# US 2026/0275040 A1 · Multifunctional heteroleptic polyhedral oligomeric silsesquioxane (poss) and fabrication methods thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0275040 A1
- Document ID: US20260275040A1
- Status: Published application
- Kind: A1
- Application number: 19/079,387
- Filed: 2025-03-13
- Published: 2026-09-17
- Earliest claimed: 2025-03-13
- Assignees: Nano and Advanced Materials Institute Limited
- Applicants: Nano and Advanced Materials Institute Limited
- Inventors: Yong ZHU; Yubo CHENG; Koonyee LIN; Fei ZHANG; Chun Lung CHOI; Li FU; Chenmin LIU
- Web page: https://patentgrep.com/patent/US20260275040A1

## CPC

- C08G 77/045: {containing less than 25 silicon atoms}
- C08G 77/06: Preparatory processes
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A method for fabricating multifunctional heteroleptic polyhedral oligomeric silsesquioxane (POSS) in a single reaction vessel is introduced. The method involves creating an alkaline environment by adding a first organic solvent, water, and a base, followed by the dropwise introduction of organosilanes at a controlled rate of 0.1-0.5 g per second to prevent rapid gelation. The organosilanes, constituting 15-50% of the solution, undergo hydrolysis and condensation reactions at a defined temperature and duration, converting alkoxy groups to silanol groups and forming siloxane bonds, resulting in POSS cage structures. The reaction mixture is then adjusted to a pH of 3-5 by adding acid to quench condensation, stabilize the POSS, and prevent aggregation, yielding a POSS crude product.

## Claims

### Claim 1

A method of fabricating a multifunctional heteroleptic polyhedral oligomeric silsesquioxane (POSS) in a single reaction vessel, comprising:
adding a first organic solvent, water, base in a reaction vessel to create an alkaline environment for hydrolysis and condensation reactions;
introducing a set of organosilanes in a dropwise manner at a controlled rate to prevent rapid gelation, wherein the total organosilane content accounts for 15-50% of the total solution, wherein the controlled rate is between 0.1-0.5 g per second to ensure uniform cage formation;
subjecting the reaction vessel to a defined temperature and duration to initiate hydrolysis and condensation reactions, wherein the hydrolysis reaction converts alkoxy groups of the organosilanes to silanol groups, and the condensation reaction condenses the silanol groups to form siloxane bonds, resulting in POSS cage structures; and
adjusting the reaction mixture to a pH value of 3-5 by adding an acid to quench the condensation reaction, stabilizing the POSS cage structures, and prevent POSS aggregation, thereby yielding a POSS crude product;
wherein the set of organosilanes comprises glycidyltrimethoxysilane, cyclohexylepoxypropyltrimethoxysilane, methacryloxypropyltrimethoxysilane, acryloxypropyltrimethoxysilane, octyltrimethoxysilane, phenyltrimethoxysilane, aminopropyltrimethoxysilane, and polyethylene glycol (PEG)-modified silanes.

### Claim 2 (depends on 1)

The method of claim 1, wherein the alkaline environment has a pH value ranging from 12 to 14.

### Claim 3 (depends on 1)

The method of claim 1, wherein the defined temperate ranges from 25° C. to 150° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the reaction duration ranges from 2 to 24 hours.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first organic solvent is selected from ethanol, acetone or a mixture thereof.

### Claim 6 (depends on 1)

The method of claim 1, further comprising adding phase transfer catalysts to facilitate interactions between hydrophilic and hydrophobic components.

### Claim 7 (depends on 1)

The method of claim 1, wherein the POSS crude product is further purified by:
removing the residual solvent and dissolving the crude POSS in a POSS-philic solvent;
using a siloxane gel-philic solvent to induce a liquid-liquid phase separation, thereby forming a siloxane gel phase and a POSS-philic solvent phase;
collecting, filtering, and evaporating the POSS-philic solvent phase to obtain a purified POSS product with a purity of over 98%.

### Claim 8 (depends on 7)

The method of claim 7, wherein the POSS-philic solvent is selected from relatively polar organic solvents, such as acetone, butanone, acetonitrile, ethanol, or methanol.

### Claim 9 (depends on 7)

The method of claim 7, wherein the siloxane gel-philic solvent is selected from toluene, n-hexane, or cyclohexane.

### Claim 10 (depends on 1)

A multifunctional heteroleptic POSS produced by the method of claim 1.

### Claim 11 (depends on 10)

The multifunctional heteroleptic POSS of claim 10, wherein the multifunctional heteroleptic POSS comprises two reactive and thermal stable groups: glycidyl-containing R1 and cyclohexylepoxy-containing R2, a photo/thermal-curable crosslinking group R3, a hydrophobic group R4, and a hydrophilic group R5.

### Claim 12 (depends on 11)

The multifunctional heteroleptic POSS of claim 11, wherein the multifunctional heteroleptic POSS has a formula: [R1mR2nR3oR4pR5q][SiO3/2]m+n+o+p+q,
wherein the R1 is selected from one of more of epoxypropoxy, epoxidized olefins, glycidyl, and glycidyl ether;
the R2 is selected from one of more of epoxycyclohexane and cycloaliphatic epoxy;
the R3 is selected from one or more of the following: amine, oxetane, episulfide, acrylate, methacrylate, thiol-acrylate, thiol-methacrylate, acrylamide, vinyl sulfide, vinyl ether, styrene, norbornyl, cyclopentadiene, and acryloxypropyl;
the R4 is selected from alkyl chains, phenyl group, perfluoropolyether (PFPE), polytetrafluoroethylene (PTFE), and polydimethylsiloxane (PDMS);
the R5 is selected from alkyl chains, phenyl group, perfluoropolyether (PFPE), polytetrafluoroethylene (PTFE), and polydimethylsiloxane (PDMS); and
the m, n, o, p and q range from 0 to 20 with a sum equal or less than 20.

### Claim 13 (depends on 10)

The multifunctional heteroleptic POSS of claim 10, wherein the multifunctional heteroleptic POSS is applied in advanced coatings, adhesives, biomedical materials, or nanocomposites.