silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, silicon oxycarbide, silicon carbon nitride, silicon oxycarbon nitride, boron nitride, metal oxide, metal nitride, metal oxynitride, metal oxycarbide, metal carbon nitride, metal oxycarbon nitride, or combinations thereof.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein
the two surface portions are formed with ─OH groups, and
when the two surface portions are heated, the ─OH groups on one of the two surface portions and the ─OH groups on the other one of the two surface portions react with each other, so as to permit the two surface portions to be bonded to each other.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein
the two surface portions are formed with ─H groups and ─NHx groups, where x is 1 or 2, and
when the two surface portions are heated, the ─NHx groups on one of the two surface portions and the ─H groups on the other one of the two surface portions react with each other, so as to permit the two surface portions to be bonded to each other.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the predetermined frequency ranges from 100 kHz to 100 GHz.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein during applying the electromagnetic field, a temperature at the two surface portions is higher than a temperature of the stress layer and a temperature of the base structure.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the electromagnetic field is applied with a power ranging from 1500 W to 10000 W for a time period ranging from 10 seconds to 30 minutes.

### Claim 11

A method for manufacturing a semiconductor structure, comprising:
forming a gap which extends into a base structure;
depositing a dielectric layer in the gap, so that a seam is formed in the dielectric layer, the dielectric layer including two surface portions at two opposite sides of the seam, respectively;
introducing a surface modification agent into the seam so that the two surface portions undergo oxidation; and
applying an electromagnetic field to heat the two surface portions such that the two surface portions are bonded to each other through oxygen.

### Claim 12 (depends on 11)

The method as claimed in claim 11, wherein
after oxidation of the two surface portions, the two surface portions are formed with ─OH groups, and
the two surface portions are bonded to each other through dehydration of the ─OH groups respectively on the two surface portions.

### Claim 13 (depends on 11)

The method as claimed in claim 11, wherein introduction of the surface modification agent into the seam is performed by immersing the dielectric layer in the atmosphere of gas molecules, the gas molecules including water steam or hydrogen peroxide.

### Claim 14 (depends on 11)

The method as claimed in claim 11, wherein the surface modification agent includes a plasma, and a precursor gas for generating the plasma includes a gas mixture of hydrogen and oxygen.

### Claim 15 (depends on 11)

The method as claimed in claim 11, after introduction of the surface modification agent into the seam, and before application of the electromagnetic field, further comprising:
depositing a stress layer on the dielectric layer to cover the seam, the stress layer having a coefficient of thermal expansion that is different from a coefficient of thermal expansion of the dielectric layer.

### Claim 16

A method for manufacturing a semiconductor structure, comprising:
forming a gap which extends into a base structure;
depositing a dielectric layer in the gap, so that a seam is formed in the dielectric layer, the dielectric layer including two surface portions at two opposite sides of the seam, respectively;
introducing a surface modification agent into the seam so that the two surface portions undergo nitridation; and
applying an electromagnetic field to heat the two surface portions such that the two surface portions are bonded to each other through nitrogen.

### Claim 17 (depends on 16)

The method as claimed in claim 16, wherein:
after nitridation of the two surface portions, the two surface portions are formed with ─H groups and ─NHx groups, where x is 1 or 2, and
the two surface portions are bonded to each other through dehydrogenation of the ─NHx groups on one of the two surface portions and the ─H groups on the other one of the two surface portions.

### Claim 18 (depends on 16)

The method as claimed in claim 16, wherein introduction of the surface modification agent into the seam is performed by immersing the dielectric layer in the atmosphere of gas molecules, the gas molecules including ammonia or hydrazine.

### Claim 19 (depends on 16)

The method as claimed in claim 16, wherein the surface modification agent includes a plasma, a precursor gas for generating the plasma includes an ammonia gas or a gas mixture of nitrogen and hydrogen.

### Claim 20 (depends on 16)

The method as claimed in claim 16, after introduction of the surface modification agent into the seam, and before application of the electromagnetic field, further comprising:
depositing a stress layer on the dielectric layer to cover the seam, the stress layer having a coefficient of thermal expansion that is different from a coefficient of thermal expansion of the dielectric layer.