# US 2026/0258215 A1 · Polyamide Aerogel and Preparation Method Therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0258215 A1
- Document ID: US20260258215A1
- Status: Published application
- Kind: A1
- Application number: 19/066,991
- Filed: 2025-02-28
- Published: 2026-09-03
- Earliest claimed: 2025-02-28
- Assignees: Microvast Advanced Membranes Inc.
- Applicants: Microvast Advanced Membranes Inc.
- Inventors: Haipeng ZHANG; Jinbo HE; Jianzhao LIU; Wenjuan Liu MATTIS
- Web page: https://patentgrep.com/patent/US20260258215A1

## CPC

- C08J 9/283: {a discontinuous liquid phase emulsified in a continuous macromolecular phase}
- C08G 69/28: Preparatory processes
- C08G 69/32: from aromatic diamines and aromatic dicarboxylic acids with both amino and carboxylic groups aromatically bound
- C08G 69/48: Polymers modified by chemical after-treatment
- C08J 3/075: Macromolecular gels
- C08J 9/28: by elimination of a liquid phase from a macromolecular composition or article, e.g. drying of coagulum
- C08J 9/286: {the liquid phase being a solvent for the monomers but not for the resulting macromolecular composition, i.e. macroporous or macroreticular polymers}
- C08J 2201/0502: the liquid phase being organic
- C08J 2201/0504: the liquid phase being aqueous
- C08J 2205/026: Aerogel, i.e. a supercritically dried gel
- C08J 2377/06: Polyamides derived from polyamines and polycarboxylic acids (C08J2377/10 takes precedence)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Polyamide aerogel and preparation method therefor are provided. The polyamide aerogel is a porous material, a porosity of the polyamide aerogel is 90-99%, and a thermal conductivity of the polyamide aerogel is less than or equal to 0.048 W/(m·K). The polyamide aerogel of the present disclosure is a porous material. The polyamide aerogel with a high porosity provides more adsorption surface area and volume, such that more active sites may be provided to the polyamide aerogel, thereby improving the adsorption capacity and catalytic activity of a material, and thus, the polyamide aerogel is suitable for air purification, wastewater treatment, and as a catalyst carrier. An extremely low thermal conductivity (less than or equal to 0.048 W/(m·K)) facilitates insulation and heat preservation. Furthermore, the polyamide aerogel has a desirable structure and mechanical property and thus is more suitable for the fields of architecture, aerospace, and energy storage.

## Claims

### Claim 1

A polyamide aerogel, wherein the polyamide aerogel is a porous material, a porosity of the polyamide aerogel is 90%-99%, and a thermal conductivity of the polyamide aerogel is less than or equal to 0.048 W/(m·K).

### Claim 2 (depends on 1)

The polyamide aerogel according to claim 1, wherein a specific surface area of the polyamide aerogel is 200 m2/g-450 m2/g.

### Claim 3 (depends on 1)

The polyamide aerogel according to claim 1, wherein an average pore diameter of pores of the polyamide aerogel is 1 nm-10 nm; and/or a density of the polyamide aerogel is 1 mg/cm3-50 mg/cm3.

### Claim 4 (depends on 1)

A method for preparing the polyamide aerogel according to claim 1, comprising:
step S1, performing a complex reaction on a raw material comprising a polyamide slurry and a coordination crosslinking agent, to obtain a composite;
step S2, performing a gelation reaction on the composite and a gelation reagent, to obtain a gelation product;
step S3, performing a solvent displacement treatment on the gelation product, to obtain a polyamide wet gel; and
step S4, performing a drying treatment on the polyamide wet gel to obtain the polyamide aerogel.

### Claim 5 (depends on 4)

The preparation method according to claim 4, wherein in step S1, a mass ratio of polyamide in the polyamide slurry to the coordination crosslinking agent is 1:0.032-0.8.

### Claim 6 (depends on 4)

The preparation method according to claim 4, wherein polyamide in the polyamide slurry is aromatic polyamide, and/or the aromatic polyamide is selected from any one or more of poly(p-phenylene terephthamide), poly(m-phenylene isophthalamide), poly(p-benzamide), and polyphenylsulfone terephthalamide.

### Claim 7 (depends on 4)

The preparation method according to claim 4, wherein in step S1, a temperature of the complex reaction is 5° C.-60° C.; and/or a time for the complex reaction is 0.3 h-33 h.

### Claim 8 (depends on 4)

The preparation method according to claim 4, wherein the polyamide slurry comprises polyamide and a first solvent; and the first solvent is selected from any one or more of dimethyl sulfoxide, N,N-dimethylformamide, N,N-Dimethylacetamide, N,N-dimethylhexanamide, N-methylpyrrolidone, and triethyl phosphate.

### Claim 9 (depends on 8)

The preparation method according to claim 8, wherein a solid content of the polyamide slurry is 1%-10%, and/or a pH value of the polyamide slurry is 4-7.

### Claim 10 (depends on 4)

The preparation method according to claim 4, wherein in step S1, the coordination crosslinking agent comprises an inorganic copper salt and/or an inorganic nickel salt.

### Claim 11 (depends on 10)

The preparation method according to claim 10, wherein in step S1, the inorganic copper salt is selected from any one or more of copper chloride, copper fluoride, and copper bromide.

### Claim 12 (depends on 10)

The preparation method according to claim 10, wherein in step S1, the inorganic copper salt comprises an inorganic copper salt powder or an inorganic copper salt solution, the inorganic copper salt solution comprises an inorganic copper salt and a second solvent, and a mass ratio of the inorganic copper salt to the second solvent is 10-20:5-10.

### Claim 13 (depends on 10)

The preparation method according to claim 10, wherein in step S1, the inorganic nickel salt is selected from any one or more of nickel chloride, nickel fluoride, and nickel bromide.

### Claim 14 (depends on 4)

The preparation method according to claim 4, wherein in step S2, a temperature of the gelation reaction is 5° C.-60° C.; and/or a time for the gelation reaction is 3 h-30 h.

### Claim 15 (depends on 4)

The preparation method according to claim 4, wherein in step S2, the gelation reaction is performed under a condition of high-speed shear dispersion, and a rotary speed of high-speed shear dispersion is 50 rpm-5000 rpm.

### Claim 16 (depends on 4)

The preparation method according to claim 4, wherein in step S2, a solid content of the gelation product is 1%-10%.

### Claim 17 (depends on 4)

The preparation method according to claim 4, wherein in step S2, the gelation reagent is selected from any one or more of water, an aqueous solution containing 20 wt. %-50 wt. % of N,N-dimethylacetamide, hydrochloric acid, sulfuric acid, ethanol, ethylene glycol, glycerol, acetone, tetrahydrofuran, chloroform, dichloromethane, and glacial acetic acid.

### Claim 18 (depends on 4)

The preparation method according to claim 4, wherein in step S4, the drying treatment comprises performing vacuum freeze drying and/or vacuum drying on the polyamide wet gel; the vacuum freeze drying process comprises: performing temperature holding on the polyamide wet gel for 4 h-10 h at −40° C. to −20° C., and then under a vacuum condition, successively performing temperature holding for 4 h-10 h at −20° C. to −10° C., temperature holding for 4 h-10 h at −10° C. to 0° C., and temperature holding for 4 h-10 h at 0° C. to 10° C. on the polyamide wet gel, wherein the vacuum condition means that a gas pressure is less than 10 Pa.

### Claim 19 (depends on 18)

The preparation method according to claim 18, wherein the vacuum drying process comprises: drying the polyamide wet gel for 6 h-10 h at 50° C.-80° C. and the gas pressure less than 10 Pa.

### Claim 20 (depends on 6)

The preparation method according to claim 6, wherein the polyamide slurry is an aromatic polyamide slurry, the preparation method further comprises a process of preparing the aromatic polyamide slurry, and the preparation process comprises:
performing an amidation reaction on a raw material comprising aromatic diacyl chloride, aromatic diamine, and a fourth solvent, to obtain an aromatic amidation product;
performing a neutralization treatment on the aromatic amidation product by using an alkaline reagent, to obtain a neutralized product;
performing a dilution treatment on the neutralized product by using the fourth solvent, to obtain the aromatic polyamide slurry; or
dissolving polyamide in a fifth solvent to obtain the aromatic polyamide slurry.