# US 2026/0257241 A1 · Protective Film, Method For Manufacturing Protective Film, And Electronic Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0257241 A1
- Document ID: US20260257241A1
- Status: Published application
- Kind: A1
- Application number: 19/551,785
- Filed: 2026-02-27
- Published: 2026-09-03
- Earliest claimed: 2025-02-28
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., Ltd.
- Inventors: Jonghwan Cho
- Web page: https://patentgrep.com/patent/US20260257241A1

## CPC

- B05D 5/06: to obtain multicolour or other optical effects (B05D5/02 takes precedence)
- B05D 1/60: {Deposition of organic layers from vapour phase (vapour phase deposition in general C23C14/00, C23C16/00)}
- B05D 7/52: {Two layers}
- B29D 11/00788: {Producing optical films}
- G02B 1/111: using layers comprising organic materials
- G02B 1/14: Protective coatings, e.g. hard coatings
- G02B 5/223: {containing organic substances, e.g. dyes, inks or pigments}
- H04M 1/0214: {Foldable telephones, i.e. with body parts pivoting to an open position around an axis parallel to the plane they define in closed position (combined with translation movement H04M1/0235)}
- H04M 1/0268: {including a flexible display panel}
- B05D 2320/00: Organic additives
- B05D 2506/10: Fluorinated polymers
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- H04M: TELEPHONIC COMMUNICATION (circuits for controlling other apparatus via a telephone cable and not involving telephone switching apparatus G08)

## Abstract

A protective film may include a base layer, a hard coating layer disposed on the base layer, and an anti-reflective layer disposed on the hard coating layer. The hard coating layer or the anti-reflective layer may include a blue-light absorber, thereby providing a low reflective characteristic and also a blue-light blocking characteristic. An electronic device may include the protective film.

## Claims

### Claim 1

A protective film comprising:
a base layer;
a hard coating layer disposed on the base layer; and
an anti-reflective layer disposed on the hard coating layer,
wherein the hard coating layer or the anti-reflective layer comprises at least one blue-light absorber comprising a benzoxazole-based compound, a phenyltriazine-based compound, or a naphthalimide-based compound.

### Claim 2 (depends on 1)

The protective film of claim 1, wherein the anti-reflective layer comprises the blue-light absorber and a fluorine-based acrylate compound.

### Claim 3 (depends on 2)

The protective film of claim 2, wherein the fluorine-based acrylate compound comprises a polymer represented by Formula 1:
wherein, in Formula 1, R1 and R2 are each independently a hydrogen atom or a binding site to a neighboring atom, and
n is an integer of 1 to 8.

### Claim 4 (depends on 3)

The protective film of claim 3, wherein n in Formula 1 is 8.

### Claim 5 (depends on 2)

The protective film of claim 2, wherein the anti-reflective layer comprises:
about 0.2 wt % to about 2 wt % of the blue-light absorber; and
about 98 wt % to about 99.8 wt % of the fluorine-based acrylate compound, based on a total weight of the blue light absorber and the fluorine-based acrylate compound.

### Claim 6 (depends on 1)

The protective film of claim 1, wherein the hard coating layer comprises the blue-light absorber.

### Claim 7 (depends on 1)

The protective film of claim 1, wherein the at least one blue-light absorber comprises the benzoxazole-based compound and the benzoxazole-based compound comprises 2,5-Bis(5-tert-butyl-2-benzoxazolyl)thiophene.

### Claim 8 (depends on 1)

The protective film of claim 1, wherein the at least one blue-light absorber comprises the phenyltriazine-based compound, and the phenyltriazine-based compound comprises at least one of 2-(2-Hydroxyphenyl)-1,3,5-triazine-4,6-diamine or 2,4,6-Tris(4-butoxy-2-hydroxyphenyl)-1,3,5-triazine.

### Claim 9 (depends on 1)

The protective film of claim 1, wherein the at least one blue-light absorber comprises the naphthalimide-based compound, and the naphthalimide-based compound comprises at least one of N-Hydroxy-1,8-naphthalimide or N-(Trifluoromethylsulfonyloxy)-1,8-naphthalimide.

### Claim 10 (depends on 1)

The protective film of claim 1, wherein a thickness of the anti-reflective layer is about 90 nm to about 110 nm.

### Claim 11 (depends on 1)

The protective film of claim 1, wherein the anti-reflective layer is formed by a vapor deposition polymerization method.

### Claim 12

A method for manufacturing a protective film, the method comprising:
providing a hard coating layer-forming material on a base layer to form a hard coating layer; and
providing an anti-reflective layer-forming material on the hard coating layer to form an anti-reflective layer,
wherein the hard coating layer-forming material or the anti-reflective layer-forming material comprises at least one blue-light absorber comprising a benzoxazole-based compound, a phenyltriazine-based compound, or a naphthalimide-based compound.

### Claim 13 (depends on 12)

The method of claim 12, wherein the forming of the anti-reflective layer is performed in a vacuum chamber, and
the anti-reflective layer-forming material comprises the blue-light absorber and a fluorine-based acrylate compound.

### Claim 14 (depends on 13)

The method of claim 13, wherein the forming of the anti-reflective layer comprises polymerizing the fluorine-based acrylate compound to form a polymerized fluorine-based acrylate compound and simultaneously depositing the polymerized fluorine-based acrylate compound and the blue-light absorber on the hard coating layer.

### Claim 15 (depends on 13)

The method of claim 13, wherein the blue-light absorber and the fluorine-based acrylate compound are provided at an ion acceleration voltage of about 100 V to about 500 V.

### Claim 16 (depends on 12)

The method of claim 12, wherein the forming of the anti-reflective layer is performed at a temperature of about −30° C. to about 10° C.

### Claim 17

An electronic device comprising:
a display module comprising a first non-folding area, a second non-folding area, and a folding area between the first non-folding area and the second non-folding area; and
a window module disposed on the display module, the window module comprising a window glass and a protective film which are stacked in sequence,
wherein the protective film comprises:
a base layer;
a hard coating layer disposed on the base layer; and
an anti-reflective layer disposed on the hard coating layer,
wherein the hard coating layer or the anti-reflective layer comprises at least one blue-light absorber comprising a benzoxazole-based compound, a phenyltriazine-based compound, or a naphthalimide-based compound.

### Claim 18 (depends on 17)

The electronic device of claim 17, further comprising at least one of a processor, a memory, or a power module.

### Claim 19 (depends on 17)

The electronic device of claim 17, wherein the hard coating layer does not comprise the blue-light absorber, and
the anti-reflective layer comprises the blue-light absorber and a fluorine-based acrylate compound.

### Claim 20 (depends on 17)

The electronic device of claim 17, wherein the blue-light absorber comprises at least one compound of Compound Group 1: