# US 2026/0265946 A1 · Method for simultaneously producing multiple sheets of sic single crystal substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265946 A1
- Document ID: US20260265946A1
- Status: Published application
- Kind: A1
- Application number: 19/662,291
- Filed: 2026-04-29
- Published: 2026-09-10
- Earliest claimed: 2024-07-29
- Assignees: NGK Corporation
- Applicants: NGK Corporation
- Inventors: Yohei OKADA; Kiyoshi MATSUSHIMA; Jun YOSHIKAWA
- Web page: https://patentgrep.com/patent/US20260265946A1

## CPC

- C30B 17/00: Single-crystal growth onto a seed which remains in the melt during growth, e.g. Nacken-Kyropoulos method (C30B15/00 takes precedence)
- C30B 19/02: using molten solvents, e.g. flux
- C30B 19/04: the solvent being a component of the crystal composition
- C30B 23/025: {characterised by the substrate}
- C30B 29/22: Complex oxides
- C30B 29/36: Carbides
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

There is provided a method capable of simultaneously manufacturing multiple SiC single crystal substrates including: preparing multiple containers; placing, in each of the multiple containers, an SiC single crystal serving as a seed crystal and an SiC mixed powder containing SiC powder and a liquid phase sintering aid so as to form an SiC mixed powder layer in which the SiC mixed powder is in contact with the SiC single crystal, wherein the liquid phase sintering aid contains an oxide; arranging the multiple containers in a firing furnace so as to be aligned horizontally and/or vertically; and heating the inside of the firing furnace to form a temperature gradient, and subjecting the multiple containers containing the seed crystal and the SiC mixed powder to heat treatment at an average furnace temperature of 2,240 to 2,560° C., whereby an SiC single crystal is grown on the seed crystal.

## Claims

### Claim 1

A method for simultaneously manufacturing multiple SiC single crystal substrates, the method comprising:
preparing a plurality of containers;
placing, in each of the plurality of containers, an SiC single crystal serving as a seed crystal and an SiC mixed powder comprising SiC powder and a liquid phase sintering aid so as to form an SiC mixed powder layer in which the SiC mixed powder is in contact with at least one surface of the SiC single crystal, wherein the liquid phase sintering aid comprises an oxide;
arranging the plurality of containers in a firing furnace so as to be aligned horizontally and/or vertically; and
heating the inside of the firing furnace to form a temperature gradient in which the temperature increases or decreases from an upper part to a lower part of the firing furnace, and subjecting the plurality of containers containing the seed crystal and the SiC mixed powder to heat treatment at an average furnace temperature of 2,240 to 2,560° C., whereby an SiC single crystal is grown on the seed crystal.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the oxide comprises a rare earth element.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the content of the oxide is 0.5 to 33.0% by weight relative to the content of the SiC powder.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the average furnace temperature during the heat treatment is 2,370 to 2,515° C.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the temperature gradient is 0.01 to 0.40° C./mm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the heat treatment is performed while providing a temperature gradient such that the temperature on the side of the container closer to the seed crystal is lower than that on the side of the container closer to the SiC mixed powder layer.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the number of the containers is 2 to 80.

### Claim 8 (depends on 2)

The method according to claim 2, wherein the rare earth element comprises at least one selected from the group consisting of Gd, Sm, La, Nd, Y, and Ce.

### Claim 9 (depends on 1)

The method according to claim 1, wherein a dense body having a relative density of 90% or more is placed on the bottom surface and/or the top surface of the SiC mixed powder layer, excluding the surface in contact with the seed crystal.

### Claim 10 (depends on 1)

The method according to claim 1, wherein a dense body having a relative density of 90% or more is placed on the outer periphery of the SiC mixed powder layer.

### Claim 11 (depends on 1)

The method according to claim 1, wherein a dense body having a relative density of 90% or more is placed on the bottom surface and/or the top surface of the SiC mixed powder layer, excluding the surface in contact with the seed crystal, and a dense body having a relative density of 90% or more is also placed on the outer periphery of the SiC mixed powder layer.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the firing furnace comprises an upper heater at the upper part of the firing furnace and a lower heater at the lower part of the firing furnace, and during the heat treatment, the upper heater and the lower heater are set to different temperatures so as to provide the temperature gradient and the average furnace temperature.