# US 2026/0265565 A1 · Mixed ink, production method for same, and production method for sintered body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265565 A1
- Document ID: US20260265565A1
- Status: Published application
- Kind: A1
- Application number: 19/166,988
- Filed: 2024-03-18
- Published: 2026-09-10
- Earliest claimed: 2023-03-30
- Assignees: Mitsui Mining & Smelting Co., Ltd.; Kansai University
- Applicants: Mitsui Mining & Smelting Co., Ltd.; Kansai University
- Inventors: Mitsuhiko NISHINO; Hiroki SAWAMOTO; Takafumi SAKAKI; Rika OOGAMI; Hideya KAWASAKI
- Web page: https://patentgrep.com/patent/US20260265565A1

## CPC

- C09D 11/52: Electrically conductive inks
- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 1/068: Flake-like particles
- B22F 1/10: Metallic powder containing lubricating or binding agents; Metallic powder containing organic material
- B22F 3/10: Sintering only
- B22F 9/00: Making metallic powder or suspensions thereof
- C09D 11/03: characterised by features other than the chemical nature of the binder
- C09D 11/033: characterised by the solvent
- C09D 11/037: characterised by the pigment
- C09D 11/04: based on proteins
- C09D 11/106: containing macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds
- C09D 11/322: Pigment inks
- C09D 11/36: based on non-aqueous solvents
- C09D 11/38: characterised by non-macromolecular additives other than solvents, pigments or dyes
- C22C 9/06: with nickel or cobalt as the next major constituent
- H01B 1/12: organic substances {(organic macromolecular compounds or compositions C08)}
- H01B 1/22: the conductive material comprising metals or alloys
- H01B 13/00: Apparatus or processes specially adapted for manufacturing conductors or cables
- B22F 2301/10: Copper
- B22F 2302/45: Others, including non-metals
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

A mixed ink contains copper microparticles and a nickel formate complex having an ammine ligand or an amino group-containing ligand containing an amino group. The copper microparticles have a volume-based cumulative particle size D50 of 1.5 μm or more and 20.0 μm or less at a cumulative volume of 50 vol %, as measured using a laser diffraction/scattering particle size distribution measurement method, and an aspect ratio of 4.0 or more and 20.0 or less or a BET specific surface area of 0.8 m2/g or more and 4.0 m2/g or less. It is preferable that the copper microparticles have a flat shape. It is also preferable that the amino group-containing ligand is at least one selected from the group consisting of 1-amino-2-propanol, ethylenediamine, and 2-amino-1-butanol.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A mixed ink comprising:
copper microparticles; and
a nickel formate complex having an ammine ligand or an amino group-containing ligand containing an amino group,
wherein the copper microparticles have a volume-based cumulative particle size D50 of 1.5 μm or more and 20.0 μm or less at a cumulative volume of 50 vol %, as measured using a laser diffraction/scattering particle size distribution measurement method, and
the copper microparticles have an aspect ratio of 4.0 or more and 20.0 or less.

### Claim 16

A mixed ink comprising:
copper microparticles; and
a nickel formate complex having an ammine ligand or an amino group-containing ligand,
wherein the copper microparticles have a volume-based cumulative particle size D50 of 1.5 μm or more and 20.0 μm or less at a cumulative volume of 50 vol %, as measured using a laser diffraction/scattering particle size distribution measurement method, and
the copper microparticles have a BET specific surface area of 0.8 m2/g or more and 4.0 m2/g or less.

### Claim 17 (depends on 15)

The mixed ink according to claim 15, wherein the copper microparticles have a volume-based cumulative particle size D90 of 2.5 μm or more and 30.0 μm or less at a cumulative volume of 90 vol %, as measured using a laser diffraction/scattering particle size distribution measurement method.

### Claim 18 (depends on 15)

The mixed ink according to claim 15, wherein the copper microparticles have a flat shape.

### Claim 19 (depends on 15)

The mixed ink according to claim 15, wherein the amino group-containing ligand contains a group represented by a formula (1) or (2) below:
wherein, in the formulae (1) and (2), * represents a bond.

### Claim 20 (depends on 15)

The mixed ink according to claim 15, wherein the amino group-containing ligand is represented by a formula (6) below:
wherein, in the formula (6), n represents an integer of 1 or more and 5 or less.

### Claim 21 (depends on 15)

The mixed ink according to claim 15, wherein the amino group-containing ligand is represented by a formula (7) below:
wherein, in the formula (7), n represents an integer of 1 or more and 10 or less.

### Claim 22 (depends on 15)

The mixed ink according to claim 15, wherein the amino group-containing ligand is represented by a formula (8) below:
wherein, in the formula (8), n represents an integer of 1 or more and 5 or less, and R represents CH3 or C2H5.

### Claim 23 (depends on 15)

The mixed ink according to claim 15, wherein the amino group-containing ligand is represented by a formula (9) below:
wherein, in the formula (9), n represents an integer of 1 or more and 5 or less, and R represents H, CH3, or C2H5.

### Claim 24 (depends on 15)

The mixed ink according to claim 15, wherein the amino group-containing ligand comprises at least one selected from the group consisting of 1-amino-2-propanol, ethylenediamine, and 2-amino-1-butanol.

### Claim 25 (depends on 15)

The mixed ink according to claim 15, wherein a ratio of a mass MNi of metallic nickel to a sum of a mass MCu of metallic copper and the mass MNi of the metallic nickel is 3 mass % or more and 40 mass % or less.

### Claim 26 (depends on 15)

A method for producing a sintered body, comprising:
sintering the mixed ink according to claim 15 at a temperature of 200° C. or lower to obtain a sintered body.

### Claim 27

A method for producing a mixed ink, the mixed ink containing
copper microparticles and
a nickel formate complex having an ammine ligand or an amino group-containing ligand containing an amino group,
the method comprising:
preparing a composition by mixing nickel formate, an ammine ligand or an amino group-containing ligand, and a solvent; and
adding copper microparticles to the composition,
wherein the copper microparticles have a volume-based cumulative particle size D50 of 1.5 μm or more and 20.0 μm or less at a cumulative volume of 50 vol %, as measured using a laser diffraction/scattering particle size distribution measurement method, and
the copper microparticles have an aspect ratio of 4.0 or more and 20.0 or less.

### Claim 28

A method for producing a mixed ink, the mixed ink containing
copper microparticles and
a nickel formate complex having an ammine ligand or an amino group-containing ligand containing an amino group,
the method comprising:
preparing a composition by mixing nickel formate, an ammine ligand or an amino group-containing ligand, and a solvent; and
adding copper microparticles to the composition,
wherein the copper microparticles have a volume-based cumulative particle size D50 of 1.5 μm or more and 20.0 μm or less at a cumulative volume of 50 vol %, as measured using a laser diffraction/scattering particle size distribution measurement method, and
the copper microparticles have a BET specific surface area of 0.8 m2/g or more and 4.0 m2/g or less.