# US 2026/0265878 A1 · Non-oriented silicon steel palte and production method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265878 A1
- Document ID: US20260265878A1
- Status: Published application
- Kind: A1
- Application number: 18/993,957
- Filed: 2023-11-08
- Published: 2026-09-10
- Earliest claimed: 2022-11-11
- Assignees: Zhangjiagang Yangtze River Cold Rolled Plate Co. Ltd; Institute of Research of Iron and Steel, Jiangsu Province/Sha-Steel, Co. Ltd (Cn); Jiangsu Shagang Group Co., Ltd.
- Applicants: Zhangjiagang Yangtze River Cold Rolled Plate Co. Ltd; Institute of Research of Iron and Steel, Jiangsu Province/Sha-Steel, Co. Ltd (Cn); Jiangsu Shagang Group Co., Ltd.
- Inventors: Jie HUANG; Shishu XIE; Chongxiang YUE; Jiadong LU
- Web page: https://patentgrep.com/patent/US20260265878A1

## CPC

- C22C 38/02: containing silicon
- C21D 1/26: Methods of annealing
- C21D 1/74: Methods of treatment in inert gas, controlled atmosphere, vacuum or pulverulent material
- C21D 1/76: Adjusting the composition of the atmosphere
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 8/0284: {Application of a separating or insulating coating}
- C21D 8/12: during manufacturing of articles with special electromagnetic properties
- C21D 8/1222: {Hot rolling}
- C21D 8/1233: {Cold rolling}
- C21D 8/1244: characterised by the heat treatment
- C21D 8/1255: {with diffusion of elements, e.g. decarburising, nitriding}
- C21D 8/1261: {following hot rolling}
- C21D 8/1272: {Final recrystallisation annealing}
- C21D 8/1283: {Application of a separating or insulating coating}
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- H01F 1/14775: {in the form of sheets}
- H01F 1/14791: {Fe-Si-Al based alloys, e.g. Sendust}
- Y02P 10/20: Recycling
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A non-oriented silicon steel plate and a production method therefor. The content of Si and the content of Al in non-oriented silicon steel are finely regulated and controlled on the basis of the value of (Si/Al)/(Si+Al), and a production process is accurately controlled, so that texture optimization of a silicon steel substrate is promoted, iron loss after secondary annealing is reduced, and thus the loss of a motor product is remarkably reduced. Moreover, the total amount of Si and Al added in the non-oriented silicon steel plate is low, so that the alloy cost is low, and the production process is simple. Therefore, the comprehensive cost of the non-oriented silicon steel plate is relatively low, and the product has better market competitiveness.

## Claims

### Claim 1

A production method for a non-oriented silicon steel plate, wherein:
chemical components of the non-oriented silicon steel composition comprise the following components in mass percentage: C≤0.005%, Si: 0.60~1.60%, Al: 0.40~0.80%, Mn: 0.20~0.80%, S≤0.003%, N≤0.003%, and the balance of Fe and other inevitable impurities; and the contents of Si and Al satisfy the following formula:
0.83
≤
S
⁢
i
Al
S
⁢
i
+
Al
≤
1.67
where the element symbols represent the mass percentages of the respective elements;
the production method comprises the following steps:
smelting and casting according to the above chemical components to obtain an slab;
heating the slab, and performing a hot rolling process on the slab after heating to obtain a hot rolled plate;
performing a cold rolling process on the hot rolled plate to obtain a cold rolled plate;
performing a recrystallization annealing process on the cold rolled plate to obtain a first annealed steel plate, wherein the recrystallization annealing temperature is controlled to be 800~950° C., and the holding time is controlled to be 50~200s;
performing a secondary annealing process on the first annealed steel plate to obtain a second annealed steel plate, wherein the secondary annealing temperature is controlled to be 750~850° C., and the holding time is controlled to be 1~3h.

### Claim 2 (depends on 1)

The production method for a non-oriented silicon steel plate according to claim 1, wherein heating the slab specifically comprises:
heating the slab to a temperature range of 1050~1200° C., controlling the heating time to be 150~200 min, and controlling the temperature fluctuation to be within ±20° C.

### Claim 3 (depends on 2)

The production method for a non-oriented silicon steel plate according to claim 2, wherein performing a hot rolling process on the slab after heating to obtain a hot rolled plate specifically comprises:
controlling the hot rolling start temperature to be ≤1200° C., controlling the finish rolling temperature to be ≥840° C., and controlling the finish rolling temperature fluctuation to be within ±20° C.

### Claim 4 (depends on 3)

The production method for a non-oriented silicon steel plate according to claim 3, wherein performing a hot rolling process on the slab after heating to obtain a hot rolled plate further comprises:
after obtaining the hot rolled plate, performing laminar flow cooling on the hot rolled plate and then coiling, and controlling the coiling temperature to be ≤700° C., with the coiling temperature fluctuation controlled to be within =20° C.

### Claim 5 (depends on 1)

The production method for a non-oriented silicon steel plate according to claim 1, wherein performing a cold rolling process on the hot rolled plate to obtain a cold rolled plate specifically comprises:
cold rolling the hot rolled plate to form a cold rolled plate with a thickness of 0.47~0.51 mm.

### Claim 6 (depends on 1)

The production method for a non-oriented silicon steel plate according to claim 1, wherein after performing the recrystallization annealing process on the cold rolled plate to obtain a first annealed steel plate, the method further comprises:
coating an insulating coating on the surface of the first annealed steel plate.

### Claim 7 (depends on 1)

The production method for a non-oriented silicon steel plate according to claim 1, wherein the recrystallization annealing process on the cold rolled plate is performed in a hydrogen-nitrogen protective atmosphere; and the secondary annealing process on the first annealed steel plate is performed in a nitrogen gas or DX gas protective atmosphere.

### Claim 8

A non-oriented silicon steel plate, wherein chemical components of the non-oriented silicon steel composition comprise the following components in mass percentage: C≤0.005%, Si: 0.60~1.60%, Al: 0.40~0.80%, Mn: 0.20~0.80%, S≤0.003%, N≤0.003%, and the balance of Fe and other inevitable impurities; and the contents of Si and Al satisfy the following formula:
0.83
≤
S
⁢
i
Al
S
⁢
i
+
Al
≤
1.67
where the element symbols represent the mass percentages of the respective elements;
the non-oriented silicon steel plate has an iron loss reduction rate ΔP15/50/P15/50 of more than 15%.