# US 2026/0279623 A1 · Thin film resistor and method of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0279623 A1
- Document ID: US20260279623A1
- Status: Published application
- Kind: A1
- Application number: 19/403,024
- Filed: 2025-11-27
- Published: 2026-09-17
- Earliest claimed: 2025-03-14
- Assignees: Yageo Corporation
- Applicants: Yageo Corporation
- Inventors: Shen-Li HSIAO; Min-Syuan HOU
- Web page: https://patentgrep.com/patent/US20260279623A1

## CPC

- C23C 14/5806: {Thermal treatment}
- H01C 7/006: {Thin film resistors}
- C23C 14/165: {by cathodic sputtering}
- C23C 14/185: {by cathodic sputtering}
- C23C 14/3464: {using more than one target (C23C14/56 takes precedence)}
- H01C 1/032: plural layers surrounding the resistive element (H01C1/028 takes precedence)
- H01C 17/12: by sputtering
- H10D 1/474: {comprising refractory metals, transition metals, noble metals, metal compounds or metal alloys, e.g. silicides}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01C: RESISTORS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A thin film resistor and a method of forming the same are provided. The method includes forming an insulated oxide film on an upper surface of a substrate; forming a first inner electrode pair on two ends of the insulated oxide film; performing a DC multi-target hybrid sputtering operation to deposit a resistor layer on a portion of the insulated oxide film and a portion of the pair of first inner electrode; performing an RF-DC hybrid sputtering operation to deposit a doping layer over the resistor layer; performing an annealing operation so as to oxidize the doping layer to an oxidized doping film; and forming a passivation layer on the oxidized doping film. Therefore, resistance value and resistivity of the thin film resistor can be controlled.

## Claims

### Claim 1

A method of forming a thin film resistor, comprising:
forming an insulated oxide film on an upper surface of a substrate;
forming a first inner electrode pair on two ends of the insulated oxide film;
performing a DC multi-target hybrid sputtering operation to deposit a resistor layer on a portion of the insulated oxide film and a portion of the first inner electrode pair, wherein the DC multi-target hybrid sputtering operation comprises sputtering Ni-Cr alloy, tantalum and molybdenum;
performing an RF-DC hybrid sputtering operation to deposit a doping layer over the resistor layer, wherein the RF-DC hybrid sputtering operation comprises RF sputtering silicon and DC sputtering aluminum;
performing an annealing operation so as to oxidize the doping layer to form an oxidized doping film; and
forming a passivation layer on the oxidized doping film.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the insulated oxide film comprises:
forming a sputtering layer on the substrate, wherein the sputtering layer comprises tantalum or silicon; and
sintering the sputtering layer to form the insulated oxide film, wherein the insulated oxide film comprises tantalum oxide or silicon oxide.

### Claim 3 (depends on 1)

The method of claim 1, wherein when performing the DC multi-target hybrid sputtering operation, a sputtering power of the tantalum is 60% to 100% of a sputtering power of the Ni-Cr alloy, and a sputtering power of the molybdenum is 5% to 30% of the sputtering power of the Ni-Cr alloy.

### Claim 4 (depends on 1)

The method of claim 1, wherein when performing the RF-DC hybrid sputtering operation, a sputtering power of the aluminum is 20% to 50% of a sputtering power of the silicon.

### Claim 5 (depends on 1)

The method of claim 1, wherein based on weight of the resistor layer as 100 wt%, the resistor layer comprises:
45 wt% to 75 wt% of the Ni-Cr alloy;
20 wt% to 40 wt% of the tantalum; and
5 wt% to 15 wt% of the molybdenum.

### Claim 6 (depends on 1)

The method of claim 1, wherein a weight ratio of the aluminum and the silicon in the doping layer is 1:1 to 1:5.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
forming a first insulated protective layer on the passivation layer; and
forming a second inner electrode pair on the ends of the insulated oxide film, wherein the first inner electrode pair and a portion of the first insulated protective layer are covered by the second inner electrode pair.

### Claim 8 (depends on 7)

The method of claim 7, further comprising:
forming a second insulated protective layer on an exposed portion of the first insulated protective layer and a portion of the second inner electrode pair.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
forming a back electrode pair on two ends of a lower surface of the substrate; and
forming an outer electrode pair from the second insulated protective layer to the back electrode pair along two side portions of the substrate.

### Claim 10 (depends on 1)

A thin film resistor, formed by the method of claim 1.

### Claim 11

A method of forming a thin film resistor, comprising:
forming an insulated oxide film on an upper surface of a substrate;
forming a first inner electrode pair on two ends of the insulated oxide film;
performing a DC multi-target hybrid sputtering operation to deposit a resistor layer on a portion of the insulated oxide film and a portion of the first inner electrode pair;
performing an RF-DC hybrid sputtering operation to deposit a doping layer over the resistor layer;
performing an annealing operation so as to oxidize the doping layer to form an oxidized doping film, wherein the oxidized doping film comprises aluminum oxide and silicon oxide;
forming a passivation layer on the oxidized doping film;
forming a first insulated protective layer on the passivation layer; and
forming a second inner electrode pair on the ends of the insulated oxide film.

### Claim 12 (depends on 11)

The method of claim 11, wherein the DC multi-target hybrid sputtering operation comprises sputtering Ni-Cr alloy, tantalum and molybdenum.

### Claim 13 (depends on 12)

The method of claim 12, wherein when performing the DC multi-target hybrid sputtering operation, a ratio of a sputtering power of the tantalum to a sputtering power of the Ni-Cr alloy is 0.6 to 1, and a ratio of a sputtering power of the molybdenum to the sputtering power of the Ni-Cr alloy is 0.05 to 0.3.

### Claim 14 (depends on 11)

The method of claim 11, wherein the RF-DC hybrid sputtering operation comprises RF sputtering silicon and DC sputtering aluminum, and a weight ratio of aluminum and silicon in the doping layer is 1:1 to 1:5.

### Claim 15 (depends on 14)

The method of claim 14, wherein when performing the RF-DC hybrid sputtering operation, a ratio of a sputtering power of the aluminum to a sputtering power of the silicon is 0.2 to 0.5.

### Claim 16 (depends on 11)

The method of claim 11, further comprising:
forming a first mask layer around the insulated oxide film and on a portion of the first inner electrode pair so as to expose an area to be sputtered on the substrate before performing the DC multi-target hybrid sputtering operation, wherein a ratio of a length of the area to be sputtered to a length of the substrate is 1/4 to 3/4, and a ratio of a width of the area to be sputtered to a width of the substrate is 2/5 to 4/5; and
removing the first mask layer after depositing the doping layer.

### Claim 17 (depends on 11)

The method of claim 11, wherein the annealing operation is performed with a heating temperature in a range from 300°C. to 600°C. and a duration time in a range from 2 hours to 6 hours.

### Claim 18 (depends on 11)

The method of claim 11, further comprising:
forming a second mask layer around the insulated oxide film and on a portion of the first inner electrode pair so as to expose an area to be passivated on the substrate before forming the passivation layer, wherein a ratio of a length of the area to be passivated to a length of the substrate is 3/4 to 4/5, and a ratio of a width of the area to be passivated to a width of the substrate is 4/5 to 1; and
removing the second mask layer after forming the passivation layer.

### Claim 19 (depends on 11)

The method of claim 11, wherein the resistor layer has a thickness in a range from 0.02 μm to 0.5 μm, and the doping layer has a thickness in a range from 0.005 μm to 0.05 μm.

### Claim 20 (depends on 11)

The method of claim 11, further comprising:
forming a second insulated protective layer on an exposed portion of the first insulated protective layer and a portion of the second inner electrode pair.