# US 2026/0265139 A1 · Method for improving strength of concrete by adding, to cement, basic alkali mixture solution used for carbon dioxide capture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265139 A1
- Document ID: US20260265139A1
- Status: Published application
- Kind: A1
- Application number: 19/165,556
- Filed: 2024-03-15
- Published: 2026-09-10
- Earliest claimed: 2023-03-15
- Assignees: Lowcarbon Co., Ltd.
- Applicants: Lowcarbon Co., Ltd.
- Inventors: Cheol LEE; Hong Ki CHOI; Bong Kwan SONG; Ha Eun JUNG; Myeong Sub JANG; Hong Sik KIM; Eun Bee LEE; Ju Yeon SEO; Da Hun LEE
- Web page: https://patentgrep.com/patent/US20260265139A1

## CPC

- B28C 5/4237: {Charging, e.g. hoppers}
- C04B 22/106: {Bicarbonates}
- B28C 5/4231: {Proportioning or supplying water (in general B28C7/12)}
- B28C 7/128: {Nozzles; Valves; Valve-actuating means}
- C01D 7/00: Carbonates of sodium, potassium or alkali metals in general
- C04B 14/28: of calcium
- C04B 20/0232: {with carbon dioxide}
- C04B 22/10: containing carbon in the anion, e.g. carbonates
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 40/0028: {Aspects relating to the mixing step of the mortar preparation}
- C04B 2103/00: Function or property of ingredients for mortars, concrete or artificial stone
- C04B 2111/00: Mortars, concrete or artificial stone or mixtures to prepare them, characterised by specific function, property or use
- C04B 2111/00017: {Aspects relating to the protection of the environment}
- C04B 2111/00019: {Carbon dioxide sequestration}
- C04B 2201/52: High compression strength concretes, i.e. with a compression strength higher than about 55 N/mm2, e.g. reactive powder concrete [RPC]
- Y02C 20/40: of CO2
- B28C: PREPARING CLAY; PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL, e.g. PLASTER (preparing material for foundry moulds B22C5/00)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02C: CAPTURE, STORAGE, SEQUESTRATION OR DISPOSAL OF GREENHOUSE GASES [GHG]

## Abstract

Proposed is a method of improving concrete strength by recycling a basic alkali mixture solution used for carbon dioxide capture and adding the recycled basic alkali mixture solution to cement, including such as the following steps of (a) bringing a basic alkali mixture solution of specific components into contact with carbon dioxide in the air to capture carbon dioxide, (b) forming a carbon dioxide reaction product containing sodium carbonate (Na2CO3) or sodium bicarbonate (NaHCO3) by a reaction of the basic alkali mixture solution brought into contact with carbon dioxide, (c) injecting, in a preset ratio, the carbon dioxide reaction product into cement powder for concrete pouring, (d) mixing, for a preset time, the cement powder into which the carbon dioxide reaction product has been injected, thereby forming a concrete paste, and (e) pouring the formed concrete paste.

## Claims

### Claim 1

A method of improving concrete strength by adding a basic alkali mixture solution used for carbon dioxide capture to cement, the method comprising:
(a) bringing a basic alkali mixture solution of specific components into contact with carbon dioxide in air to capture carbon dioxide;
(b) forming a carbon dioxide reaction product containing sodium carbonate (Na2CO3) or sodium bicarbonate (NaHCO3) by a reaction of the basic alkali mixture solution brought into contact with the carbon dioxide;
(c) injecting, in a preset ratio, the carbon dioxide reaction product into cement powder for concrete pouring;
(d) mixing, for a preset time, the cement powder into which the carbon dioxide reaction product has been injected, thereby forming a concrete paste; and
(e) pouring the formed concrete paste.

### Claim 2 (depends on 1)

The method of claim 1, wherein the basic alkali mixture solution comprises:
one or more oxides selected from the group consisting of SiO2, Al2O3, Fe2O3, TiO2, MgO, MnO, Cao, Na2O, K2O, and P2O3;
one or more metals selected from the group consisting of Li, Cr, Co, Ni, Cu, Zn, Ga, Sr, Cd, and Pb;
a crystallized synthetic zeolite prepared using an alumina-based raw material, a silica-based raw material, and sodium hydroxide; and
one or more liquid compositions selected from the group consisting of sodium tetraborate (Na2B4O7·10H2O), sodium hydroxide (NaOH), sodium silicate (Na2SiO3), potassium hydroxide (KOH), and hydrogen peroxide (H2O2).

### Claim 3 (depends on 1)

The method of claim 1, wherein in the (c) injecting, the carbon dioxide reaction product is injected through spraying in an amount of 10 wt % or less, based on the cement powder for concrete pouring.

### Claim 4 (depends on 1)

The method of claim 1, wherein in the (d) mixing, the cement powder into which the carbon dioxide reaction product has been injected is mixed for the preset time, such that sodium carbonate (Na2CO3) or sodium bicarbonate (NaHCO3) in the carbon dioxide reaction product reacts with the cement powder (Ca(OH)2) to produce calcium carbonate (CaCO3), thereby forming the concrete paste in which the produced calcium carbonate is infiltrated into cement pores.

### Claim 5 (depends on 4)

The method of claim 4, wherein the produced calcium carbonate (CaCO3) has an average particle size of less than 100 μm.

### Claim 6 (depends on 3)

The method of claim 3, wherein the carbon dioxide reaction product is stored in a carbon dioxide reaction product tank provided at one side of a ready-mix concrete mixing drum and is sprayed into the cement powder inside the ready-mix concrete mixing drum using a full cone-type nozzle.

### Claim 7 (depends on 1)

The method of claim 1, wherein in the (c) injecting and the (d) mixing, the carbon dioxide reaction product is continuously sprayed, 10 minutes before concrete pouring, into a ready-mix concrete mixing drum for 5 minutes, followed by uniformly mixing contents inside the ready-mix concrete mixing drum while continuously rotating the ready-mix concrete mixing drum for 5 minutes.

### Claim 8 (depends on 6)

The method of claim 6, wherein the full cone-type nozzle sprays the carbon dioxide reaction product at a flow rate of 38.8 L/min based on a spray pressure of 0.5 kgf/cm2 when a single nozzle is used, and
the full cone-type nozzle sprays the carbon dioxide reaction product at a flow rate of 20.2 L/min based on a spray pressure of 0.7 kgf/cm2 when two nozzles are used.