# US 2026/0258515 A1 · A method of manufacturing molten pig iron into an electrical smelting furnace

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0258515 A1
- Document ID: US20260258515A1
- Status: Published application
- Kind: A1
- Application number: 18/994,724
- Filed: 2022-07-29
- Published: 2026-09-03
- Earliest claimed: 2022-07-29
- Applicants: ArcelorMittal
- Inventors: Jean-Christoph HUBER; Mathieu SANCHEZ; Eric Alain HESS
- Web page: https://patentgrep.com/patent/US20260258515A1

## CPC

- C21B 11/10: in electric furnaces
- C21B 13/0073: {Selection or treatment of the reducing gases}
- C21B 13/0086: {Conditioning, transformation of reduced iron ores}
- C21C 1/02: Dephosphorising or desulfurising
- C21C 5/28: Manufacture of steel in the converter {(C21C5/005 takes precedence)}
- C21C 7/064: Dephosphorising; Desulfurising
- C21B 13/12: in electric furnaces
- C21B 13/143: {Injection of partially reduced ore into a molten bath}
- C21B 2200/00: Recycling of non-gaseous waste material
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS

## Abstract

A method for manufacturing molten pig iron into an electrical smelting furnace, the method including the following successive steps: providing a directly reduced iron product, providing a carbon and iron containing material, feeding at least a part of the smelting furnace with the DRI product in alternance with the carbon and iron containing material, and melting the DRI Product and the carbon and iron containing material to produce molten pig iron. It also deals with the manufacturing of steel from the pig iron.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A method of manufacturing molten pig iron into an electrical smelting furnace, the method comprising the following successive steps:
providing a directly reduced iron product;
providing a carbon and iron-containing material;
feeding at least a part of the smelting furnace in alternance with the DRI product and with the carbon and iron-containing material; and
melting the DRI product and the carbon and iron-containing material to produce molten pig iron.

### Claim 15 (depends on 14)

The method according to claim 14 wherein the carbon and iron-containing material is injected in an amount sufficient to reach a final carbon content of 4.0 to 4.5% in weight in the molten pig iron.

### Claim 16 (depends on 14)

The method according to claim 14 wherein the carbon and iron-containing material is a mixture of a carbon source and an iron source.

### Claim 17 (depends on 16)

The method according to claim 16 wherein the carbon source is chosen from at least one of the group consisting of: coke, anthracite, silicon carbide, calcium carbide, biomass, carbon coming from the combustion of biomass and a mixture of any of those materials.

### Claim 18 (depends on 16)

The method according to claim 16 wherein the iron source is chosen from at least one of the group consisting of: ferro-silicon, iron fines, sinter dust, DRI Fines, shredded scrap, steelmaking slag, steelmaking dust, scale and steelmaking sludge.

### Claim 19 (depends on 14)

The method according to claim 14 wherein the carbon and iron-containing material is formed so that more than 50% of the external surface is made of iron material.

### Claim 20 (depends on 14)

The method according to claim 14 wherein the DRI product is provided at a temperature of 500 to 700° C.

### Claim 21 (depends on 14)

The method according to claim 14 wherein the DRI product is manufactured using a reducing gas containing at least 50 % in volume of hydrogen before being loaded in the smelting furnace.

### Claim 22 (depends on 14)

The method according to claim 14 wherein a silicon containing material is added to the carbon and iron-containing material to be fed into the smelting furnace.

### Claim 23 (depends on 14)

The method according to claim 14 wherein the carbon and iron-containing material and the DRI product are provided as briquettes, the briquettes having a same size.

### Claim 24 (depends on 14)

A method for manufacturing steel employing the method as recited in claim 14 comprising the steps of:
transferring the pig iron from the smelting furnace to a converter; and
lowering a carbon content of the pig iron to a value below 2.1 percent in weight by blowing oxygen to obtain liquid steel.

### Claim 25 (depends on 24)

The method for manufacturing steel according to claim 24 wherein ferrous scraps are added to the pig iron in the converter, the ferrous scraps being melted.

### Claim 26 (depends on 24)

A method for manufacturing steel according to claim 24 wherein the pig iron is being transferred from the smelting furnace to a desulphurization station before being transferred to the converter.