# US 2026/0255878 A1 · Methods of forming group iii piezoelectric thin films via removal of portions of first sputtered material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0255878 A1
- Document ID: US20260255878A1
- Status: Published application
- Kind: A1
- Application number: 19/642,356
- Filed: 2026-04-08
- Published: 2026-08-27
- Earliest claimed: 2017-10-16
- Assignees: Akoustis Technologies Corp.
- Applicants: Akoustis Technologies Corp.
- Inventors: Craig Moe; Jeffrey B. Shealy; Mary Winters; Dae Ho Kim; Abhay Saranswarup Kochhar
- Web page: https://patentgrep.com/patent/US20260255878A1

## CPC

- H03H 9/173: {Air-gaps}
- H10N 30/076: by vapour phase deposition
- H03H 3/02: for the manufacture of piezoelectric or electrostrictive resonators or networks (H03H3/08 takes precedence)
- H03H 9/02031: {consisting of ceramic}
- H03H 9/105: {the enclosure being defined by a cover cap mounted on an element forming part of the BAW device}
- H03H 9/174: {Membranes}
- H03H 9/175: {Acoustic mirrors}
- H10N 30/053: by integrally sintering piezoelectric or electrostrictive bodies and electrodes
- H10N 30/06: Forming electrodes or interconnections, e.g. leads or terminals
- H03H 2003/021: {the resonators or networks being of the air-gap type}
- H03H 2003/023: {the resonators or networks being of the membrane type}
- H03H 2003/025: {the resonators or networks comprising an acoustic mirror}
- Y10T 29/42: Piezoelectric device making
- Y10T 29/49005: Acoustic transducer
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of forming a piezoelectric thin film includes sputtering a first surface of a substrate to provide a piezoelectric thin film comprising AlN, AlScN, AlCrN, HfMgAlN, or ZrMgAlN thereon, processing a second surface of the substrate that is opposite the first surface of the substrate to provide an exposed surface of the piezoelectric thin film from beneath the second surface of the substrate, wherein the exposed surface of the piezoelectric thin film includes a first crystalline quality portion, removing a portion of the exposed surface of the piezoelectric thin film to access a second crystalline quality portion that is covered by the first crystalline quality portion, wherein the second crystalline quality portion has a higher quality than the first crystalline quality portion and processing the second crystalline quality portion to provide an acoustic resonator device on the second crystalline quality portion.

## Claims

### Claim 1

A method of forming a piezoelectric thin film, the method comprising:
providing an inert gas and a nitrogen process gas to a process chamber including a substrate and a target comprising one or more Group III elements;
sputtering the one or more Group III elements from the target onto a first surface of the substrate to provide the piezoelectric thin film including a nitride of the one or more Group III elements on the first surface of the substrate;
forming a first electrode on the piezoelectric thin film;
forming a support layer on the first electrode to have a recess therein providing access to the first electrode;
coupling a bond substrate to the support layer to form a cavity between the first electrode and the bond substrate;
processing a second surface of the substrate that is opposite the first surface of the substrate to provide an exposed surface of the piezoelectric thin film from beneath the second surface of the substrate, wherein the exposed surface of the piezoelectric thin film comprises a first crystalline quality portion of the piezoelectric thin film;
removing a portion of the exposed surface of the piezoelectric thin film to access a second crystalline quality portion of the piezoelectric thin film that is covered by the first crystalline quality portion of the piezoelectric thin film, wherein the second crystalline quality portion of the piezoelectric thin film has a higher quality than the first crystalline quality portion of the piezoelectric thin film; and
processing the second crystalline quality portion of the piezoelectric thin film to provide an acoustic resonator device on the second crystalline quality portion of the piezoelectric thin film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the piezoelectric thin film comprises AlN, AlScN, AlCrN, HfMgAlN, or ZrMgAlN.

### Claim 3 (depends on 2)

The method of claim 2, wherein processing the second crystalline quality portion of the piezoelectric thin film comprises forming an opening in the second crystalline quality portion of the piezoelectric thin film exposed by removal of about 500 Angstroms of the piezoelectric thin film to expose the first electrode.

### Claim 4 (depends on 1)

The method of claim 1, wherein sputtering the one or more Group III elements from the target onto the first surface of the substrate comprises heating the substrate to a temperature in a range between about 350 degrees Centigrade to about 850 degrees Centigrade.

### Claim 5 (depends on 1)

The method of claim 1, wherein sputtering the one or more Group III elements from the target onto the first surface of the substrate comprises heating the substrate to a temperature in a range between about 400 degrees Centigrade to about 600 degrees Centigrade.

### Claim 6 (depends on 1)

The method of claim 1, wherein sputtering the one or more Group III elements from the target onto the first surface of the substrate comprises sputtering a seed layer directly including the one or more Group III elements onto the first surface of the substrate to form a nucleation layer prior to formation of the piezoelectric thin film.

### Claim 7 (depends on 6)

The method of claim 6, further comprising:
sputtering the one or more Group III elements onto the nucleation layer to form the piezoelectric thin film.

### Claim 8 (depends on 2)

The method of claim 2, wherein the second crystalline quality portion of the piezoelectric thin film has a crystallinity of less than about 1.0 degree at Full Width Half Maximum (FWHM) to about 10 arcseconds at FWHM measured using X-ray diffraction (XRD).

### Claim 9 (depends on 8)

The method of claim 8, wherein the second crystalline quality portion of the piezoelectric thin film has a crystallinity in a range between about 1.0 degree at FWHM to about 0.5 degrees at FWHM measured using XRD.