# US 2026/0271636 A1 · Method of forming a dielectric layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0271636 A1
- Document ID: US20260271636A1
- Status: Published application
- Kind: A1
- Application number: 19/555,993
- Filed: 2026-03-04
- Published: 2026-09-10
- Earliest claimed: 2025-03-07
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Kamesh Mullapudi
- Web page: https://patentgrep.com/patent/US20260271636A1

## CPC

- H10P 14/6544: {to change the morphology of the insulating materials, e.g. transformation of an amorphous layer into a crystalline layer}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6548: {by forming intermediate materials, e.g. capping layers or diffusion barriers}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P 14/6909: {the material containing hafnium}
- H10P 14/6912: {the material containing zirconium}
- H10P 14/6914: {the material containing two or more metal elements}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Methods for forming a dielectric layer in a feature, where the dielectric layer may be free of voids and/or seams, are disclosed. An exemplary method includes providing a substrate comprising one or more features in a reaction chamber, depositing a dielectric layer in the one or more features, and performing a treatment. The treatment may change the crystal structure from a first crystal structure to a second crystal structure. The treatment may remove voids and/or seams from the dielectric layer.

## Claims

### Claim 1

A method for forming a dielectric layer, the method comprising:
providing a substrate comprising one or more features on a surface of the substrate;
depositing a dielectric layer in the one or more features;
performing a treatment to change a crystal structure of the dielectric layer from a first crystal structure to a second crystal structure, wherein the first crystal structure is different than the second crystal structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein depositing the dielectric layer comprises depositing a dielectric layer with one or more seams or voids, and wherein performing the treatment comprises removing the one or more seams or voids from the dielectric layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second crystal structure is a tetragonal crystal structure.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first crystal structure is a monoclinic crystal structure.

### Claim 5 (depends on 1)

The method of claim 1, wherein an aspect ratio of the one or more features is greater than 25.

### Claim 6 (depends on 1)

The method of claim 1, wherein performing the treatment increases a volume of the dielectric layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein performing the treatment on the dielectric layer increases a volume of the dielectric layer by between about 3% and 7%.

### Claim 8 (depends on 1)

The method of claim 1, wherein depositing the dielectric layer comprises a cyclical deposition process.

### Claim 9 (depends on 1)

The method of claim 1, wherein depositing the dielectric layer comprises a conformal deposition process.

### Claim 10 (depends on 1)

The method of claim 1, wherein the dielectric layer comprises a metal oxide.

### Claim 11 (depends on 1)

The method of claim 1, wherein the dielectric layer comprises one or more of a hafnium, zirconium, aluminum, titanium, scandium, yttrium, lanthanum, tantalum, and niobium.

### Claim 12 (depends on 1)

The method of claim 1, wherein the dielectric layer comprises one or more HfO2, ZrO2, and HfZrO4.

### Claim 13 (depends on 1)

The method of claim 1, wherein the dielectric layer comprises between 0.1 at % and 5 at % dopant, wherein the dopant comprises yttrium, magnesium, cerium, or aluminum.

### Claim 14

A method for forming a dielectric layer, the method comprising:
providing a substrate comprising one or more features on a surface of the substrate;
depositing a dielectric layer in the one or more features, wherein the dielectric layer comprises one or more seams or voids; and
treating the dielectric layer, wherein treating the dielectrics layer removes the one or more seams or voids,
wherein treating the dielectric layer comprises heating the substrate to a temperature between about 350° C. and about 450° C., or providing an inert gas at a temperature above 300° C. and a pressure between about 0.1 Torr and 60 Torr, exposing the substrate to a reactive plasma, laser annealing the dielectric layer, or forming a stress layer directly on the dielectric layer, wherein the stress layer has a different lattice constant that the dielectric layer.

### Claim 15 (depends on 14)

The method of claim 14, wherein treating the dielectric layer comprises heating the substrate to a temperature between about 350° C. and about 450° C.

### Claim 16 (depends on 14)

The method of claim 14, treating the dielectric layer comprises forming the stress layer directly on the dielectric layer, wherein the stress layer comprises one or more of boron nitride, aluminum nitride, silicon carbide, indium nitride, titanium nitride, germanium, and magnesium oxide.

### Claim 17 (depends on 14)

The method of claim 14, wherein treating the dielectric layer comprises forming the stress layer directly on the dielectric layer.

### Claim 18 (depends on 17)

The method of claim 17, further comprising removing the stress layer.

### Claim 19 (depends on 14)

The method of claim 14, wherein treating the dielectric layer changes a crystal structure of the dielectric layer from a first crystal structure to a second crystal structure.

### Claim 20

A method for removing one or more voids or seams from a dielectric layer, the method comprising:
providing a substrate comprising the dielectric layer in one or more features on a surface of the substrate wherein the dielectric layer comprises one or more seams or voids; and
treating the dielectric layer, wherein treating the dielectric layer changes a crystal structure of the dielectric layer form a first crystal structure to a second crystal structure and removes the one or more seams or voids,
wherein treating the dielectric layer comprises heating the substrate to a temperature between about 350° C. and about 450° C., or providing an inert gas at a above 300° C. and a pressure between about 0.1 Torr and 60 Torr, exposing the substrate to a reactive plasma, laser annealing the dielectric layer, or forming a stress layer directly on the dielectric layer, wherein the stress layer has a different lattice constant that the dielectric layer.