# US 2026/0265869 A1 · TiAl-BASED ALLOY AND METHOD FOR PRODUCING THE SAME

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265869 A1
- Document ID: US20260265869A1
- Status: Published application
- Kind: A1
- Application number: 19/162,405
- Filed: 2024-02-28
- Published: 2026-09-10
- Earliest claimed: 2023-03-07
- Assignees: Mitsubishi Heavy Industries Aero Engines, Ltd.; Institute of Science Tokyo; Osaka Yakin Kogyo Co., Ltd.
- Applicants: Mitsubishi Heavy Industries Aero Engines, Ltd.; Institute of Science Tokyo; Osaka Yakin Kogyo Co., Ltd.
- Inventors: Shintaro SOBU; Kentaro SHINDO; Akira FUKUSHIMA; Masao TAKEYAMA; Hirotoyo NAKASHIMA; Ryosuke YAMAGATA; Kazuki HANAMI; Kenji DOI; Yasuhiro IWASA
- Web page: https://patentgrep.com/patent/US20260265869A1

## CPC

- C22C 14/00: Alloys based on titanium
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- C22C 1/0416: {Aluminium-based alloys}
- C22C 1/0458: {Alloys based on titanium, zirconium or hafnium}
- C22C 21/003: {containing at least 2.6% of one or more of the elements: tin, lead, antimony, bismuth, cadmium, and titanium}
- C22F 1/002: {by rapid cooling or quenching; cooling agents used therefor}
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/183: {of titanium or alloys based thereon}
- B22F 3/225: {by injection molding}
- B22F 10/64: by thermal means (control of energy beam parameters for post heating B22F10/364)
- B22F 2003/1051: {by electric discharge}
- B22F 2003/248: {Thermal after-treatment}
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING

## Abstract

A TiAl-based alloy includes, in atomic percent, Al: 45% to 49%, β-stabilizing elements: 3% to 11%, Ni: ≤1.0%, C: ≤0.6%, Si: ≤0.5%, O: ≤1.5%, the balance being Ti and inevitable impurities, in which the β-stabilizing elements are any of Cr, Nb, V, Mn and Mo or a combination thereof, the metal structure comprises (α2/γ) lamellar grains and a cellular structure or a secondary lamellar structure precipitated at (α2/γ) lamellar grain boundaries, the cellular structure is a (β/γ) cellular structure or an (α2/γ/β) cellular structure, the secondary lamellar structure has (α2/γ) lamellar grains having a grain diameter smaller than that of the (α2/γ) lamellar grains, and a volume fraction of the cellular structure or the secondary lamellar structure is 1 vol % or more and 50 vol % or less.

## Claims

### Claim 1

A TiAl-based alloy comprising, in atomic percent, Al: 45% to 49%, β-stabilizing elements: 3% to 11%, Ni: ≤1.0%, C: ≤0.6%, Si: ≤0.5%, O: ≤1.5%, the balance being Ti and inevitable impurities, the β-stabilizing elements being any of Cr, Nb, V, Mn and Mo or a combination thereof,
wherein the TiAl-based alloy has a metal structure comprising (α2/γ) lamellar grains and a cellular structure or a secondary lamellar structure precipitated at (α2/γ) lamellar grain boundaries,
the cellular structure is a (β/γ) cellular structure or an (α2/γ/β) cellular structure,
the secondary lamellar structure has (α2/γ) lamellar grains having a grain diameter smaller than that of the (α2/γ) lamellar grain, and
a volume fraction of the cellular structure or the secondary lamellar structure is 1 vol % or more and 50 vol % or less.

### Claim 2 (depends on 1)

The TiAl-based alloy according to claim 1,
wherein the metal structure comprises other constituent phases,
the other constituent phases comprise massive γ phases, and
the volume fraction of the other constituent phases is 30 vol % or less.

### Claim 3

A method for producing a TiAl-based alloy, wherein the TiAl-based alloy is held at a first temperature for a predetermined period of time in an (α+γ) two-phase region, an α single-phase region, a (β+α) two-phase region, or a (β+α+γ) three-phase region, then the TiAl-based alloy is quenched at a cooling rate equal to or higher than air cooling, and the quenched TiAl-based alloy is held at a second temperature for a predetermined period of time in a (β+γ) two-phase region, a (β+α2+γ) three-phase region, or an (α2+γ) two-phase region to form a metal structure comprising (α2/γ) lamellar grains and a cellular structure or a secondary lamellar structure precipitated at (α2/γ) lamellar grain boundaries, and wherein
the second temperature and a holding time at the second temperature are controlled so that the cellular structure is a (β/γ) cellular structure or an (α2/γ/β) cellular structure;
the secondary lamellar structure has (α2/γ) lamellar grains finer than the (α2/γ) lamellar grains; and
a volume fraction of the cellular structure or the secondary lamellar structure is 1 vol % or more and 50 vol % or less, the TiAl-based alloy containing, in atomic percent, Al: 45% to 49%, β-stabilizing elements: 3% to 11%, Ni: ≤1.0%, C: ≤0.6%, Si: ≤0.5%, O: ≤1.5%, the balance being Ti and inevitable impurities, the β-stabilizing elements being any of Cr, Nb, V, Mn and Mo or a combination thereof.

### Claim 4 (depends on 3)

The method for producing a TiAl-based alloy according to claim 3,
wherein the metal structure comprises other constituent phases,
the other constituent phases comprise massive γ phases, and
the first temperature, a holding time at the first temperature, and the cooling rate are controlled such that a volume fraction of the other constituent phases is 30 vol % or less.