# US 2026/0265548 A1 · Compositions and methods for microbiological control in a paper machine coating kitchen

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265548 A1
- Document ID: US20260265548A1
- Status: Published application
- Kind: A1
- Application number: 19/552,383
- Filed: 2026-02-27
- Published: 2026-09-10
- Earliest claimed: 2025-03-05
- Assignees: Ecolab USA Inc.
- Applicants: ECOLAB USA Inc.
- Inventors: Bjorn KAMLIN; Arie Michiel POOS; Jean-Michel MAQUINGHEN; Laura E. RICE; Markus REHMONEN; Bert SIMONS
- Web page: https://patentgrep.com/patent/US20260265548A1

## CPC

- C09D 7/61: inorganic
- A01N 59/00: Biocides, pest repellants or attractants, or plant growth regulators containing elements or inorganic compounds
- A01P 1/00: Disinfectants; Antimicrobial compounds or mixtures thereof
- C12Q 3/00: Condition responsive control processes (apparatus therefor C12M1/36; controlling or regulating in general G05)
- D21H 21/36: Biocidal agents, e.g. fungicidal, bactericidal, insecticidal agents
- G05D 21/02: characterised by the use of electric means
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- A01N: PRESERVATION OF BODIES OF HUMANS OR ANIMALS OR PLANTS OR PARTS THEREOF (preservation of food or foodstuff A23); BIOCIDES, e.g. AS DISINFECTANTS, AS PESTICIDES OR AS HERBICIDES (preparations for medical, dental or toiletry purposes which kill or prevent the growth or proliferation of unwanted organisms A61K); PEST REPELLANTS OR ATTRACTANTS; PLANT GROWTH REGULATORS
- A01P: BIOCIDAL, PEST REPELLANT, PEST ATTRACTANT OR PLANT GROWTH REGULATORY ACTIVITY OF CHEMICAL COMPOUNDS OR PREPARATIONS
- C12Q: MEASURING OR TESTING PROCESSES INVOLVING ENZYMES, NUCLEIC ACIDS OR MICROORGANISMS (immunoassay G01N33/53); COMPOSITIONS OR TEST PAPERS THEREFOR; PROCESSES OF PREPARING SUCH COMPOSITIONS; CONDITION-RESPONSIVE CONTROL IN MICROBIOLOGICAL OR ENZYMOLOGICAL PROCESSES
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- G05D: SYSTEMS FOR CONTROLLING OR REGULATING NON-ELECTRIC VARIABLES

## Abstract

The present disclosure provides compositions and methods for controlling microbiological activity. A method for controlling microbiological activity in a coating slurry and/or a component thereof may include adding a stabilizer, a chlorine source, and water to a reactor, mixing the stabilizer, the chlorine source, and the water in the reactor to form a stabilized chlorine composition, measuring a first pH of the coating slurry and/or the component thereof with a pH sensor and/or measuring a first oxidation-reduction potential (ORP) of the coating slurry and/or the component thereof with an ORP sensor, adding the stabilized chlorine composition to the coating slurry and/or the component thereof via a delivery conduit, and adding additional stabilized chlorine composition to the coating slurry and/or the component thereof via the delivery conduit if the measured first pH and/or first ORP decreases.

## Claims

### Claim 1

A method for controlling microbiological activity in a coating slurry and/or a component thereof, comprising:
adding a stabilizer, a chlorine source, and water to a reactor;
mixing the stabilizer, the chlorine source, and the water in the reactor to form a stabilized chlorine composition;
measuring a first pH of the coating slurry and/or the component thereof with a pH sensor and/or measuring a first oxidation-reduction potential (ORP) of the coating slurry and/or the component thereof with an ORP sensor;
adding the stabilized chlorine composition to the coating slurry and/or the component thereof via a delivery conduit; and
adding additional stabilized chlorine composition to the coating slurry and/or the component thereof via the delivery conduit if the measured first pH and/or first ORP decreases.

### Claim 2 (depends on 1)

The method of claim 1, wherein from about 0.1 wt. % to about 0.5 wt. % of water is added to the coating slurry with the stabilized chlorine.

### Claim 3 (depends on 1)

The method of claim 1, wherein the stabilizer is selected from the group consisting of an ammonium salt, ammonium chloride, ammonium sulphate, ammonium bromide, ammonium carbamate, ammonium hydroxide, ammonia, urea, dimethylhydantoin, and any combination thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the stabilizer comprises an ammonium source and/or a single species of stabilizer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the chlorine source is selected from the group consisting of a hypochlorite, hypochloric acid, electrochemically generated chlorine, and any combination thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the stabilized chlorine composition comprises a weight ratio of chlorine to stabilizer of about 1:1 to about 1:30.

### Claim 7 (depends on 1)

The method of claim 1, wherein the stabilized chlorine comprises monochloramine.

### Claim 8 (depends on 1)

The method of claim 1, further comprising adding a base to the reactor.

### Claim 9 (depends on 1)

The method of claim 1, wherein the stabilized chlorine comprises a pH from about 7 to about 14.

### Claim 10 (depends on 1)

The method of claim 1, wherein the pH sensor and/or the ORP sensor is submerged in the coating slurry and/or the component thereof.

### Claim 11 (depends on 1)

The method of claim 1, wherein a skid comprises the pH sensor and/or ORP sensor.

### Claim 12 (depends on 1)

The method of claim 1, further comprising adding additional stabilized chlorine to the coating slurry and/or the component thereof when the first pH decreases by about 0.5 pH units.

### Claim 13 (depends on 1)

The method of claim 1, further comprising adding additional stabilized chlorine to the coating slurry and/or the component thereof when the first ORP decreases by about 50 mV.

### Claim 14 (depends on 1)

The method of claim 1, further comprising flushing the delivery conduit with water after adding the stabilized chlorine to the coating slurry and/or the component thereof.

### Claim 15 (depends on 1)

The method of claim 1, wherein the component of the coating slurry comprises a calcium carbonate slurry, a clay slurry, a starch slurry, a paint slurry, and any combination thereof.

### Claim 16 (depends on 1)

The method of claim 1, further comprising flushing the reactor with water prior to adding the stabilizer and/or the chlorine source.

### Claim 17 (depends on 1)

The method of claim 1, excluding adding urea, sulfamic acid, ammonium sulfate, an organic biocide, bromine, and/or bromide to the reactor, the coating slurry, and/or the component thereof.

### Claim 18

A method of monitoring and controlling microbiological activity in a coating slurry and/or a component thereof, comprising:
(a) providing a monitoring and controlling unit comprising a controller and a plurality of sensors in communication with the controller, wherein the plurality of sensors includes a pH sensor operable to measure a pH of the coating slurry and/or the component thereof and an ORP sensor operable to measure an ORP of the coating slurry and/or the component thereof;
(b) entering an acceptable range for the pH of the coating slurry and/or the component thereof and the ORP of the coating slurry and/or the component thereof into the controller;
(c) adding a stabilizer, a chlorine source, and water to a reactor;
(d) mixing the stabilizer, the chlorine source, and the water in the reactor;
(e) forming a stabilized chlorine composition in the reactor;
(f) adding the stabilized chlorine composition to the coating slurry and/or the component thereof via a delivery conduit;
(g) transporting a portion of the coating slurry and/or the component thereof via a side stream conduit to an inlet of the monitoring and controlling unit;
(h) measuring the pH and the ORP of the coating slurry and/or the component thereof with the pH sensor and the ORP sensor, respectively;
(i) determining if the measured pH is within the acceptable range entered into the controller in step (b);
(j) determining if the measured ORP is within the acceptable range entered into the controller in step (b);
(k) carrying out a corrective action if the measured pH and/or ORP is outside of the acceptable range entered into the controller in step (b); and
(l) optionally repeating one or more of steps (a) to (k) to determine if the pH and/or ORP of the coating slurry and/or the component thereof has been brought within the acceptable range entered in step (b).

### Claim 19 (depends on 18)

The method of claim 18, wherein the acceptable range for the pH of the coating slurry and/or the component thereof is from about 6 to about 11 and/or wherein the acceptable range for the ORP of the coating slurry and/or the component thereof is from about −200 mV to about 500 mV.

### Claim 20

A method for controlling microbiological activity in a coating slurry and/or a component thereof, comprising:
measuring a first pH of the coating slurry and/or the component thereof with a pH sensor and/or measuring a first oxidation-reduction potential (ORP) of the coating slurry and/or the component thereof with an ORP sensor;
adding a stabilizer and a chlorine source to the coating slurry;
mixing the stabilizer and the chlorine source in the slurry to form a stabilized chlorine composition; and
adding additional stabilizer, chlorine source, and/or stabilized chlorine to the coating slurry and/or the component thereof if the measured first pH and/or first ORP decreases.