# US 2026/0275145 A1 · Eco-friendly anti-icing coating composition including switchable hydrophilic-hydrophobic copolymer and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0275145 A1
- Document ID: US20260275145A1
- Status: Published application
- Kind: A1
- Application number: 19/348,309
- Filed: 2025-10-02
- Published: 2026-09-17
- Earliest claimed: 2025-03-13
- Assignees: Pusan National University Industry-University Cooperation Foundation
- Applicants: Pusan National University Industry-University Cooperation Foundation
- Inventors: Chae Bin KIM; Se Hui AN
- Web page: https://patentgrep.com/patent/US20260275145A1

## CPC

- C09D 125/08: Copolymers of styrene (C09D129/08, C09D135/06, C09D155/02 take precedence)
- C09D 7/61: inorganic
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

An eco-friendly anti-icing coating composition includes a switchable hydrophilic-hydrophobic copolymer, which includes a styrene-maleic anhydride switchable hydrophilic-hydrophobic copolymer between hydrophilic and hydrophobic, enabling an eco-friendly coating using water as a solvent while simultaneously exhibiting excellent waterproofing properties and durability. A method for preparing the eco-friendly anti-icing coating composition includes: preparing a styrene-maleic anhydride (SMA) copolymer; preparing a copolymer mixture by mixing the SMA copolymer and graphene oxide (GO); and preparing a coating composition by adding an alcohol to the copolymer mixture.

## Claims

### Claim 1

An eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer, the composition comprising:
a styrene-maleic anhydride (SMA) copolymer including styrene and maleic anhydride; and
graphene oxide (GO).

### Claim 2 (depends on 1)

The eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 1, wherein the SMA copolymer is represented by the following [Chemical Formula 1]:

### Claim 3 (depends on 1)

The eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 1, wherein the SMA copolymer includes the styrene and the maleic anhydride in a molar ratio of 1 to 4:1.

### Claim 4 (depends on 1)

The eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 1, wherein the SMA copolymer reversibly exhibits a ring-opening reaction and a ring-closing reaction.

### Claim 5 (depends on 4)

The eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 4, wherein the ring-opening reaction occurs when the coating composition is added to a basic solution and stirred.

### Claim 6 (depends on 4)

The eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 4, wherein the ring-closing reaction occurs when the coating composition is heated at 180 to 220° C. for three to seven minutes.

### Claim 7 (depends on 1)

The eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 1, wherein the coating composition includes 0.5% to 10% by weight of the GO based on 100% by weight of the coating composition.

### Claim 8

A method for preparing an eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer, the method comprising:
a step of preparing a styrene-maleic anhydride (SMA) copolymer;
a step of preparing a copolymer mixture by mixing the SMA copolymer and graphene oxide (GO); and
a step of preparing a coating composition by adding an alcohol to the copolymer mixture.

### Claim 9 (depends on 8)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 8, wherein the step of preparing the SMA copolymer includes:
a step of preparing a reaction solution by adding styrene, maleic anhydride, and an initiator to a polar organic solvent and then heating and stirring;
a step of purifying unreacted monomers by precipitating the reaction solution in an alcohol;
a step of obtaining an SMA copolymer by filtering the reaction solution purified from unreacted monomers; and
a step of drying the SMA copolymer.

### Claim 10 (depends on 9)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 9, wherein the polar organic solvent is tetrahydrofuran (THF), and the initiator is azobisisobutyronitrile (AIBN).

### Claim 11 (depends on 9)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 9, wherein, in the step of preparing the reaction solution, the styrene and the maleic anhydride are added in a molar ratio of 1 to 4:1 and then heated and stirred.

### Claim 12 (depends on 9)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 9, wherein, in the step of preparing the reaction solution, heating is performed to 60 to 80° C. and stirring is performed for 22 to 26 hours.

### Claim 13 (depends on 9)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 9, wherein, in the step of purifying unreacted monomers by precipitating the reaction solution in an alcohol, the reaction solution is precipitated in an alcohol in a weight ratio of 1:3 to 5.

### Claim 14 (depends on 9)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 9, wherein, in the step of drying the SMA copolymer, heating is performed at 40 to 60° C. for 13 to 17 hours.

### Claim 15 (depends on 8)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 8, wherein, in the step of preparing a copolymer mixture by mixing the SMA copolymer and GO, 0.5% to 10% by weight of the GO is mixed based on 100% by weight of the copolymer mixture.

### Claim 16 (depends on 8)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 8, wherein the step of preparing a copolymer mixture by mixing the SMA copolymer and GO includes:
a step of preparing a dispersion by adding GO to water and then dispersing; and
a step of adding the SMA copolymer and a basic solution to the dispersion and then stirring and dispersing.

### Claim 17 (depends on 16)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 16, wherein, in the step of adding the SMA copolymer and a basic solution to the dispersion and then stirring and dispersing, the basic solution is added in a weight ratio of 1:0.3 to 0.9 based on the water.

### Claim 18 (depends on 8)

The method for preparing the eco-friendly anti-icing coating composition including a switchable hydrophilic-hydrophobic copolymer according to claim 8, wherein, in the step of preparing a coating composition by adding an alcohol to the copolymer mixture, the alcohol is added in a weight ratio of 1:0.8 to 1.2 based on the water.