# US 2026/0265859 A1 · Method for the recovery of metals from e-waste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265859 A1
- Document ID: US20260265859A1
- Status: Published application
- Kind: A1
- Application number: 19/473,653
- Filed: 2024-03-27
- Published: 2026-09-10
- Earliest claimed: 2023-04-11
- Assignees: Renewable Metals Pty Ltd
- Applicants: Renewable Metals Pty Ltd
- Inventors: Mark Daniel URBANI
- Web page: https://patentgrep.com/patent/US20260265859A1

## CPC

- C22B 7/008: {by an alkaline or ammoniacal leaching}
- C01D 15/06: Sulfates; Sulfites
- C01G 45/024: Manganese dioxide
- C01G 45/026: Dimanganese trioxide
- C01G 45/028: Trimanganese tetraoxide
- C22B 3/24: by adsorption on solid substances, e.g. by extraction with solid resins
- C22B 3/30: Oximes
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 7/005: {Separation by a physical processing technique only, e.g. by mechanical breaking}
- C22B 15/0071: {containing sulfur}
- C22B 15/0078: {with ammoniacal solutions, e.g. ammonium hydroxide}
- C22B 15/0086: {by physical methods}
- C22B 15/0089: {by chemical methods}
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0446: {with an ammoniacal liquor or with a hydroxide of an alkali or alkaline-earth metal}
- C22B 23/0461: {by chemical methods}
- C22B 23/0476: {Separation of nickel from cobalt}
- C22B 26/12: Obtaining lithium
- C22B 47/00: Obtaining manganese
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Disclosed herein is a method of recovering metals from a leachate of an alkaline leach of electronic waste, the leachate including Cu, Li, and Mn ions, the method including recovering Mn from the leachate; after the step of recovering Mn from the leachate, recovering Cu from the leachate; and after the step of recovering Cu from the leachate, recovering Li from the leachate.

## Claims

### Claim 1

A method of recovering metals from a leachate of an alkaline leach of electronic waste, the leachate comprising Cu, Li, and Mn ions, the method comprising:
recovering Mn from the leachate;
after the step of recovering Mn from the leachate, recovering Cu from the leachate; and
after the step of recovering Cu from the leachate, recovering Li from the leachate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the leachate additionally comprises Co ions, and after the step of recovering Cu from the leachate and prior to the step of recovering Li from the leachate, the method further comprises recovering Co from the leachate.

### Claim 3

A method of recovering metals from a leachate of an alkaline leach of electronic waste, the leachate comprising Cu, Li, Ni, and Mn ions, the method comprising:
recovering Mn from the leachate;
after the step of recovering Mn from the leachate, recovering Cu and Ni from the leachate; and
after the step of recovering Cu and Ni from the leachate, recovering Li from the leachate.

### Claim 4 (depends on 2)

The method of claim 2, wherein the leachate additionally comprises Co ions, and after the step of recovering Cu and Ni from the leachate and prior to the step of recovering Li from the leachate, the method further comprises recovering Co from the leachate.

### Claim 5 (depends on 1)

The method of claim 1, wherein the step of recovering Mn from the leachate comprises:
treating the leachate with an oxidant to form a Mn precipitate, and
separating the Mn precipitate from the leachate.

### Claim 6 (depends on 5)

The method of claim 5, wherein the oxidant is selected from a group consisting of air, hydrogen peroxide, and hypochlorite.

### Claim 7 (depends on 5)

The method of claim 5, wherein the Mn precipitate is a manganese oxide selected from a group consisting of Mn2O3, Mn3O4, and MnO2.

### Claim 8 (depends on 1)

The method of claim 1, wherein the step of recovering Li from the leachate comprises:
crystallising ammonium lithium sulfate from the leachate, and
separating crystallised ammonium lithium sulfate from the leachate.

### Claim 9 (depends on 8)

The method of claim 8, further comprising thermally decomposing the crystallised ammonium lithium sulfate to form a gas comprising ammonia and sulfur oxides, and solid lithium sulfate.

### Claim 10 (depends on 1)

The method of claim 1, wherein the step of recovering Cu ions from the leachate uses a solvent extraction process, the solvent extraction process comprising:
contacting the leachate with an extractant to adsorb Cu ions into the extractant to form a Cu-loaded extractant, and
separating the Cu-loaded extractant from the leachate.

### Claim 11 (depends on 10)

The method of claim 10, wherein the method further comprises stripping the Cu ions from the Cu-loaded extractant.

### Claim 12 (depends on 2)

The method of claim 2, wherein the step of recovering Cu and Ni ions from the leachate comprises contemporaneously recovering Cu and Ni ions with a solvent extraction process, the solvent extraction process comprising:
contacting the leachate with an extractant to adsorb Cu and Ni ions into the extractant to form a Cu-, Ni-loaded extractant, and
separating the Cu-, Ni-loaded extractant from the leachate.

### Claim 13 (depends on 12)

The method of claim 12, wherein the method further comprises stripping the Cu and Ni ions from the Cu-, Ni-loaded extractant using a stripping agent, wherein Ni ions are selectively recovered at a first stripping agent concentration and Cu ions are subsequently recovered at a second stripping agent concentration, the first stripping agent concentration being less than the second stripping agent concentration.

### Claim 14 (depends on 3)

The method of claim 3, wherein prior to the step of recovering Cu the method further comprises treating the leachate with an oxidant to oxidise Co ions from Co2+ to Co3+.

### Claim 15 (depends on 4)

The method of claim 4, wherein prior to the step of recovering Cu and Ni the method further comprises treating the leachate with an oxidant to oxidise Co ions from Co2+ to Co3+.

### Claim 16 (depends on 2)

The method of any one of claims 2, wherein the step of recovering Co from the leachate comprises:
treating the leachate with a precipitant to form a Co precipitate; and
separating the Co precipitate from the leachate.

### Claim 17 (depends on 1)

The method of claim 1, wherein the leachate comprises ammonium sulfate and ammonia.

### Claim 18 (depends on 1)

The method of claim 1, wherein:
the leachate has an initial pH in the range of from about 8.5 up to 10.5; and/or
during one or more or each of the recovery steps the leachate has a pH in the range of from about 8.5 to 10.5.

### Claim 19 (depends on 1)

The method of claim 1, wherein the leach solution comprises ammonia and ammonium sulfate in a ratio of from about 1:2 to about 1:20.

### Claim 20 (depends on 1)

The method of claim 1, wherein:
the leachate has a Cu:Mn ratio of from about 0.5:1 up to about 2:1; or
the leachate has a Cu:(Mn+Co) ratio of from about 0.5:1 up to about 2:1; or
the leachate has a Cu:(Mn+Ni) ratio of from about 0.5:1 up to about 2:1; or
the leachate has a Cu:(Mn+Co+Ni) ratio of from about 0.5:1 up to about 2:1.