# US 2026/0275434 A1 · Method for producing molten pig iron

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0275434 A1
- Document ID: US20260275434A1
- Status: Published application
- Kind: A1
- Application number: 19/168,722
- Filed: 2024-02-28
- Published: 2026-09-17
- Earliest claimed: 2023-03-29
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Yuji IWAMI; Nobuhiko ODA; Naoto NAKAMURA; Takahide HIGUCHI
- Web page: https://patentgrep.com/patent/US20260275434A1

## CPC

- C21B 11/10: in electric furnaces
- C21B 13/12: in electric furnaces
- C21B 13/008: {Use of special additives or fluxing agents}
- C21B 13/02: in shaft furnaces
- C21B 13/143: {Injection of partially reduced ore into a molten bath}
- C21C 1/00: Refining of pig-iron; Cast iron
- C21C 5/527: {Charging of the electric furnace}
- C21C 5/54: Processes yielding slags of special composition
- Y02P 10/20: Recycling
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing molten pig iron that can achieve high energy efficiency in a melting step of melting reduced iron in a submerged arc furnace, including: a melting step of melting, in a submerged arc furnace, an iron source raw material including reduced iron with an average metallization rate of 60% or greater to obtain molten pig iron, the melting step also including at least one or both of adding a slag forming material to adjust the basicity (CaO/SiO2) of molten slag formed on the molten pig iron, and adding a carbonaceous material to adjust the C content of the molten pig iron. Herein, the metallization rate refers to the mass percentage of a metallic iron component to the total mass of an iron component contained in the reduced iron, and the basicity (CaO/SiO2) of the molten slag refers to the mass ratio of CaO to SiO2.

## Claims

### Claim 1

A method for producing molten pig iron, comprising:
a melting step of melting an iron source raw material including reduced iron with an average metallization rate of 60% or greater in a submerged arc furnace to obtain molten pig iron, the melting step also including at least one or both of the following; adding a slag forming material to adjust a basicity (CaO/SiO2) of molten slag formed on the molten pig iron; and
adding a carbonaceous material to adjust a C content of the molten pig iron, wherein the metallization rate refers to a mass percentage of a metallic iron component to a total mass of an iron component contained in the reduced iron, and the basicity (CaO/SiO2) of the molten slag refers to a mass ratio of CaO to SiO2.

### Claim 2 (depends on 1)

The method for producing molten pig iron according to claim 1, further comprising:
a step for preparing a raw material for direct reduction including a process for acquiring iron ore pellets produced from low-grade iron ore with a total Fe content of 63 mass % or less; and
a reduced iron production step including a process for producing the reduced iron from the raw material for direct reduction.

### Claim 3 (depends on 2)

The method for producing molten pig iron according to claim 2, wherein
the raw material for direct reduction used in the reduced iron production step includes lump ore.

### Claim 4 (depends on 1)

The method for producing molten pig iron according to claim 1, wherein
the slag forming material is added to achieve the basicity (CaO/SiO2) of the molten slag within the range of 1.0 to 1.3.

### Claim 5 (depends on 1)

The method for producing molten pig iron according to claim 1, wherein
the carbonaceous material is added to achieve the C content of the molten pig iron within the range of 2 to 5 mass %.

### Claim 6 (depends on 2)

The method for producing molten pig iron according to claim 2, wherein
the slag forming material is added to achieve the basicity (CaO/SiO2) of the molten slag within the range of 1.0 to 1.3.

### Claim 7 (depends on 3)

The method for producing molten pig iron according to claim 3, wherein
the slag forming material is added to achieve the basicity (CaO/SiO2) of the molten slag within the range of 1.0 to 1.3.

### Claim 8 (depends on 2)

The method for producing molten pig iron according to claim 2, wherein
the carbonaceous material is added to achieve the C content of the molten pig iron within the range of 2 to 5 mass %.

### Claim 9 (depends on 3)

The method for producing molten pig iron according to claim 3, wherein
the carbonaceous material is added to achieve the C content of the molten pig iron within the range of 2 to 5 mass %.

### Claim 10 (depends on 4)

The method for producing molten pig iron according to claim 4, wherein
the carbonaceous material is added to achieve the C content of the molten pig iron within the range of 2 to 5 mass %.

### Claim 11 (depends on 6)

The method for producing molten pig iron according to claim 6, wherein
the carbonaceous material is added to achieve the C content of the molten pig iron within the range of 2 to 5 mass %.

### Claim 12 (depends on 7)

The method for producing molten pig iron according to claim 7, wherein
the carbonaceous material is added to achieve the C content of the molten pig iron within the range of 2 to 5 mass %.