# US 2026/0260907 A1 · Process for preparing a supported metal catalyst and the so-obtained catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0260907 A1
- Document ID: US20260260907A1
- Status: Published application
- Kind: A1
- Application number: 18/869,528
- Filed: 2023-05-16
- Published: 2026-09-03
- Earliest claimed: 2022-05-26
- Assignees: Studiengesellschaft Kohle gGmbH
- Applicants: Studiengesellschaft Kohle gGmbH
- Inventors: Ferdi SCHUETH; Alexander GUNNARSON (Birth Name: HOPF); Jacopo DE BELLIS
- Web page: https://patentgrep.com/patent/US20260260907A1

## CPC

- H01M 4/926: {on carbon or graphite}
- H01M 4/8842: {Coating using a catalyst salt precursor in solution followed by evaporation and reduction of the precursor}
- H01M 4/8882: {Heat treatment, e.g. drying, baking}
- H01M 8/10: Fuel cells with solid electrolytes
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention refers to a process for preparing a supported metallic, in particular a bimetallic, catalyst and the so-obtained catalyst combining high stability with unique electronic and structural properties.

## Claims

### Claim 1

A process for preparing a supported metal catalyst comprising, in a first step, ball milling at least one metal compound with an electrically conductive support which is selected from electrically conductive carbon materials to yield a first product and, in a second step, hydrogenating the first product under a H2 pressure of 1 to 10 atm in a temperature range from 100° C. to 500° C. for a time period of 1 to 3 hours to form a second product and, in an optional third step, annealing the second product under a protective gas atmosphere in a temperature range from 400° C. to 1200° C. for a time period of 2 to 12 hours.

### Claim 2 (depends on 1)

Process according to claim 1, wherein the at least one metal compound is selected from metal halides, metal nitrates, metal sulfates, metal carbonates, metal carboxylates of a carboxylic acid having 1 to 12 carbon atoms, metal β-diketonates, metal carbonyls, metallocenes, or cyclopentadienyl metal complexes.

### Claim 3 (depends on 1)

Process according to claim 1, wherein the metal of the at least one metal compound is selected from at least one catalytically active metal selected from V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Zr, Mo, Re, Ru, Rh, Pd, Ag, Cd, Sn, Ir, Pt, Au, or mixtures thereof.

### Claim 4 (depends on 1)

Process according to claim 1, wherein the loading of the metal compound on the support is in the range of 0.5 to 50% by weight, based on the support and calculated with any ligand excluded.

### Claim 5 (depends on 1)

Process according to claim 1, wherein the electrically conductive support is an electrically conductive carbon material, selected from carbon, graphite, carbon black, or titanium carbide, or titanium nitride.

### Claim 6 (depends on 1)

Process according to claim 1, wherein the ball milling is performed in any ball milling machine selected from attritor mills, Simoloyer-type ball mills, and planetary ball mills, in a frequency range from 200 to 1400 rpm with balls in a size range from 2 to 20 mm, for a time period from 15 min to 720 min.

### Claim 7 (depends on 1)

Process according to claim 1, wherein the hydrogenating is carried out under a flow of hydrogen in an inert gas with a hydrogen ratio of 5 to 50 vol-%.

### Claim 8 (depends on 1)

Process according to claim 1, which comprises ball milling a metal acetylacetonate, selected from Pd or Pt acetylacetonate, with carbon to obtain a product, and subjecting the obtained product to hydrogenation and finally to an annealing treatment.

### Claim 9 (depends on 1)

A supported metal catalyst obtainable according to the process as claimed in claim 1.

### Claim 10 (depends on 9)

A process comprising conducting a reaction in the presence of a catalyst, wherein the catalyst is the supported metal catalyst as claimed in claim 9.

### Claim 11 (depends on 1)

The process according to claim 1, wherein the electrically conductive carbon materials are selected from the group consisting of carbon, graphite, carbon black, titanium carbide, or from titanium nitride, boron nitride, niobium nitride, indium tin oxide, and antimony tin oxide.

### Claim 12 (depends on 1)

The process according to claim 1, wherein the electrically conductive carbon materials are selected from the group consisting of carbon, titanium nitride, and boron nitride.

### Claim 13 (depends on 1)

The process according to claim 1, wherein the electrically conductive carbon material is carbon.

### Claim 14 (depends on 1)

Process according to claim 1, wherein the at least one metal compound is selected from metal carboxylates of a carboxylic monoacid or diacid having 1 to 12 carbon atoms, metal halides, metal nitrates, and metal carboxylates.

### Claim 15 (depends on 1)

Process according to claim 1, wherein the at least one metal compound is selected from metal carboxylates of a carboxylic monoacid or diacid having 1 to 6 carbon atoms, or metal s-diketonates.

### Claim 16 (depends on 1)

Process according to claim 1, wherein the metal of the at least one metal compound is selected from Fe, Co, Ni, Ru, Pd, Ag, Rh, Ir, Sn, Pt, and mixtures thereof.

### Claim 17 (depends on 6)

Process according to claim 6, wherein the balls are made of steel, carbides, oxides, nitrides, or polymeric materials.

### Claim 18 (depends on 10)

The process as claimed in claim 10, wherein the supported metal catalysts is an electrocatalyst.

### Claim 19 (depends on 10)

The process as claimed in claim 10, wherein the reaction is a cathode side oxygen reduction reaction (ORR) in a PEM fuel cell.