# US 2026/0265123 A1 · Chemically strengthened glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0265123 A1
- Document ID: US20260265123A1
- Status: Published application
- Kind: A1
- Application number: 18/876,802
- Filed: 2023-06-29
- Published: 2026-09-10
- Earliest claimed: 2022-07-13
- Assignees: Nippon Electric Glass Co., Ltd.
- Applicants: Nippon Electric Glass Co., Ltd.
- Inventors: Kiyotaka KINOSHITA; Kazumi MAEDA; Kosei OSADA
- Web page: https://patentgrep.com/patent/US20260265123A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 10/0018: {containing SiO2, Al2O3 and monovalent metal oxide as main constituents}
- C03C 10/0027: {containing SiO2, Al2O3, Li2O as main constituents}
- C03C 10/0054: {containing PbO, SnO2, B2O3}
- C03C 21/00: Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A chemically tempered glass includes a compressive stress layer having a compressive stress in a surface layer portion and a tensile stress layer having a tensile stress in an inner portion. The chemically tempered glass has a temper filling rate FIOX represented by Equation (1) of 0.75 or more and 1.00 or less: F IOX = U CT U CT ⁢ limit = ∫ DOC t 2 σ ⁡ ( x ) 2 ⁢ dx 1.618 K 1 ⁢ C - 0.121 ( 1 ) where, for the chemically tempered glass, UCT represents a tensile square area [MPa2·m], UCT limit represents an explosion threshold value [MPa2·m], “t” represents a thickness [m], DOC represents a depth of compression [m] of the compressive stress layer, “x” represents a depth [m] from a surface, σ(x) represents a compressive stress value [MPa] at a depth “x”, and K1C represents a fracture toughness value [MPa·m1/2] in a composition of a thickness center portion.

## Claims

### Claim 1

A chemically tempered glass, comprising a compressive stress layer having a compressive stress in a surface layer portion and comprising a tensile stress layer having a tensile stress in an inner portion,
wherein the chemically tempered glass has a temper filling rate Fox represented by Equation (A) of 0.75 or more and 1.00 or less:
F
IOX
=
U
CT
U
CT
⁢
limit
(
A
)
where
UCT represents a tensile square area [MPa2·m] of the chemically tempered glass represented by Equation (B), and
UCT limit represents an explosion threshold value [MPa2·m] of the chemically tempered glass represented by Equation (C);
U
CT
=
∫
DOC
t
2
σ
⁡
(
x
)
2
⁢
dx
(
B
)
U
CT
⁢
limit
=
1.618
K
1
⁢
C
-
0.121
(
C
)
where
“t” represents a thickness [m] of the chemically tempered glass,
DOC represents a depth of compression [m] of the compressive stress layer of the chemically tempered glass,
“x” represents a depth [m] of the chemically tempered glass from a surface thereof,
σ(x) represents a compressive stress value [MPa] at a depth “x” of the chemically tempered glass, and
K1C represents a fracture toughness value [MPa·m1/2] in a composition of a thickness center portion of the chemically tempered glass.

### Claim 2 (depends on 1)

The chemically tempered glass according to claim 1, wherein the tensile square area UCT is 0.90 MPa2·m or more.

### Claim 3 (depends on 1)

The chemically tempered glass according to claim 1, wherein the fracture toughness value K1C is 0.80 MPa·m1/2 or more.

### Claim 4 (depends on 1)

The chemically tempered glass according to claim 1,
wherein the depth of compression DOC of the compressive stress layer is 90 μm or more, and
wherein the chemically tempered glass has a tensile stress value CT at a depth of t/2 of 80 MPa or more.

### Claim 5 (depends on 1)

The chemically tempered glass according to claim 1,
wherein the thickness “t” is from 0.1 mm to 1.5 mm,
wherein the chemically tempered glass has a compressive stress value CS in the surface of 700 MPa or more,
wherein the chemically tempered glass has a compressive stress value CS30 at a depth of 30 μm of 140 MPa or more, and
wherein the chemically tempered glass has a compressive stress value CS50 at a depth of 50 μm of 100 MPa or more.

### Claim 6 (depends on 1)

The chemically tempered glass according to claim 1, wherein the chemically tempered glass has a diffusion depth of layer DOLK of a potassium ion of 4 μm or more.

### Claim 7 (depends on 1)

The chemically tempered glass according to claim 1, wherein a stress profile of the chemically tempered glass obtained by measuring a stress from the surface in a depth direction, with a compressive stress being a positive number and a tensile stress being a negative number, has an inflection portion.

### Claim 8 (depends on 1)

The chemically tempered glass according to claim 1, comprising as the glass composition of the thickness center portion, in terms of mol %, 40% to 80% of SiO2, 10% to 30% of Al2O3, 0% to 10% of B2O3, 0.1% to 25% of Na2O, 0% to 10% of K2O, 0.1% to 20% of Li2O, 0% to 10% of MgO, and 0% to 10% of P2O5.

### Claim 9 (depends on 8)

The chemically tempered glass according to claim 8, comprising as the glass composition of the thickness center portion, in terms of mol %, 50% to 70% of SiO2, 10% to 20% of Al2O3, 0% to 3% of B2O3, 1% to 25% of Na2O, 0% to 10% of K2O, 3% to 12% of Li2O, 0% to 5% of MgO, and 1% to 10% of P2O5.

### Claim 10 (depends on 1)

The chemically tempered glass according to claim 1, comprising as the glass composition of the thickness center portion, in terms of mol %, 40% to 80% of SiO2, 10% to 30% of Al2O3, 0% to 3% of B2O3, 5% to 25% of Na2O, 0% to 5.5% of K2O, 0% to 0.09% of Li2O, and 0% to 10% of MgO.

### Claim 11 (depends on 1)

The chemically tempered glass according to claim 1, wherein the chemically tempered glass is a crystallized glass.