# US 2026/0265125 A1 · Method for manufacturing composite cement

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265125 A1
- Document ID: US20260265125A1
- Status: Published application
- Kind: A1
- Application number: 19/489,296
- Filed: 2024-06-25
- Published: 2026-09-10
- Earliest claimed: 2023-06-27
- Assignees: HSustainability GmbH
- Applicants: HSustainability GmbH
- Inventors: Tim SCHADE; Jan SKOCEK; Gerd BOLTE; Nicolas PATO; Ahmed HANAFI; Arnaud MULLER
- Web page: https://patentgrep.com/patent/US20260265125A1

## CPC

- C04B 7/02: Portland cement
- C04B 7/13: Mixtures thereof with inorganic cementitious materials, e.g. Portland cements
- C04B 7/434: {Preheating with addition of fuel, e.g. calcining}
- C04B 7/52: Grinding {; After-treatment of ground cement}
- C04B 14/10: Clay {(sepiolite C04B14/042; grog C04B18/025)}
- C04B 28/04: Portland cements
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Composite cement comprising Portland cement, a calcium carbonate and a mechanochemically activated clay obtained by grinding a clay raw material which was mined from one or more natural clay deposits in a ball mill or roller mill at a temperature below 150° C. until the absorbance units of the OH peak at 3600 to 3700 cm−1 and the SiO2 peak at 900 to 1000 cm−1 in an FTIR spectrum decrease by at least 20%, as well as method for manufacturing the composite cement by blending Portland cement, calcium carbonate and the mechanochemically activated clay.

## Claims

### Claim 1

A composite cement comprising Portland cement, a calcium carbonate and a mechanochemically activated clay, wherein a clay raw material was obtained by mining one or more natural clay deposits and activated by grinding in a ball mill or roller mill at a temperature ≤150° C. until the absorbance units of the OH peak at 3600 to 3700 cm−1 and the SiO2 peak at 900 to 1000 cm−1 in an FTIR spectrum decrease by at least 20% to provide the mechanochemically activated clay wherein the clay raw material and calcination conditions are selected so that the activated clay does not contain more than 3 wt.-% free lime.

### Claim 2 (depends on 1)

The composite cement according to claim 1, wherein the composite cement comprises
at least 45 wt.-% Portland cement,
from 3 to 34 wt.-% calcium carbonate(s)
from 1 to 40 wt.-% activated clay.

### Claim 3 (depends on 1)

The composite cement according to claim 1, wherein the calcium carbonate is limestone, dolomite, precipitated calcium carbonate, carbonated recycled concrete paste, or a mixture of two or all of them, and/or the CaCO3 content of the calcium carbonate is at least 40 wt.-%.

### Claim 4 (depends on 1)

The composite cement according to claim 1, wherein the clay raw material comprises at least 10 wt.-% clay minerals, and/or up to 90 wt.-% clay minerals with respect to the total clay raw material weight.

### Claim 5 (depends on 1)

The composite cement according to claim 1, wherein the composite cement comprises one or more additional supplementary cementitious materials, selected from the group consisting of latent-hydraulic or pozzolanic slags, calcium rich fly ashes, calcium lean fly ashes, burnt oil shale, natural pozzolans, artificial pozzolans, recycled concrete paste, process dusts from cement clinker manufacturing, and mixtures thereof and/or the composite cement or a hydraulically hardening building material made from it contains admixtures and/or additives.

### Claim 6

A method for manufacturing a composite cement comprising the steps
providing Portland cement,
providing a calcium carbonate,
manufacturing activated clay by grinding a clay raw material obtained by mining one or more natural clay deposits in a ball mill or roller mill at a temperature ≤150° C. until the absorbance units of the OH peak at 3600 to 3700 cm−1 and the SiO2 peak at 900 to 1000 cm−1 in an FTIR spectrum decrease by at least 20%, wherein the clay raw material and the calcination conditions are selected so that the activated clay does not contain more than 3 wt.-% free lime, and
blending the Portland cement with the calcium carbonate and the activated clay.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the clay raw material is ground until the absorbance units of the OH peak and the SiO2 peak decrease by at least 25%.

### Claim 8 (depends on 6)

The method according to claim 6, wherein the temperature during grinding remains below 130° C. and/or grinding takes place in air.

### Claim 9 (depends on 6)

The method according to claim 6, wherein the mill is not additionally heated during grinding and/or the mill is not cooled during grinding.

### Claim 10 (depends on 6)

The method according to claim 6, wherein the clay raw material is dried to a free water content of 4 wt. % before grinding or during grinding.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the clay raw material is dried during grinding by introducing a hot gas into the mill, wherein the temperature of the clay raw material in the mill remains below 150° C.

### Claim 12 (depends on 6)

The method according to claim 6, wherein the clay raw material comprises one or more of kaolinite, dickite, halloysite, nacrite, montmorillonite, nontronite, beidellite, saponite, illite, palygorskite, and/or sepiolite.

### Claim 13 (depends on 6)

The method according to claim 6, wherein the clay raw material is partially calcined before grinding at a temperature from 400 to 1000° C., either for 10 to 120 minutes in a kiln or for 1 to 30 seconds in a flash calciner, so that of clay minerals contained in the clay raw material at least 5 wt.-% remain non-calcined in the calcined clay raw material.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the clay raw material and the calcination conditions are selected so that the activated clay does not contain more than 1 wt.-% free lime.

### Claim 15 (depends on 6)

The method according to claim 6, wherein providing the Portland cement comprises grinding a Portland cement clinker and/or a sulfate carrier and mixing them.

### Claim 16 (depends on 15)

The method according to claim 15, wherein blending Portland cement, calcium carbonate and mechanochemically activated clay is combined with grinding Portland cement clinker or sulfate carrier or both or blending is combined with grinding the Portland cement and/or the calcium carbonate.

### Claim 17 (depends on 2)

The composite cement according to claim 2, wherein the composite cement comprises
at least 50 wt.-% Portland cement
from 6 to 20 wt.-% calcium carbonate(s)
from 5 to 30 wt.-% activated clay.

### Claim 18 (depends on 3)

The composite cement according to claim 3, wherein the calcium carbonate is limestone, and/or the CaCO3 content of the calcium carbonate is at least 75 wt.-%.

### Claim 19 (depends on 4)

The composite cement according to claim 4, wherein the clay raw material comprises at least 30 wt.-% clay minerals and/or up to 70 wt.-% clay minerals with respect to the total clay raw material weight.

### Claim 20 (depends on 7)

The method according to claim 7, wherein the clay raw material is ground until the absorbance units of the OH peak and the SiO2 peak decrease by at least 30%.

### Claim 21 (depends on 10)

The method according to claim 10, wherein the clay raw material is dried to a free water content of less than 2 wt.-% before grinding or during grinding.

### Claim 22 (depends on 11)

The method according to claim 11, wherein the hot gas is an exhaust gas from cement manufacturing.

### Claim 23 (depends on 20)

The method according to claim 20, wherein the clay raw material is dried during grinding by introducing a hot gas into the mill, wherein the temperature of the clay raw material in the mill remains below 130° C. and the hot gas is an exhaust gas from cement manufacturing.

### Claim 24 (depends on 13)

The method according to claim 13, wherein of clay minerals contained in the clay raw material at least 10 wt.-% remain non-calcined in the calcined clay raw material.