# US 2026/0275551 A1 · Methods for selectively depositing nano- or microscopic plugs in membranes for electrochemical applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0275551 A1
- Document ID: US20260275551A1
- Status: Published application
- Kind: A1
- Application number: 19/566,459
- Filed: 2026-03-13
- Published: 2026-09-17
- Earliest claimed: 2025-03-14
- Assignees: The Trustees of Columbia University in the City of New York
- Applicants: The Trustees of Columbia University in the City of New York
- Inventors: DANIEL VINCENT ESPOSITO; Jesse Dondapati; Alan West; Lucas Cohen
- Web page: https://patentgrep.com/patent/US20260275551A1

## CPC

- C25B 13/02: characterised by shape or form
- C25B 13/07: based on ceramics
- C25B 9/19: with diaphragms
- C25B 9/23: comprising ion-exchange membranes in or on which electrode material is embedded
- C25B 9/75: having bipolar electrodes
- C25B 9/77: having diaphragms
- C25B 11/031: Porous electrodes
- C25B 11/052: Electrodes comprising one or more electrocatalytic coatings on a substrate
- C25B 11/077: the compound being a non-noble metal oxide
- C25B 13/05: based on inorganic materials
- C25B 13/08: based on organic materials
- C25B 1/04: by electrolysis of water
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)

## Abstract

Crossover through submicron thick SiO2 membranes can be mitigated by selectively depositing oxide, e.g., carbon-containing silicon oxide (SiOxCy) “nanoplugs” into the pinholes and cracks of the membranes. Defect-containing membranes are contacted with a deposition solution including hydrolysable precursors, e.g., metal alkoxides like tetraethyl orthosilicate (TEOS), and a nanoplug directing agent, e.g., tetramethylammonium bromide (TMAB). Current is applied to the defect-containing membranes in pulses, including a shorter “on” phase where current is applied and a longer “off phase” where current is not applied. The SiOxCy nanoplugs are deposited to the structural defects during the “on” phase. The longer “off phase” enables reactants to diffuse back to the structural defects for deposition of additional nanoplugs during the next “on” phase, as well as prevent deposition of SiOxCy on non-defective regions. Treatment of plugged SiO2 membranes reduced H2 permeation rates by 5-6 orders of magnitude compared to unmodified SiO2 and 1-2 orders of magnitude compared to Nafion-117 membranes.

## Claims

### Claim 1

A method for depositing plugs into defects of an electrolyzer membrane, comprising:
contacting an oxide-material membrane with a deposition solution, wherein the oxide-material membrane includes a plurality of structural defects; and
applying a current for two or more pulses across the oxide-material membrane to provide oxide-material nanoplugs to at least some of the structural defects,
wherein the deposition solution includes a hydrolysable oxide precursor compound and a nanoplug directing agent.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the hydrolysable oxide precursor compound includes tetraethyl orthosilicate (TEOS), tetramethyl orthosilicate (TMOS), methyltriethoxysilane (MTES), n-dodecyltriethoxysilane (DTES), n-dodecyltrimethoxysilane (DTMS), or combinations thereof.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the nanoplug directing agent includes tetramethylammonium bromide (TMAB), tetramethylammonium fluoride (TMAF), tetraethylammonium bromide (TEAB), tetrapropylammonium bromide (TPAB), cetyltrimethylammonium bromide (CTAB), cetyltrimethylammonium chloride (CTAC), 1-dodecyl-3-methylimidazolium bromide, and cetylpyridinium chloride, or combinations thereof.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the pulses are on average about 0.2 seconds at 10 second intervals.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the current is applied for 20 or more pulses.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the oxide-material membrane is composed of undoped SiO2.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the oxide-material membrane has a thickness of at most 100 nm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the current density is between about −4 and about −5 mA cm−2.

### Claim 9 (depends on 1)

The method according to claim 1, further comprising:
removing the oxide-material membrane from the deposition solution;
drying the oxide-material membrane to form a dried membrane;
contacting the dried membrane with an additional amount of deposition solution; and
applying a second current for two or more pulses across the dried membrane.

### Claim 10 (depends on 1)

The method according to claim 1, further comprising:
flexing the oxide-material membrane to form cracks therein prior to contacting the oxide-material membrane with the deposition solution.

### Claim 11

A method of making a membrane-electrode assembly, comprising:
depositing a layer of oxide material on an electrode assembly including a first electrode, wherein the layer includes a plurality of structural defects;
contacting the layer with a deposition solution including a hydrolysable oxide precursor compound and a nanoplug directing agent;
applying a current for two or more pulses across the electrode assembly to electrochemically generate hydroxide ions in the deposition solution; and
depositing oxide-material nanoplugs to at least some structural defects in the layer and form a plugged membrane.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the hydrolysable oxide precursor compound includes tetraethyl orthosilicate (TEOS) and the nanoplug directing agent includes tetramethylammonium bromide (TMAB).

### Claim 13 (depends on 11)

The method according to claim 11, wherein the layer has an H2-gas permeance greater than 3.2×10−10 molH2 m−2 s−1 Pa−1.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the electrode assembly includes a catalyst layer, a porous layer, or combinations thereof.

### Claim 15 (depends on 11)

The method according to claim 11, wherein the layer is flexed to form additional structural defects prior to contacting the layer with the deposition solution.

### Claim 16 (depends on 11)

The method according to claim 11, wherein the current is applied for 50 or more pulses.

### Claim 17 (depends on 11)

The method according to claim 11, further comprising:
drying the plugged membrane;
contacting the plugged membrane with a second deposition solution; and
applying a second current for two or more pulses across the plugged membrane.

### Claim 18

A method of making a membrane-electrode assembly, comprising:
depositing a layer of oxide material on an electrode assembly including a first electrode, wherein the layer includes undoped SiO2;
fracturing the layer via a force applied thereto;
contacting the layer with an acidic deposition solution including tetraethyl orthosilicate (TEOS) and tetramethylammonium bromide (TMAB);
applying a first current for two or more first pulses across the layer to electrochemically generate hydroxide ions in structural defects in the layer;
reacting hydroxide ions with TEOS in at least some of the structural defects to form SiOxCy nanoplugs therein and produce a first plugged membrane;
drying the first plugged membrane to form a dried plugged membrane;
contacting the dried plugged membrane with a second acidic deposition solution including TEOS and TMAB;
applying a second current for two or more second pulses across the dried plugged membrane;
reacting hydroxide ions with TEOS to form additional SiOxCy nanoplugs in the dried plugged membrane and produce a second plugged membrane; and
positioning a second electrode on the electrode assembly such that the second plugged membrane is positioned between the first electrode and the second electrode.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the first pulses are greater than about 50 pulses and the second pulses are greater than about 20 pulses.

### Claim 20 (depends on 18)

The method according to claim 18, wherein the layer has an H2-gas permeance greater than 3.2×10−10 molH2 m2 s−1 Pa−1 and the second plugged membrane has an H2-gas permeance less than about 4.9×10−11 molH2 m−2 s−1 Pa−1.