# US 2026/0273511 A1 · Spherical alumina and supported catalyst, and preparation methods and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0273511 A1
- Document ID: US20260273511A1
- Status: Published application
- Kind: A1
- Application number: 19/222,272
- Filed: 2025-05-29
- Published: 2026-09-17
- Earliest claimed: 2025-03-13
- Assignees: Tianjin University; Dalian University of Technology
- Applicants: Tianjin University; Dalian University of Technology
- Inventors: Lun Pan; Jijun Zou; Chong Peng; Linlin Liu; Kang Xue; Ruijie Gao; Chengxiang Shi; Zhenfeng Huang; Minhua Ai; Xiangwen Zhang
- Web page: https://patentgrep.com/patent/US20260273511A1

## CPC

- B01J 21/04: Alumina
- B01J 37/0072: {Preparation of particles, e.g. dispersion of droplets in an oil bath}
- B01J 23/40: of the platinum group metals
- B01J 23/42: Platinum
- B01J 23/44: Palladium
- B01J 23/58: with alkali- or alkaline earth metals
- B01J 35/36: Mechanical strength
- B01J 35/37: Crush or impact strength
- B01J 35/394: {Metal dispersion value, e.g. percentage or fraction}
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/50: characterised by their shape or configuration
- B01J 35/51: Spheres
- B01J 35/55: Cylinders or rings
- B01J 35/613: {10-100 m2/g}
- B01J 35/615: {100-500 m2/g}
- B01J 35/647: {2-50 nm}
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/0036: {Grinding}
- B01J 37/0201: {Impregnation}
- B01J 37/0207: {Pretreatment of the support}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 37/18: with gases containing free hydrogen
- C01F 7/021: After-treatment of oxides or hydroxides
- C07C 5/325: {of the platinum group}
- C07C 2523/56: Platinum group metals
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

Provided are a spherical alumina and a supported catalyst, and preparation methods and use thereof. A method for preparing the spherical alumina includes: kneading an alumina powder, an adhesive, and water, and subjecting a resulting mixture to extrusion to obtain a strip-shaped sample; and subjecting the strip-shaped sample to spheronization to obtain spherical particles, and subjecting the spherical particles to a first calcination to obtain the spherical alumina. The spherical alumina with a higher sphericity is prepared from the alumina powder using a process that integrates kneading, extrusion, and spheronization, and a diameter of the spherical alumina could be adjusted and controlled by adjusting a diameter of the strip-shaped sample obtained after the extrusion.

## Claims

### Claim 1

A method for preparing a spherical alumina, comprising the following steps:
kneading an alumina powder, an adhesive, and water, and subjecting a resulting mixture to extrusion to obtain a strip-shaped sample; and
subjecting the strip-shaped sample to spheronization to obtain spherical particles, and subjecting the spherical particles to a first calcination to obtain the spherical alumina.

### Claim 2 (depends on 1)

The method of claim 1, wherein the adhesive comprises one selected from the group consisting of an inorganic acid, formic acid, acetic acid, and citric acid;
a mass ratio of the alumina powder to the adhesive is in a range of 100: 0.5-6; and
a mass ratio of the alumina powder to the water is in a range of 1:0.5-2.0.

### Claim 3 (depends on 1)

The method of claim 1, wherein the extrusion is performed by using a single-screw extruder with auto-feed compression; and
the strip-shaped sample has a diameter of not less 0.6 millimetres (mm).

### Claim 4 (depends on 1)

The method of claim 1, wherein the spheronization is performed by placing the strip-shaped sample into a spheronizer and subjecting the strip-shaped sample to spheronization to obtain the spherical particles.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first calcination is conducted at a temperature of 500° C. to 600° C. for 3 hours to 6 hours.

### Claim 6 (depends on 1)

A spherical alumina prepared by the method of claim 1, wherein the spherical alumina has an average diameter of not less 0.6 mm, a sphericity of 0.911 to 0.986, and a strength of 6.7 N/particle to 10.7 N/particle.

### Claim 7 (depends on 6)

A method of using the spherical alumina of claim 6, comprising using the spherical alumina as a catalyst support.

### Claim 8 (depends on 6)

A supported catalyst, comprising a support and a catalytically active component loaded on the support, wherein the support is the spherical alumina of claim 6, and the catalytically active component comprises a noble metal; and
a loading amount of the catalytically active component in the supported catalyst is 0.5 wt % to 4 wt %.

### Claim 9 (depends on 8)

A method for preparing the supported catalyst of claim 8, comprising the following steps:
impregnating the spherical alumina as the support with a noble metal salt solution by an incipient wetness impregnation process to obtain a spherical alumina loaded with a noble metal salt; and
subjecting the spherical alumina loaded with the noble metal salt to a second calcination to obtain the supported catalyst.

### Claim 10 (depends on 8)

A method of using the supported catalyst of claim 8, comprising using the supported catalyst in a hydrogenation reaction or a dehydrogenation reaction in a fixed-bed reactor.

### Claim 11 (depends on 6)

The spherical alumina of claim 6, wherein the adhesive comprises one selected from the group consisting of an inorganic acid, formic acid, acetic acid, and citric acid;
a mass ratio of the alumina powder to the adhesive is in a range of 100: 0.5-6; and
a mass ratio of the alumina powder to the water is in a range of 1:0.5-2.0.

### Claim 12 (depends on 6)

The spherical alumina of claim 6, wherein the extrusion is performed by using a single-screw extruder with auto-feed compression; and
the strip-shaped sample has a diameter of not less 0.6 mm.

### Claim 13 (depends on 6)

The spherical alumina of claim 6, wherein the spheronization is performed by placing the strip-shaped sample into a spheronizer and subjecting the strip-shaped sample to spheronization to obtain the spherical particles.

### Claim 14 (depends on 6)

The spherical alumina of claim 6, wherein the first calcination is conducted at a temperature of 500° C. to 600° C. for 3 hours to 6 hours.