# US 2026/0265603 A1 · Method for injecting an aqueous polymer solution into an underground formation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265603 A1
- Document ID: US20260265603A1
- Status: Published application
- Kind: A1
- Application number: 19/164,975
- Filed: 2024-03-13
- Published: 2026-09-10
- Earliest claimed: 2023-03-14
- Assignees: Snf Group
- Applicants: SNF Group
- Inventors: Cédrick FAVERO
- Web page: https://patentgrep.com/patent/US20260265603A1

## CPC

- C09K 8/68: containing organic compounds
- C08F 120/56: Acrylamide; Methacrylamide
- C09K 8/588: characterised by the use of specific polymers {(polymeric surfactants C09K8/584)}
- C09K 8/665: {containing inorganic compounds (proppants C09K8/80)}
- C09K 8/885: {obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present invention relates to a method for injecting an aqueous solution of a 2-acrylamido-2-methylpropanesulfonate homopolymer P and/or its salts having an average molecular weight greater than 1 million daltons, said method comprising the following successive steps: in a location A: preparation in a mobile unit U1 of sodium 2-acrylamido-2-methylpropanesulfonate in crystalline form (AMPS.S), collection of an AMPS.OS sodium 2-acrylamido-2-methylpropanesulfonate aqueous solution S1, coming from the purge of the preparation of the AMPS.s in the mobile unit U1, in a location A′: preparation in a mobile unit U3 of a homopolymer P by gel polymerisation of an AMPS.S aqueous solution S3, dissolution in a mobile unit U4 of the polymer P in a saline solution SS1 to obtain a polymer P solution SM, transfer of the solution SM from the location A′ to a location B, in the location B: dilution in a mobile unit U5 of the solution SM by a saline solution SS2 to obtain a solution SF, injection of the solution SF in the underground formation for the assisted extraction of hydrocarbons or hydraulic fracturing.

## Claims

### Claim 1

A method for injecting a sodium or potassium or ammonium 2-acrylomido-2-methylpropanesulfonate homopolymer P aqueous solution and/or its salts, the homopolymer P having an average molecular weight by weight greater than 1 million daltons, the homopolymer P aqueous solution being injected into an underground formation for the assisted extraction of hydrocarbons or hydraulic fracturing, said method comprising the following successive steps:
in a location A:
preparing, in a mobile unit U1, of sodium or potassium or ammonium 2-acrylamido-2-methylpropanesulfonate in crystalline form (AMPS.S),
sodium 2-acrylamido-2-methylpropanesulfonate in crystalline form having a powder X-ray diffraction pattern comprising peaks at 11.70°; 12.20°; 13.2°; 13.5°; 15.60°; 16.80°; 17.80°; 18.5°; 19.1°; 20.6°; 21.4°; 23.3°; 25.1°; 25.8°; 26.9°; 29.10°; 29.50°; 31.0°; 33°; 33.6°; 34.4°; 35.2°; 35.9°; 37.1°; 38.4°; 39.6°; 41.10°; 42.90°; 45.10°; 46.0°; 47.2°; 47.6°, 2-theta degrees,
potassium 2-acrylamido-2-methylpropanesulfonate in crystalline form having a powder X-ray diffraction pattern comprising peaks at 13.10°; 14.4°; 16.3°; 19.8°; 23.50°; 24.3°; 26.9°; 27.6°; 29.3°; 30.6°; 31.6°; 34.3°; 36.1°; 41.7°; 44.6°; 46.7°, degrees 2-theta,
ammonium 2-acrylamido-2-methylpropanesulfonate in crystalline form having a powder X-ray diffraction pattern comprising peaks at 10.10°; 13.10°; 13.2°; 17.5°; 15.60°; 18.10°; 19.50°; 20.0°; 21.4°; 22.8°; 23.6°; 24.8°; 25.1°; 25.8°; 26.2°; 27.4°; 28.10°; 29.4°; 30.2°; 30.8°; 32.0°; 32.9°; 33.2°; 33.9°; 34.4°; 35.0°; 36.2°; 37.7°; 38.8°; 39.6°; 40.4°; 41.4°; 41.9°; 42.8°; 43.5°; 44.8°; 45.5°; 45.7°; 46.5°; 47.0°; 47.4°, degrees 2-theta,
collecting of an aqueous solution S1 of sodium or potassium or ammonium 2-acrylamido-2-methylpropanesulfonate AMPS.OS, coming from the purge of the AMPS.S preparation in the mobile unit U1,
polymerizing, in a unit U2, the AMPS.OS solution S1 collected in the mobile unit U1 to obtain a polymer P′ aqueous solution S2,
transferring by pipes the solution S2 from unit U2 of location A to a mobile unit U3 of a location A′,
in the location A′:
preparing, in a mobile unit U3, a composition CA′ containing an AMPS.S solution S3 and at least some of the polymer P′ solution S2, the mass ratio [P′]/[AMPS.S] being of between 0.05 and 0.20, with [P′] concentration by weight of polymer P′ in the composition CA′ and [AMPS.S] concentration by weight of AMPS.S in the composition CA′,
preparing, in the mobile unit U3, a homopolymer P by gel polymerisation of AMPS.S aqueous solution S3 in composition CA′,
dissolving, in a mobile unit U4, the polymer P in a saline solution SS1 containing at least 1 g/L of alkaline and/or alkaline earth salts in water to obtain a polymer P solution SM,
transferring the solution SM from the location A′ to a location B,
in the location B:
diluting, in a mobile unit U5, of at least a factor 4 and as a maximum a factor 60 of the solution SM by a saline solution SS2 containing at least 1 g/L of alkaline and/or alkaline earth salts in water to obtain a solution SF containing less than 0.6% by weight of polymer P, and
injecting of the solution SF into the underground formation.

### Claim 2 (depends on 1)

The method according to claim 1, characterised in that the locations A and A′ overlap or are contiguous.

### Claim 3 (depends on 1)

The method according to claim 1, characterised in that the transfer of the solution SM from the location A′ to the location B is done by pipes or by transport units.

### Claim 4 (depends on 1)

The method according to claim 1, characterised in that the AMPS.S is prepared by purification of 2-acrylamido-2-methylpropane sulfonic acid previously stored in the location A in a mobile storage unit.

### Claim 5 (depends on 1)

The method according to claim 1, characterised in that at the end of preparing the polymer P by gel polymerisation of the AMPS.S solution S3 in composition CA′ in the mobile unit U3, the polymer P gel obtained is granulated in a granulation unit to obtain polymer P gel pieces, which are directly dissolved in the saline solution containing at least 1 g/L of alkaline and/or alkaline earth salts to obtain the solution SM in the mobile unit U4.

### Claim 6 (depends on 1)

The method according claim 1, characterised in that the polymerisation of the polymer P in the mobile unit U3 is initiated in the presence of glucose oxidase.

### Claim 7 (depends on 1)

The method according to claim 1, characterised in that the solution SM at the location A′ is stored in a maturation and storage unit before being transferred to the location B.

### Claim 8 (depends on 1)

The method according to claim 1, characterised in that the polymerisation of the AMPS.S solution S3 in composition CA′ in the mobile unit U3 is done with an initial concentration of AMPS.S in the solution S3 greater than 20% by weight.

### Claim 9 (depends on 1)

The method according to claim 1, characterised in that the final temperature of the polymerisation of the AMPS.S solution S3 in composition CA′ in the mobile unit U3 is greater than 80° C.

### Claim 10 (depends on 1)

The method according to claim 1, characterised in that the injection of the solution SF into the underground formation is followed by a step of recovering hydrocarbons by assisted extraction by sweeping the underground formation by means of the solution SF.

### Claim 11 (depends on 1)

The method according to claim 1, characterised in that the injection of the solution SF in the underground formation is followed by a step of recovering hydrocarbons by hydraulic fracturing of the underground formation by means of the solution SF.

### Claim 12 (depends on 3)

The method according to claim 3, characterised in that the polymer P′ has an average molecular weight by weight of between 500 and 500000 Daltons.

### Claim 13 (depends on 2)

The method according to claim 2, characterised in that the transfer of the solution SM from the location A′ to the location B is done by pipes or by transport units.

### Claim 14 (depends on 2)

The method according to claim 2, characterised in that the AMPS.S is prepared by purification of 2-acrylamido-2-methylpropane sulfonic acid previously stored in the location A in a mobile storage unit.

### Claim 15 (depends on 3)

The method according to claim 3, characterised in that the AMPS.S is prepared by purification of 2-acrylamido-2-methylpropane sulfonic acid previously stored in the location A in a mobile storage unit.

### Claim 16 (depends on 2)

The method according to claim 2, characterised in that at the end of preparing the polymer P by gel polymerisation of the AMPS.S solution S3 in composition CA′ in the mobile unit U3, the polymer P gel obtained is granulated in a granulation unit to obtain polymer P gel pieces, which are directly dissolved in the saline solution containing at least 1 g/L of alkaline and/or alkaline earth salts to obtain the solution SM in the mobile unit U4.

### Claim 17 (depends on 16)

The method according claim 16, characterised in that the polymerisation of the polymer P in the mobile unit U3 is initiated in the presence of glucose oxidase.

### Claim 18 (depends on 17)

The method according to claim 17, characterised in that the solution SM at the location A′ is stored in a maturation and storage unit before being transferred to the location B.

### Claim 19 (depends on 18)

The method according to claim 18, characterised in that the polymerisation of the AMPS.S solution S3 in composition CA′ in the mobile unit U3 is done with an initial concentration of AMPS.S in the solution S3 greater than 20% by weight.

### Claim 20 (depends on 5)

The method according to claim 5, characterised in that the polymer P′ has an average molecular weight by weight of between 500 and 500000 Daltons.