# US 2026/0260880 A1 · Superfast recharging zinc-based energy storage devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0260880 A1
- Document ID: US20260260880A1
- Status: Published application
- Kind: A1
- Application number: 18/845,813
- Filed: 2023-03-10
- Published: 2026-09-03
- Earliest claimed: 2022-03-11
- Assignees: Nanotech Energy, Inc.
- Applicants: NanoTech Energy, Inc.
- Inventors: Maher F. EL-KADY; Mir F. MOUSAVI; Haosen WANG
- Web page: https://patentgrep.com/patent/US20260260880A1

## CPC

- H01M 4/42: Alloys based on zinc
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- B82Y 40/00: Manufacture or treatment of nanostructures
- H01M 4/049: {Manufacturing of an active layer by chemical means}
- H01M 4/244: {Zinc electrodes}
- H01M 4/26: Processes of manufacture
- H01M 4/52: of nickel, cobalt or iron
- H01M 4/5815: {Sulfides}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/663: {containing carbon or carbonaceous materials as conductive part, e.g. graphite, carbon fibres}
- H01M 10/24: Alkaline accumulators
- H01M 10/26: Selection of materials as electrolytes
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0014: Alkaline electrolytes
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided herein are rechargeable aqueous Zn∥Ni energy storage devices that exhibit improved electrochemical performance high performance and super-long life. The combination of a high-performance Zn-based anode and an efficient Ni-based cathode herein, which aqueous battery chemistry with outstanding, form an energy storage device with high energy and power densities and cycling stability.

## Claims

### Claim 1

An energy storage device comprising:
(a) an anode comprising a bimetallic particle on a graphene scaffold, the bimetallic particle comprising ZnxM1-xCO3 nanoparticles, wherein M is iron, cobalt, aluminum, manganese, or any combination thereof, and wherein x is less than 1;
(b) a cathode comprising a layered double hydroxide (LDH) nanotube; and
(c) an electrolyte.

### Claim 2 (depends on 1)

The energy storage device of claim 1, wherein layered double hydroxide (LDH) nanotube comprises one or more layered double hydroxide nanoparticles.

### Claim 3 (depends on 1)

The energy storage device of claim 1, wherein the bimetallic particle comprises ZnxM1-xCO3 nanoparticles, wherein M is manganese, and wherein x is less than 1.

### Claim 4 (depends on 1)

The energy storage device of claim 1, wherein a molar ratio of Zn to M is about 1:1 to about 7:1.

### Claim 5 (depends on 1)

The energy storage device of claim 1, wherein the graphene scaffold comprises graphene aerogel, graphene hydrogel, or both.

### Claim 6 (depends on 1)

The energy storage device of claim 1, wherein the LDH nanotubes comprise sulfidated Ni—Co—Fe nanotubes.

### Claim 7 (depends on 1)

The energy storage device of claim 1, wherein the LDH nanotubes have a diameter of about 50 to about 150 nm.

### Claim 8 (depends on 1)

The energy storage device of claim 1, wherein the LDH nanotubes have a diameter of about 100 nm.

### Claim 9 (depends on 1)

The energy storage device of claim 1, wherein the LDH particles comprise sulfidated Ni—Co—Fe particles.

### Claim 10 (depends on 1)

The energy storage device of claim 1, wherein the LDH nanotubes or LDH particles comprise aluminum, barium, bismuth, cadmium, calcium, chromium, cobalt, coppern, indium, iron, lead, manganese, mercury, nickel, strontium, tin, zinc, or any combination thereof.

### Claim 11 (depends on 1)

The energy storage device of claim 1, wherein the electrolyte comprises a hydroxide and a stabilizer.

### Claim 12 (depends on 1)

The energy storage device of claim 1, wherein the hydroxide comprises aluminum hydroxide, barium hydroxide, benzyltrimethylammonium hydroxide, beryllium hydroxide, cadmium hydroxide, cesium hydroxide, calcium hydroxide, cerium(III) hydroxide, chromium acetate hydroxide, chromium(III) hydroxide, cobalt(II) hydroxide, cobalt(III) hydroxide, copper(I) hydroxide, copper(II) hydroxide, curium hydroxide, gallium(III) hydroxide, germanium(II) hydroxide, gold(III) hydroxide, indium(III) hydroxide, iron(II) hydroxide, iron(III) oxide-hydroxide, lanthanum hydroxide, lead(II) hydroxide, lead(IV) hydroxide, lithium hydroxide, magnesium hydroxide, manganese(II) hydroxide, mercury(II) hydroxide, metal hydroxide, nickel(II) hydroxide, potassium hydroxide, rubidium hydroxide, sodium hydroxide, strontium hydroxide, tetrabutylammonium hydroxide, tetramethylammonium hydroxide, thallium hydroxide, thallium(I) hydroxide, thallium(III) hydroxide, tin(II) hydroxide, uranyl hydroxide, zinc hydroxide, zirconium(IV) hydroxide, or any combination thereof.

### Claim 13 (depends on 1)

The energy storage device of claim 1, wherein the stabilizer comprises zinc oxide, zinc hydroxide, sodium zincate, potassium zincate, bismuth oxide, cadmium oxide, indium sulfate, lead oxide, a metallic zinc powder, or any combination thereof. In some embodiments, the hydrogen evolution inhibitor comprises bismuth oxide, cadmium oxide, a conductive ceramic, lead oxide, a metallic zinc powder antimony sulfate, gallium hydroxide, indium sulfate, lithium hydroxide, or any combination thereof.

### Claim 14 (depends on 1)

The energy storage device of claim 1, wherein the electrolyte has a concentration by mass, by volume, or both of the hydroxide of about 22% to about 91%.

### Claim 15 (depends on 1)

The energy storage device of claim 1, wherein the electrolyte has a concentration by volume of the hydroxide of about 220 g/L to about 900 g/L.

### Claim 16 (depends on 1)

The energy storage device of claim 1, wherein the electrolyte has a concentration by mass, by volume, or both of the stabilizer of about 1% to about 5%.

### Claim 17 (depends on 1)

The energy storage device of claim 1, wherein the electrolyte further comprises a conductivity enhancer comprising a conductive ceramic.

### Claim 18 (depends on 1)

The energy storage device of claim 1, wherein the conductive ceramic comprises lead zirconate titanate (PZT), barium titanate(BT), strontium titanate (ST), calcium titanate (CT), magnesium titanate (MT), calcium magnesium titanate (CMT), zinc titanate (ZT), lanthanum titanate (LT), and neodymium titanate (NT), barium zirconate (BZ), calcium zirconate (CZ), lead magnesium niobate (PMN), lead zinc niobate (PZN), lithium niobate (LN), barium stannate (BS), calcium stannate (CS), magnesium aluminum silicate, magnesium silicate, barium tantalate, titanium dioxide, niobium oxide, zirconia, quartz, silica, sapphire, beryllium oxide, zirconium tin titanate, indium tin oxide (ITO), lanthanum-doped strontium titanate (SLT), yttrium-doped strontium titanate (SYT), yttria-stabilized zirconia (YSZ), gadolinium-doped ceria (GDC), lanthanum strontium gallate magnesite (LSGM), or any combination thereof.

### Claim 19 (depends on 1)

The energy storage device of claim 1, wherein the electrolyte further comprises:
(a) an additive comprising calcium hydroxide, calcium titanate, calcium zincate, potassium fluoride, sodium phosphate tribasic, potassium phosphate, sodium fluoride, potassium borate, potassium carbonate, or any combination thereof,
(b) a hydrogen evolution inhibitor comprising bismuth oxide, cadmium oxide, a conductive ceramic, lead oxide, a metallic zinc powder antimony sulfate, gallium hydroxide, indium sulfate, lithium hydroxide, or any combination thereof, or
(c) both.

### Claim 20 (depends on 1)

The energy storage device of claim 1, wherein a mass ratio between the electroactive materials in the anode and the cathode is about 1:1 to about 7:1.

### Claim 21 (depends on 1)

The energy storage device of claim 1, wherein the electrolyte has a concentration of the KOH of about 1 M to about 20 M.

### Claim 22 (depends on 1)

The energy storage device of claim 1, further comprising a separator between the anode and the cathode.

### Claim 23 (depends on 1)

The energy storage device of claim 1, having a rate capability of at least about 300 mAh/g at 12 A/g.

### Claim 24 (depends on 1)

The energy storage device of claim 1, having a rate capability of at least about 100 mAh/g at 300 A/g.

### Claim 25 (depends on 1)

The energy storage device of claim 1, having a specific energy of at least about 550 Wh/kg.

### Claim 26 (depends on 1)

The energy storage device of claim 1, having a specific power of at least about 400 kW/kg.

### Claim 27 (depends on 1)

The energy storage device of claim 1, having a capacity retention of at least about 95% after about 16,000 cycles at 100% depth of discharge.

### Claim 28 (depends on 1)

The energy storage device of claim 1, having a time constant of less than about 0.5 seconds.

### Claim 29 (depends on 1)

The energy storage device of claim 1, configured for use in an electric vehicle, an energy grid, a home battery, or any combination thereof.

### Claim 30

An energy storage device comprising:
(a) an anode comprising bimetallic ZnxM1-xCO3 nanoparticles on a graphene scaffold, wherein M is manganese, and wherein x is less than 1;
(b) a cathode comprising sulfidated Ni—Co—Fe layered double hydroxide nanotube; and
(c) an electrolyte.

### Claim 31

A method of forming an electrode, the method comprising:
(a) forming a first solution comprising graphene oxide and a solvent;
(b) adding zinc nitrate hexahydrate and manganese nitrate tetrahydrate to the first solution;
(c) adding a reducing agent to the first solution to form a second solution;
(d) heating the second solution;
(e) cooling the second solution;
(f) washing the second solution; and
(g) freeze drying the second solution.

### Claim 32 (depends on 31)

The method of claim 31, wherein step (a) comprises ultrasonicating the graphene oxide in the solvent.

### Claim 33 (depends on 31, 32)

The method of claim 31 or 32, wherein a concentration of the graphene oxide in the first solution is about 0.5 g/L to about 10 g/L.

### Claim 34 (depends on 31, 32)

The method of claim 31, 32, or 33, wherein the ultrasonification is performed for about 1 minute to about 120 minutes.

### Claim 35 (depends on 31, 32, 33, 34)

The method of any one of claims 31-34, wherein the ultrasonification is performed at room temperature.

### Claim 36 (depends on 31, 32, 33, 34, 35)

The method of any one of claims 31-35, wherein the zinc nitrate hexahydrate has a concentration of about 1 mM to about 1,000 mM.

### Claim 37 (depends on 31, 32, 33, 34, 35, 36)

The method of any one of claims 31-36, wherein the manganese nitrate tetrahydrate has a concentration of about 0.3 mM to about 300 mM.

### Claim 38 (depends on 31, 32, 33, 34, 35, 36, 37)

The method of any one of claims 31-37, wherein step (c) occurs for a period of time of at least about 0.1 hour to about 10 hours.

### Claim 39 (depends on 31, 32, 33, 34, 35, 36, 37, 38)

The method of any one of claims 31-38, wherein a molar ratio of Zn2+ to Mn2+ is about 1:1 to about 7:1.

### Claim 40 (depends on 31, 32, 33, 34, 35, 36, 37, 38, 39)

The method of any one of claims 31-39, wherein the reducing/doping agent comprises urea, hydrazine hydrate, sodium borohydride, ascorbic acid, hydroquinone, sodium cholate, sodium citrate, hydroiodic acid, bovine serum albumin, dopamine, glucose, fructose, sucrose, melatonin, starch, oxalic acid, tannic acid, gallic acid, caffeic acid, or any combination thereof.

### Claim 41 (depends on 31, 32, 33, 34, 35, 36, 37, 38, 39, 40)

The method of any one of claims 31-40, wherein step (d) is performed at a temperature of about 90° C. to about 200° C.

### Claim 42 (depends on 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41)

The method of any one of claims 31-41, wherein step (d) is performed for a period of time of about 1 hour to about 24 hours.

### Claim 43 (depends on 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41, 42)

The method of any one of claims 31-42, further comprising stirring the first solution before step (c), after step (c), or both.

### Claim 44 (depends on 43)

The method of claim 43, wherein stirring the first solution is performed for a period of time of about 1 minute to about 100 minutes.

### Claim 45 (depends on 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41, 42, 43, 44)

The method of any one of claims 31-44, further comprising:
(a) adding a conductive additive, a binder, and a solvent to the second solution to form a slurry;
(b) coating a current collector with the slurry; and
(c) drying the slurry on the current collector.

### Claim 46 (depends on 45)

The method of claim 45, wherein the conductive additive comprises carbon black, graphene, carbon nanotubes, graphite, carbon nanofibers, or any combination thereof.

### Claim 47 (depends on 45, 46)

The method of claim 45 or 46, wherein the binder comprises polytetrafluoroethylene, styrene butadiene rubber, carboxymethyl cellulose, polyvinylidene fluoride, or any combination thereof.

### Claim 48 (depends on 45, 46)

The method of claim 45, 46, or 47, wherein the solvent comprises ethanol, polyvinylidene fluoride, or any combination thereof.

### Claim 49 (depends on 45, 46, 47, 48)

The method of any one of claims 45-48, wherein the slurry is dried on the current collector a temperature of about 30° C. to about 100° C.

### Claim 50 (depends on 45, 46, 47, 48, 49)

The method of any one of claims 45-49, wherein the slurry is dried on the current collector for a period of time of about 1 hour to about 24 hours.

### Claim 51

A method of forming an electrode, the method comprising:
(a) synthesizing Ni—Co—Fe layer double hydroxide nanoplatelets;
(b) heating the Ni—Co—Fe layer double hydroxide nanoplatelets; and
(c) drying the Ni—Co—Fe layer double hydroxide nanoplatelets.

### Claim 52 (depends on 51)

The method of claim 51, wherein step (a) comprises:
(a) immersing a metal foam in an acid;
(b) washing the metal foam;
(c) electrodepositing the metal foam in a electrosynthesis solution; and
(d) washing the Ni—Co—Fe layer double hydroxide nanoplatelets on the metal foam.

### Claim 53 (depends on 51, 52)

The method of claim 51 or 52, wherein the electrodeposition is performed by a three-electrode (3E) cell comprising:
(a) the metal foam as a working electrode;
(b) a reference electrode; and
(c) a counter electrode.

### Claim 54 (depends on 51, 52, 53)

The method of claim 51, 52 or 53, wherein the reference electrode comprises Ag/AgCl, Hg/HgO, saturated calomel, or any combination thereof.

### Claim 55 (depends on 51, 52, 53, 54)

The method of any one of claims 51-54, wherein the counter electrode comprises platinum, gold, carbon, graphite, or any combination thereof.

### Claim 56 (depends on 51, 52, 53, 54, 55)

The method of any one of claims 51-55, wherein the acid comprises HCl, HNO3, or both.

### Claim 57 (depends on 51, 52, 53, 54, 55, 56)

The method of any one of claims 51-56, wherein the washing is performed for a period of time of about 1 minute to about 10 minutes.

### Claim 58 (depends on 51, 52, 53, 54, 55, 56, 57)

The method of any one of claims 51-57, wherein the electrodeposition is performed by applying two or more consecutive potential cycles.

### Claim 59 (depends on 51, 52, 53, 54, 55, 56, 57, 58)

The method of any one of claims 51-58, wherein the electrodeposition is performed by applying about 10 to about 15 consecutive potential cycles.

### Claim 60 (depends on 51, 52, 53, 54, 55, 56, 57, 58, 59)

The method of any one of claims 51-59, wherein the electrodeposition is performed for a period of time of less than about 5 minutes.

### Claim 61 (depends on 51, 52, 53, 54, 55, 56, 57, 58, 59, 60)

The method of any one of claims 51-60, wherein the electrodeposition is performed from about −0.7 V to about −1.2 V.

### Claim 62 (depends on 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61)

The method of any one of claims 51-61, wherein the electrodeposition is performed at a scan rate of about 1 mV/s to about 1,000 mV/s.

### Claim 63 (depends on 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62)

The method of any one of claims 51-62, wherein the electrosynthesis solution comprises Co(NO3)2·6H2O, Ni(NO3)2·6H2O, Fe(NO3)3·9H2O, and KNO3.

### Claim 64 (depends on 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62, 63)

The method of any one of claims 51-63, further comprising drying the Ni—Co—Fe layer double hydroxide nanoplatelets on the metal foam.

### Claim 65 (depends on 64)

The method of claim 64, wherein drying the Ni—Co—Fe layer double hydroxide nanoplatelets on the metal foam is performed at a temperature of about 30° C. to about 100° C.

### Claim 66 (depends on 64, 65)

The method of claim 64 or 65, wherein drying the Ni—Co—Fe layer double hydroxide nanoplatelets on the metal foam is performed for a period of time of about 1 hour to about 24 hours.

### Claim 67 (depends on 64, 65)

The method of claim 64, 65, or 66, wherein the Ni—Co—Fe layer double hydroxide nanoplatelets is heated at a temperature of about 90° C. to about 200° C.

### Claim 68 (depends on 64, 65, 66, 67)

The method of any one of claims 64-67, wherein the Ni—Co—Fe layer double hydroxide nanoplatelets is heated for a time period of about 1 hour to about 24 hours.

### Claim 69 (depends on 64, 65, 66, 67, 68)

The method of any one of claims 64-68, wherein the Ni—Co—Fe layer double hydroxide nanoplatelets are dried at room temperature.

### Claim 70 (depends on 64, 65, 66, 67, 68, 69)

The method of any one of claims 64-69, further comprising washing the Ni—Co—Fe layer double hydroxide nanoplatelets before heating the Ni—Co—Fe layer double hydroxide nanoplatelets.

### Claim 71 (depends on 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62, 63, 64, 65, 66, 67, 68, 69, 70)

The method of any one of claims 51-70, wherein the method is performed in less than about 5 minutes.

### Claim 72 (depends on 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62, 63, 64, 65, 66, 67, 68, 69, 70, 71)

The method of any one of claims 51-71, wherein the metal foam comprises a nickel foam.

### Claim 73 (depends on 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62, 63, 64, 65, 66, 67, 68, 69, 70, 71, 72)

The method of any one of claims 51-72, further comprising sulfidating the Ni—Co—Fe layer double hydroxide nanoplatelets.

### Claim 74 (depends on 73)

The method of claim 73, wherein sulfidating the Ni—Co—Fe layer double hydroxide nanoplatelets comprises heating the Ni—Co—Fe layer double hydroxide nanoplatelets in the presence of a sulfidizing agent.

### Claim 75 (depends on 74)

The method of claim 74, wherein the sulfidizing agent comprises Na2S.

### Claim 76 (depends on 74)

The method of claim 74, wherein the heating is performed at a temperature of about 100° C. to about 180° C.

### Claim 77 (depends on 74)

The method of claim 74, wherein the heating is performed for a period of time of about 4 hours to about 12 hours.

### Claim 78

A method of applying regenerative voltage pulse to a zinc-based energy storage device to maintain or increase the initial capacity, the method comprising: after a sequence of at least 10 galvanostatic charge-discharge (GCD) cycles:
(a) applying a first voltage pulse at a first voltage for a first period of time;
(b) applying a second voltage pulse at a second voltage for a second period of time;
(c) repeating (a) and (b) at least every 10 galvanostatic charge-discharge (GCD) cycles; and
(d) maintaining 100% of the initial device capacity after about 100 galvanostatic charge-discharge (GCD) cycles.

### Claim 79 (depends on 78)

The method of claim 78, wherein the first voltage is greater than the second voltage.

### Claim 80 (depends on 78)

The method of claim 78, wherein the first voltage is about 1.5 V to about 2.5 V.

### Claim 81 (depends on 78)

The method of claim 78, wherein the first voltage is 2.05 V.

### Claim 82 (depends on 78, 79)

The method of claim 78 or 79, wherein the second voltage is about 1 V to about 1.5 V.

### Claim 83 (depends on 78)

The method of claim 78, wherein the second voltage is 1.3 V.

### Claim 84 (depends on 78, 79)

The method of claim 78, 79, or 82, wherein the first period of time, the second period of time, or both is about 15 seconds to about 30 seconds.

### Claim 85 (depends on 78, 79, 80, 81, 82, 83, 84)

The method of any one of claims 78-84, wherein the sequence of GCD cycles comprises about 8 GCD cycles to about 14 GCD cycles.

### Claim 86 (depends on 78)

The method of claim 78, wherein (a) and (b) result in structural reorganization of an active materials during cycling of the energy storage device.

### Claim 87 (depends on 78)

The method of claim 78, wherein (a) and (b) result in the expansion of pores within an active material during cycling of the energy storage device.

### Claim 88 (depends on 78)

The method of claim 78, wherein (a) and (b) result in the expansion of pores within an active material during cycling of the energy storage device and increased penetration of electrolyte ions the pores.

### Claim 89 (depends on 78)

The method of claim 78, wherein (a) and (b) result in kinetic activation of the electrode.

### Claim 90 (depends on 78)

The method of claim 78, wherein the zinc-based energy storage device comprises:
(a) an anode comprising bimetallic ZnxM1-xCO3 nanoparticles on a graphene scaffold, wherein M is iron, cobalt, aluminum, manganese, or any combination thereof, and wherein x is less than 1;
(b) a cathode comprising sulfidated Ni—Co—Fe layered double hydroxide nanotubes;
(c) an electrolyte; or
(d) combinations thereof.