Electroplating additive solution and preparation method thereof, silver-graphene electroplating mixture liquid
AssigneeZhejiang Chint Electrics Co., Ltd.
InventorsZhengli XU, Tongyang Li, Lang Zeng, Wei Zhao
Life of this patent
Estimating the term…
Abstract
An electroplating additive solution, a preparation method thereof, and a hard silver-graphene electroplating mixture liquid are provided. The electroplating additive solution includes metal oxide, glycerol, alkali metal hydroxide and water. The metal oxide, the glycerol, the alkali metal hydroxide and the water have a mass ratio of 1:(1-3):(3-6):(8-15). When the electroplating additive of the present disclosure is used in an electroplating mixture liquid, it can increase the hardness of the finally formed plating layer.
Claims20
An electroplating additive solution, wherein
- the electroplating additive solution comprises metal oxide, glycerol, alkali metal hydroxide and water;
- a mass ratio of the metal oxide, the glycerol, the alkali metal hydroxide and the water is 1:(1-3):(3-6):(8-15).
A preparation method for an electroplating additive solution, wherein the method comprises:
- mixing alkali metal hydroxide with glycerol and performing stirring to obtain a first solution;
- adding metal oxide and water to the first solution, performing stirring and heating to obtain a second solution;
- allowing the second solution to stand, and taking an upper clear liquid as the electroplating additive solution,
- wherein the electroplating additive solution comprises metal oxide, glycerol, alkali metal hydroxide and water;
- and
- a mass ratio of the metal oxide, the glycerol, the alkali metal hydroxide and the water is 1:(1-3):(3-6):(8-15).