# US 2026/0275456 A1 · Copper alloy sheet material, method for producing same, and current-carrying component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0275456 A1
- Document ID: US20260275456A1
- Status: Published application
- Kind: A1
- Application number: 19/168,930
- Filed: 2024-02-14
- Published: 2026-09-17
- Earliest claimed: 2023-03-29
- Assignees: Dowa Metaltech Co., Ltd.
- Applicants: Dowa Metaltech Co., Ltd.
- Inventors: Ryosuke MIYAHARA; Yuta SASAI; Tomotsugu AOYAMA
- Web page: https://patentgrep.com/patent/US20260275456A1

## CPC

- C22C 9/00: Alloys based on copper
- C22F 1/08: of copper or alloys based thereon
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

[Problem] To provide a sheet material having excellent strength and electrical conduction property and also having an increased bending workability level in a Cu—Fe—P-based copper alloy. [Solution]A copper alloy sheet material, having a chemical composition containing, in mass %, Fe: 0.05 to 1.10%, P: 0.02 to 0.50%, Mg: 0 to 0.50%, Ni: 0 to 0.80%, Sn: 0 to 0.80%, Zn: 0 to 0.80%, and elements other than Fe, P, Mg, Ni, Sn, Zn, and Cu: 0 to 0.10% in total, with a balance including Cu, in which a crystallite size, as determined using a Halder-Wagner method based on an integral width of a peak in an X-ray diffraction pattern using Cu-Kα radiation on a sheet surface, is 30 nm or less, and a 0.2% proof stress in a direction perpendicular to a rolling direction is 450 N/mm2 or more.

## Claims

### Claim 1

A copper alloy sheet material, having a chemical composition comprising, in mass %, Fe: 0.05 to 1.10%, P: 0.02 to 0.50%, Mg: 0 to 0.50%, Ni: 0 to 0.80%, Sn: 0 to 0.80%, Zn: 0 to 0.80%, and elements other than Fe, P, Mg, Ni, Sn, Zn, and Cu: 0 to 0.10% in total, with a balance including Cu, wherein a crystallite size, as determined using a Halder-Wagner method based on an integral width of a peak in an X-ray diffraction pattern using Cu-Kα radiation on a sheet surface, is 30 nm or less, and a 0.2% proof stress in a direction perpendicular to a rolling direction is 450 N/mm2 or more.

### Claim 2 (depends on 1)

The copper alloy sheet material according to claim 1, wherein a number density of precipitate particles having a major axis of 10 to 100 nm is 50 particles/m2 or more in an observation plane parallel to a sheet surface.

### Claim 3 (depends on 1)

The copper alloy sheet material according to claim 1, wherein an electrical conductivity is 50% IACS or more.

### Claim 4 (depends on 1)

The copper alloy sheet material according to claim 1, wherein MBR/t being a ratio of a minimum bending radius MBR without cracking to a sheet thickness t in a 90° L bending test with a bending axis parallel to a rolling direction (B.W.) is 0.7 or less.

### Claim 5

A method for producing a copper alloy sheet material, comprising, in the following order:
a hot rolling step of subjecting a cast slab having a chemical composition containing, in mass %, Fe: 0.05 to 1.10%, P: 0.02 to 0.50%, Mg: 0 to 0.50%, Ni: 0 to 0.80%, Sn: 0 to 0.80%, Zn: 0 to 0.80%, and elements other than Fe, P, Mg, Ni, Sn, Zn, and Cu: 0 to 0.10% in total, with a balance including Cu to rolling at a rolling reduction rate of 70% or more in a temperature range of 950° C. or lower and 650° C. or higher, and then rolling at a rolling reduction rate of 60% or more in a temperature range of lower than 650° C. and 350° C. or higher;
an intermediate cold rolling step of performing cold rolling at a rolling reduction rate of 30% or more;
an intermediate heat treatment step of subjecting a material obtained in the intermediate cold rolling step to a heat treatment of holding the material at a temperature of 400° C. or higher and 700° C. or lower for 1 hour or more;
a finish cold rolling step of subjecting a material obtained in the intermediate heat treatment step to cold rolling at a rolling reduction rate of 80% or more; and
a finish heat treatment step of subjecting a material obtained in the finish cold rolling step to a heat treatment of heating the material in a temperature range of 180° C. or higher and 500° C. or lower.

### Claim 6 (depends on 5)

The method for producing a copper alloy sheet material according to claim 5, wherein in the finish heat treatment step, a material having a crystallite size, as determined using a Halder-Wagner method based on an integral width of a peak in an X-ray diffraction pattern using Cu-Kα radiation on a sheet surface, of 30 nm or less is obtained.

### Claim 7 (depends on 1)

A current-carrying component formed using the copper alloy sheet material according to claim 1.