# US 2026/0255622 A1 · Schottky diode and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0255622 A1
- Document ID: US20260255622A1
- Status: Published application
- Kind: A1
- Application number: 19/059,884
- Filed: 2025-02-21
- Published: 2026-08-27
- Earliest claimed: 2025-02-21
- Assignees: ProAsia Semiconductor Corporation
- Applicants: ProAsia Semiconductor Corporation
- Inventors: Ming-Chi Kuo; I-Tai Li
- Web page: https://patentgrep.com/patent/US20260255622A1

## CPC

- H10D 8/60: Schottky-barrier diodes
- H10D 8/051: {of Schottky diodes}
- H10D 62/054: {by high energy implantations in bulk semiconductor bodies, e.g. forming pillars}
- H10D 62/111: {Multiple RESURF structures, e.g. double RESURF or 3D-RESURF structures}
- H10D 62/8325: {Silicon carbide}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A Schottky diode and a manufacturing method thereof are provided. The Schottky diode comprises a substrate, a first conductive type epitaxial layer, a plurality of trench structures, a plurality of second conductive type heavily-doped barrier regions and a plurality of second conductive type doped regions. The first conductive type epitaxial layer is disposed on the substrate, and a plurality of trench structures are disposed in the first conductive type epitaxial layer. Each of the second conductivity type heavily-doped barrier regions are correspondingly disposed at the bottom of each trench structure, and each of the second conductivity type doping regions are correspondingly disposed on the side walls of each trench structure, so that a plurality of super junctions are formed between each second conductivity type doped region and the first conductivity type epitaxial layer between each trench structure.

## Claims

### Claim 1

A Schottky diode, comprising:
a substrate;
a first conductive type epitaxial layer, disposed on the substrate;
a plurality of trench structures, disposed in the first conductive type epitaxial layer;
a plurality of second conductive type heavily-doped barrier regions, correspondingly disposed at the bottom of each of the trench structures; and
a plurality of second conductive type doped regions, correspondingly disposed on the side walls of each of the trench structures, so that a plurality of super junctions are formed between each of the second conductivity type doped regions and the first conductivity type epitaxial layer between each of the trench structures.

### Claim 2 (depends on 1)

The Schottky diode of claim 1, wherein each of the second conductive type doped regions has aluminum doping with a doping concentration of 1~10E18 (cm−3).

### Claim 3 (depends on 1)

The Schottky diode of claim 1, wherein each of the second conductive type heavily-doped barrier regions has aluminum doping with a doping concentration of 1E18~5E19 (cm−3).

### Claim 4 (depends on 1)

The Schottky diode of claim 1, wherein the substrate is a first conductive type heavily-doped silicon carbide substrate.

### Claim 5 (depends on 1)

The Schottky diode of claim 1, further comprising an anode metal covering the first conductive type epitaxial layer and each of the trench structures so that Schottky contact is formed between the anode metal and the first conductive type epitaxial layer, and ohmic contact is formed between the anode metal and each of the second conductive type heavily-doped barrier regions and each of the second conductive type doped regions.

### Claim 6 (depends on 5)

The Schottky diode of claim 5, wherein the anode metal is selected from one of the group consisting of aluminum, chromium, gold, platinum, titanium, cobalt and nickel and combinations thereof.

### Claim 7

A manufacturing method of a Schottky diode, comprising:
providing a first conductive type epitaxial layer, disposed on a substrate;
providing a plurality of trench structures, disposed in the first conductive type epitaxial layer;
providing a plurality of second conductive type heavily-doped barrier regions, correspondingly disposed at the bottom of each of the trench structures; and
providing a plurality of second conductive type doped regions, correspondingly disposed on the side walls of each of the trench structures, so that a plurality of super junctions are formed between each of the second conductivity type doped regions and the first conductivity type epitaxial layer between each of the trench structures.

### Claim 8 (depends on 7)

The manufacturing method of a Schottky diode of claim 7, wherein the step of providing a first conductive type epitaxial layer is to implant nitrogen (N) or phosphorus (P) with a doping concentration of 1E14~1E16 (cm−3) after providing a silicon carbide epitaxial layer on the substrate.

### Claim 9 (depends on 7)

The manufacturing method of a Schottky diode of claim 7, wherein the step of providing a plurality of trench structures is to remove a portion of the first conductive type epitaxial layer by using a patterned mask disposed on the first conductive type epitaxial layer.

### Claim 10 (depends on 9)

The manufacturing method of a Schottky diode of claim 9, wherein the step of providing a plurality of second conductive type heavily-doped barrier regions is to use the patterned mask to perform ion implantation on the bottom of each of the trench structures by implanting aluminum with a doping concentration of 1E18~5E19 (cm−3).

### Claim 11 (depends on 9)

The manufacturing method of a Schottky diode of claim 9, wherein the step of providing a plurality of second conductive type doped regions is to use the patterned mask to perform tilt ion implantation to the side walls of each of the trench structures by implanting aluminum with an ion implantation dose of 1~10E13 (cm−2) and an ion implantation energy of 20~100 (keV).

### Claim 12 (depends on 11)

The manufacturing method of a Schottky diode of claim 11, wherein the tilt ion implantation is to implant ions with an implantation tilt angle of 30°~45° between a vertical normal.

### Claim 13 (depends on 7)

The manufacturing method of a Schottky diode of claim 7, further comprising a step of providing an anode metal covering the first conductive type epitaxial layer and each of the trench structures so that Schottky contact is formed between the anode metal and the first conductive type epitaxial layer, and ohmic contact is formed between the anode metal and each of the second conductive type heavily-doped barrier regions and each of the second conductive type doped regions.

### Claim 14 (depends on 13)

The manufacturing method of a Schottky diode of claim 13, wherein the step of providing an anode metal is to provide a material selected from one of the group consisting of aluminum, chromium, gold, platinum, titanium, cobalt and nickel and combinations thereof.