# US 2026/0275562 A1 · Metal sheet with zinc hydroxysulfate/zinc sulfate-based protection layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0275562 A1
- Document ID: US20260275562A1
- Status: Published application
- Kind: A1
- Application number: 19/681,699
- Filed: 2026-05-19
- Published: 2026-09-17
- Earliest claimed: 2012-01-10
- Applicants: ArcelorMittal
- Inventors: Daniel Chaleix; Christian Allely; Maxime Monnoyer; Pascale Feltin
- Web page: https://patentgrep.com/patent/US20260275562A1

## CPC

- C25D 11/34: of metals or alloys not provided for in groups C25D11/04 - C25D11/32
- C23C 22/53: Treatment of zinc or alloys based thereon
- C23C 22/68: using aqueous solutions with pH between 6 and 8
- C25D 5/48: After-treatment of electroplated surfaces
- Y10T 428/1266: O, S, or organic compound in metal component
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A sheet includes a steel substrate; a coating covering at least one face of the steel substrate, the coating comprising zinc, magnesium and aluminum; and a zinc hydroxysulfate/zinc sulfate-based temporary protection layer applied over the coating, the temporary protection layer having a sulfur content greater than or equal to 0.5 mg/m2 and less than or equal to 30 mg/m2.

## Claims

### Claim 1

A coiled and stored steel sheet, wherein the coiled and stored steel sheet consists of:
a steel substrate;
a multilayer coating covering at least one face of the steel substrate, the multilayer coating consisting of a layer of zinc and a layer of zinc and magnesium over the layer of zinc, the multilayer coating having a nonuniform distribution of zinc;
a zinc hydroxysulfate/zinc sulfate-based temporary protection layer applied over the multilayer coating, the temporary protection layer having a sulfur content greater than or equal to 0.5 mg/m2 and less than or equal to 30 mg/m2 wherein the zinc hydroxysulfate/zinc sulfate temporary protection layer is stabilized by the magnesium in the multilayer coating to prevent the formation of zinc carbonates in the presence of atmospheric CO2;
an optional film of oil applied over the zinc hydroxysulfate/zinc sulfate-based temporary protection layer.

### Claim 2 (depends on 1)

The sheet as recited in claim 1, wherein the layer of zinc and the layer of zinc and magnesium are applied by vacuum deposition.

### Claim 3 (depends on 1)

The sheet as recited in claim 1, wherein the zinc hydroxysulfate/zinc sulfate temporary protection layer is stabilized by the magnesium in the coating such that, when tested by a test performed in a humidity and temperature controlled corrosion-test chamber in accordance with DIN EN ISO 6270-2, less than 10% of a surface of a test piece is visually altered after 10 cycles with 1 g/m2 oil or after 15 cycles with 1.2 g/m2 of oil.

### Claim 4 (depends on 1)

The sheet as recited in claim 1, wherein the layer of zinc and magnesium has a thickness of less than or equal to 20 μm, and the magnesium content is 0.1 to 20% by weight.

### Claim 5 (depends on 4)

The sheet as recited in claim 4, wherein the layer of zinc has a higher content of zinc than the layer of zinc and magnesium.

### Claim 6 (depends on 1)

The sheet as recited in claim 1, wherein the multilayer coating comprises approximately 80% by weight zinc and 20% by weight magnesium.

### Claim 7 (depends on 1)

The sheet as recited in claim 1, wherein the sheet has a polarization resistance between between 840 Ω and 1200 Ω.

### Claim 8

A coiled and stored steel sheet, wherein the coiled and stored steel sheet consists of:
a steel substrate;
a multilayer coating covering at least one face of the steel substrate, the multilayer coating consisting of a layer of zinc deposited by electrodeposition and a layer of zinc and magnesium over the layer of zinc;
a zinc hydroxysulfate/zinc sulfate-based temporary protection layer applied over the multilayer coating, the temporary protection layer having a sulfur content greater than or equal to 0.5 mg/m2 and less than or equal to 30 mg/m2;
an optional film of oil applied over the zinc hydroxysulfate/zinc sulfate-based temporary protection layer;
wherein the zinc hydroxysulfate/zinc sulfate temporary protection layer is stabilized by the magnesium in the coating such that, when tested by a test performed in a humidity and temperature controlled corrosion-test chamber in accordance with DIN EN ISO 6270-2, less than 10% of a surface of a test piece is visually altered after 10 cycles with 1 g/m2 oil or after 15 cycles with 1.2 g/m2 of oil.

### Claim 9 (depends on 8)

The sheet as recited in claim 8, wherein the layer of zinc and magnesium has a thickness of less than or equal to 20 μm, and the magnesium content is 0.1 to 20% by weight.

### Claim 10 (depends on 8)

The sheet as recited in claim 8, wherein the multilayer coating has a nonuniform distribution of zinc, with the layer of zinc having a higher content of zinc than the layer of zinc and magnesium.

### Claim 11 (depends on 8)

The sheet as recited in claim 8, wherein the layer of zinc and magnesium is an alloyed layer of zinc and magnesium.

### Claim 12 (depends on 11)

The sheet as recited in claim 11, wherein the multilayer coating comprises approximately 80% by weight zinc and 20% by weight magnesium.

### Claim 13 (depends on 8)

The sheet as recited in claim 8, wherein the sheet has a polarization resistance between between 840 Ω and 1200 Ω.

### Claim 14 (depends on 8)

The sheet as recited in claim 8, wherein the zinc hydroxysulfate/zinc sulfate-based temporary protection layer is of a thickness that is effective to reduce tarnishing of the multilayer coating, based on an aging test under natural exposure conditions under shelter in accordance with standard VDA 230-213 (test length 12 weeks), as compared to a coiled and stored steel sheet consisting of a steel substrate coated with a multilayer coating consisting of a layer of zinc deposited by electrodeposition and a layer of zinc and magnesium over the layer of zinc.

### Claim 15 (depends on 8)

The sheet as recited in claim 8, wherein the zinc hydroxysulfate/zinc sulfate-based temporary protection layer is of a thickness that is effective to reduce blackening of the multilayer coating, based on a test performed in humidity and temperature controlled corrosion-test chamber, as specified by DIN EN ISO 6270-2 following application of the oil, as compared to a coiled and stored steel sheet consisting of a steel substrate coated with a multilayer coating consisting of a layer of zinc deposited by electrodeposition and a layer of zinc and magnesium over the layer of zinc.

### Claim 16

A coiled and stored steel sheet, wherein the coiled and stored steel sheet consists of:
a cold-rolled steel substrate;
a multilayer coating consisting of a layer of zinc and a layer of zinc and magnesium over the layer of zinc;
a zinc hydroxysulfate/zinc sulfate-based temporary protection layer applied over the multilayer coating, the temporary protection layer having a sulfur content greater than or equal to 0.5 mg/m2 and less than or equal to 30 mg/m2 wherein the zinc hydroxysulfate/zinc sulfate temporary protection layer is stabilized by the magnesium in the multilayer coating to prevent the formation of zinc carbonates in the presence of atmospheric CO2;
an optional film of oil applied over the zinc hydroxysulfate/zinc sulfate-based temporary protection layer.

### Claim 17 (depends on 16)

The sheet as recited in claim 16, wherein the zinc hydroxysulfate/zinc sulfate-based temporary protection layer is of a thickness that is effective to reduce tarnishing of the multilayer coating, based on an aging test under natural exposure conditions under shelter in accordance with standard VDA 230-213 (test length 12 weeks), as compared to a coiled and stored steel sheet consisting of a cold-rolled steel substrate coated with a multilayer coating consisting of a layer of zinc and a layer of zinc and magnesium over the layer of zinc.

### Claim 18 (depends on 16)

The sheet as recited in claim 16, wherein the zinc hydroxysulfate/zinc sulfate-based temporary protection layer is of a thickness that is effective to reduce blackening of the multilayer coating, based on a test performed in humidity and temperature controlled corrosion-test chamber, as specified by DIN EN ISO 6270-2 following application of the oil, as compared to a coiled and stored steel sheet consisting of a cold-rolled steel substrate coated with a multilayer coating consisting of a layer of zinc, a layer of zinc and magnesium over the layer of zinc, and a film film of oil applied over the layer of zinc and magnesium.

### Claim 19 (depends on 16)

The sheet as recited in claim 16, wherein the zinc hydroxysulfate/zinc sulfate temporary protection layer is stabilized by the magnesium in the coating such that, when tested by a test performed in a humidity and temperature controlled corrosion-test chamber in accordance with DIN EN ISO 6270-2, less than 10% of a surface of a test piece is visually altered after 10 cycles with 1 g/m2 oil or after 15 cycles with 1.2 g/m2 of oil.

### Claim 20 (depends on 19)

The sheet as recited in claim 19, wherein the multilayer coating has a nonuniform distribution of zinc, with the layer of zinc having a higher content of zinc than the layer of zinc and magnesium.

### Claim 21 (depends on 19)

The sheet as recited in claim 19, wherein the multilayer coating comprises approximately 80% by weight zinc and 20% by weight magnesium.

### Claim 22 (depends on 19)

The sheet as recited in claim 19, wherein the layer of zinc and magnesium has a thickness of less than or equal to 20 μm.

### Claim 23

A coiled and stored steel sheet, wherein the coiled and stored steel sheet consists of:
a steel substrate;
a multilayer coating covering at least one face of the steel substrate, the multilayer coating produced by heat treating a layer of zinc deposited by electrodeposition and a layer of magnesium deposited by vacuum deposition over the layer of zinc;
a zinc hydroxysulfate/zinc sulfate-based temporary protection layer applied over the multilayer coating, the temporary protection layer having a sulfur content greater than or equal to 0.5 mg/m2 and less than or equal to 30 mg/m2;
an optional film of oil applied over the zinc hydroxysulfate/zinc sulfate-based temporary protection layer;
wherein the zinc hydroxysulfate/zinc sulfate temporary protection layer is stabilized by the magnesium in the coating such that, when tested by a test performed in a humidity and temperature controlled corrosion-test chamber in accordance with DIN EN ISO 6270-2, less than 10% of a surface of a test piece is visually altered after 10 cycles with 1 g/m2 oil or after 15 cycles with 1.2 g/m2 of oil.

### Claim 24 (depends on 23)

The sheet as recited in claim 23, wherein the zinc hydroxysulfate/zinc sulfate-based temporary protection layer is of a thickness that is effective to reduce tarnishing of the multilayer coating, based on an aging test under natural exposure conditions under shelter in accordance with standard VDA 230-213 (test length 12 weeks), as compared to a coiled and stored steel sheet consisting of a steel substrate coated with a multilayer coating produced by heat treating a layer of zinc deposited by electrodeposition and a layer of zinc and magnesium deposited by vacuum deposition over the layer of zinc.

### Claim 25 (depends on 23)

The sheet as recited in claim 23, wherein the zinc hydroxysulfate/zinc sulfate-based temporary protection layer is of a thickness that is effective to reduce blackening of the multilayer coating, based on a test performed in humidity and temperature controlled corrosion-test chamber, as specified by DIN EN ISO 6270-2 following application of the oil, as compared to a coiled and stored steel sheet consisting of a steel substrate coated with a multilayer coating produced by heat treating a layer of zinc deposited by electrodeposition and a layer of zinc and magnesium deposited by vacuum deposition over the layer of zinc.

### Claim 26 (depends on 23)

The sheet as recited in claim 23, wherein the sheet has a polarization resistance between between 840 Ω and 1200 Ω.

### Claim 27

A coiled and stored steel sheet, wherein the coiled and stored steel sheet consists of:
a steel substrate;
a multilayer coating covering at least one face of the steel substrate, the multilayer coating consisting of a layer of zinc deposited by vacuum deposition and a layer of zinc and magnesium over the layer of zinc;
a zinc hydroxysulfate/zinc sulfate-based temporary protection layer applied over the multilayer coating, the temporary protection layer having a sulfur content greater than or equal to 0.5 mg/m2 and less than or equal to 30 mg/m2
an optional film of oil applied over the zinc hydroxysulfate/zinc sulfate-based temporary protection layer;
wherein the zinc hydroxysulfate/zinc sulfate temporary protection layer is stabilized by the magnesium in the coating such that, when tested by a test performed in a humidity and temperature controlled corrosion-test chamber in accordance with DIN EN ISO 6270-2, less than 10% of a surface of a test piece is visually altered after 10 cycles with 1 g/m2 oil or after 15 cycles with 1.2 g/m2 of oil.

### Claim 28

A coiled and stored steel sheet, wherein the coiled and stored steel sheet consists of:
a steel substrate;
a multilayer coating covering at least one face of the steel substrate, the multilayer coating made by heat treating a layer of zinc deposited by vacuum deposition and a layer magnesium deposited by vacuum deposition over the layer of zinc, consisting of a layer of zinc deposited by vacuum deposition and a layer of zinc and magnesium over the layer of zinc;
a zinc hydroxysulfate/zinc sulfate-based temporary protection layer applied over the multilayer coating, the temporary protection layer having a sulfur content greater than or equal to 0.5 mg/m2 and less than or equal to 30 mg/m2
an optional film of oil applied over the zinc hydroxysulfate/zinc sulfate-based temporary protection layer;
wherein the zinc hydroxysulfate/zinc sulfate temporary protection layer is stabilized by the magnesium in the coating such that, when tested by a test performed in a humidity and temperature controlled corrosion-test chamber in accordance with DIN EN ISO 6270-2, less than 10% of a surface of a test piece is visually altered after 10 cycles with 1 g/m2 oil or after 15 cycles with 1.2 g/m2 of oil.