# US 2026/0258534 A1 · A bainite seamless steel pipe and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0258534 A1
- Document ID: US20260258534A1
- Status: Published application
- Kind: A1
- Application number: 18/846,982
- Filed: 2023-03-17
- Published: 2026-09-03
- Earliest claimed: 2022-03-29
- Assignees: Baoshan Iron & Steel Co., Ltd.
- Applicants: Baoshan Iron & Steel Co., Ltd.
- Inventors: Wen Sun; Zhan Gao; Guoli Zhai; Suzhen Luo; Ping Hu
- Web page: https://patentgrep.com/patent/US20260258534A1

## CPC

- C22C 38/38: with more than 1.5% by weight of manganese
- B22D 11/001: {of specific alloys}
- C21C 5/562: {starting from scrap}
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/19: by interrupted quenching
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 1/56: characterised by the quenching agents
- C21D 1/84: Controlled slow cooling (cooling-beds for metal rolling B21B43/00)
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 7/13: by hot working
- C21D 8/10: during manufacturing of tubular bodies
- C21D 9/08: for tubular bodies or pipes
- C21D 9/085: {Cooling or quenching}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/32: with boron
- B21B 17/10: in a continuous process
- B21B 19/04: Rolling basic material of solid, i.e. non-hollow, structure; Piercing {, e.g. rotary piercing mills}
- B21B 19/10: Finishing, e.g. smoothing, sizing {, reeling}
- B21B 23/00: Tube-rolling not restricted to methods provided for in only one of groups B21B17/00, B21B19/00, B21B21/00, e.g. combined processes {planetary tube rolling, auxiliary arrangements, e.g. lubricating, special tube blanks, continuous casting combined with tube rolling}(B21B25/00 takes precedence)
- C21D 2211/002: Bainite
- Y02P 10/20: Recycling
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention provides a bainite seamless steel pipe and a manufacturing method therefor. In addition to Fe and inevitable impurities, the bainite seamless steel pipe further comprises the following chemical elements in percentage by mass: C: 0.16-0.18%, Si: 0.56-1%, Mn: 1.8-2.05%, Cr: 0.85-1.25%, Al: 0.015-0.04%, B: 0.001-0.005%, 0<N≤0.006%, wherein Al/N≥3. The bainite seamless steel pipe of the present invention can obtain good strength-toughness matching in a rolled state or a single tempered state without the need for quenching and tempering heat treatment.

## Claims

### Claim 1

A bainite seamless steel pipe, wherein in addition to Fe and inevitable impurities, the bainite seamless steel pipe further comprises the following chemical elements in percentage by mass:
C: 0.16-0.18%, Si: 0.56-1%, Mn: 1.8-2.05%, Cr: 0.85-1.25%, Al: 0.015-0.04%, B: 0.001-0.005%, 0<N≤0.006%, wherein Al/N≥3.

### Claim 2 (depends on 1)

The bainite seamless steel pipe according to claim 1, wherein the bainite seamless steel pipe comprises the following chemical elements in percentage by mass:
C: 0.16-0.18%, Si: 0.56-1%, Mn: 1.8-2.05%, Cr: 0.85-1.25%, Al: 0.015-0.04%, B: 0.001-0.005%, 0<N≤0.006%, the balance being Fe and inevitable impurities, wherein Al/N≥3.

### Claim 3 (depends on 1)

The bainite seamless steel pipe according to claim 1, wherein the inevitable impurities include S and P; wherein S≤0.01%, P≤0.005%.

### Claim 4 (depends on 1)

The bainite seamless steel pipe according to claim 1, wherein the bainite seamless steel pipe has the following performances in a rolled state: a yield strength of 552-758 MPa, a tensile strength of ≥980 MPa, a longitudinal impact toughness of ≥40 J, a yield ratio of 0.6-0.75, an elongation of 12-15%, a local residual stress of ≤200 MPa within a range of 1-2 mm in a wall thickness direction of its outer wall, an overall residual stress of ≤100 MPa throughout its pipe body.

### Claim 5 (depends on 1)

The bainite seamless steel pipe according to claim 1, wherein the bainite seamless steel pipe after being tempered at a temperature of 200-350° C. has the following performances in a tempered state: a yield strength of 650-860 MPa, a tensile strength of ≥980 MPa, a longitudinal impact toughness of ≥60 J, a yield ratio of 0.7-0.83.

### Claim 6 (depends on 1)

The bainite seamless steel pipe according to claim 1, wherein the bainite seamless steel pipe after being tempered at a temperature of 400-460° C. has the following performances in a tempered state: a yield strength of 650-860 MPa, a tensile strength of ≥980 MPa.

### Claim 7 (depends on 1)

The bainite seamless steel pipe according to claim 1, wherein the bainite seamless steel pipe is free of Mo, Ni, Nb, V and/or Ti; and/or, the bainite seamless steel pipe satisfies one or more of the following: Si content is in a range of 0.66-0.85%, preferably 0.75-0.85%; Mn content is in a range of 1.85-2%; Cr content is in a range of 0.9-1.1%; B content is in a range of 0.002-0.0045%; N content is in a range of 0.004-0.006%.

### Claim 8 (depends on 1)

The bainite seamless steel pipe according to claim 1, wherein the bainite seamless steel pipe has a bainite structure.

### Claim 9 (depends on 1)

A method for manufacturing the bainite seamless steel pipe according to claim 1, wherein the method comprises the following steps:
(1) smelting molten steel and performing continuous casting to obtain a steel billet;
(2) performing perforation, continuous rolling and sizing of the steel billet to obtain a steel pipe;
(3) air cooling the steel pipe after sizing in three-stages: cooling is performed in a range of 500-850° C. in the first stage in a controlled cooling rate of 2-5° C./s; after cooling to 500° C., a cooling rate in the second stage is controlled to be 5-15° C./s, preferably 8.5-15° C./s; after cooling to 300° C., natural air cooling is performed to obtain the bainite seamless steel pipe.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the method satisfies one or more of the following:
a: in step (1), scrap steel and blast furnace molten iron are used to make the molten steel, wherein the blast furnace molten iron is used at a mass percentage of 50-60%; and/or, in the continuous casting, the molten steel has a superheat of lower than 30° C., and a drawing speed during the continuous casting is 1.8-2.2 m/min;
b: before step (2), the steel billet is cooled and then heated, a heating temperature is 1240-1300° C., a heating time is 3-6 h;
c: in step (2), the perforation is performed at a temperature of 1180-1240° C., the continuous rolling is performed at a temperature of 1000° C.-1100° C.;
d: in step (2), after the continuous rolling and before the sizing, the pipe body is naturally cooled and then heated to 950-980° C., and then taken out of the furnace for sizing at a temperature of 850-950° C.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the method further comprises step (4): tempering the bainite seamless steel pipe obtained in step (3) at a temperature of 200-350° C. or 400-460° C.

### Claim 12 (depends on 2)

The bainite seamless steel pipe according to claim 2, wherein the inevitable impurities include S and P; wherein S≤0.01%, P≤0.005%.

### Claim 13 (depends on 2)

The bainite seamless steel pipe according to claim 2, wherein the bainite seamless steel pipe has the following performances in a rolled state: a yield strength of 552-758 MPa, a tensile strength of ≥980 MPa, a longitudinal impact toughness of ≥40 J, a yield ratio of 0.6-0.75, an elongation of 12-15%, a local residual stress of ≤200 MPa within a range of 1-2 mm in a wall thickness direction of its outer wall, an overall residual stress of ≤100 MPa throughout its pipe body.

### Claim 14 (depends on 2)

The bainite seamless steel pipe according to claim 2, wherein the bainite seamless steel pipe after being tempered at a temperature of 200-350° C. has the following performances in a tempered state: a yield strength of 650-860 MPa, a tensile strength of ≥980 MPa, a longitudinal impact toughness of ≥60 J, a yield ratio of 0.7-0.83.

### Claim 15 (depends on 2)

The bainite seamless steel pipe according to claim 2, wherein the bainite seamless steel pipe after being tempered at a temperature of 400-460° C. has the following performances in a tempered state: a yield strength of 650-860 MPa, a tensile strength of ≥980 MPa.

### Claim 16 (depends on 2)

The bainite seamless steel pipe according to claim 2, wherein the bainite seamless steel pipe is free of Mo, Ni, Nb, V and/or Ti; and/or, the bainite seamless steel pipe satisfies one or more of the following: Si content is in a range of 0.66-0.85%, preferably 0.75-0.85%; Mn content is in a range of 1.85-2%; Cr content is in a range of 0.9-1.1%; B content is in a range of 0.002-0.0045%; N content is in a range of 0.004-0.006%.

### Claim 17 (depends on 2)

The bainite seamless steel pipe according to claim 2, wherein the bainite seamless steel pipe has a bainite structure.

### Claim 18 (depends on 9)

The method according to claim 9, wherein the bainite seamless steel pipe comprises the following chemical elements in percentage by mass:
C: 0.16-0.18%, Si: 0.56-1%, Mn: 1.8-2.05%, Cr: 0.85-1.25%, Al: 0.015-0.04%, B: 0.001-0.005%, 0<N≤0.006%, the balance being Fe and inevitable impurities, wherein Al/N≥3.

### Claim 19 (depends on 9)

The method according to claim 9, wherein the inevitable impurities include S and P; wherein S≤0.01%, P≤0.005%.

### Claim 20 (depends on 9)

The method according to claim 9, wherein the bainite seamless steel pipe has the following performances in a rolled state: a yield strength of 552-758 MPa, a tensile strength of ≥980 MPa, a longitudinal impact toughness of ≥40 J, a yield ratio of 0.6-0.75, an elongation of 12-15%, a local residual stress of ≤200 MPa within a range of 1-2 mm in a wall thickness direction of its outer wall, an overall residual stress of ≤100 MPa throughout its pipe body.