# US 2026/0253947 A1 · Lithium ion conductive glass material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0253947 A1
- Document ID: US20260253947A1
- Status: Published application
- Kind: A1
- Application number: 18/875,916
- Filed: 2023-06-15
- Published: 2026-08-27
- Earliest claimed: 2022-06-21
- Assignees: Ohara Inc.
- Applicants: Ohara Inc.
- Inventors: Kazuhito Ogasa; Chie Yamaguchi
- Web page: https://patentgrep.com/patent/US20260253947A1

## CPC

- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0562: Solid materials
- C01B 25/45: containing plural metal, or metal and ammonium
- C03C 3/17: containing aluminium or beryllium
- C03C 4/18: for ion-sensitive glass
- C03C 10/00: Devitrified glass ceramics, i.e. glass ceramics having a crystalline phase dispersed in a glassy phase and constituting at least 50% by weight of the total composition
- H01B 1/06: mainly consisting of other non-metallic substances
- H01B 1/08: oxides
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 2300/0068: inorganic
- H01M 2300/0071: Oxides
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

There is provided a lithium ion conductive glass material from which a solid electrolyte having both a high density and a high lithium ion conductivity can be formed by mixing and sintering with a lithium ion conductive material at 700° C. or lower. Then, the above problem is solved by a lithium ion conductive glass material containing, in mole percent on an oxide basis, 43.5 to 49.0% of a P2O5 component, 0.5 to 4.0% of an Al2O3 component, and 47.0 to 55.0% of a Li2O component.

## Claims

### Claim 1

A lithium ion conductive glass material comprising, in mole percent on an oxide basis,
43.5 to 49.0% of a P2O5 component,
0.5 to 4.0% of an Al2O3 component, and
47.0 to 55.0% of a Li2O component.

### Claim 2 (depends on 1)

The lithium ion conductive glass material according to claim 1, satisfying at least two or more selected from the group consisting of (1), (2), and (3) below, and having a lithium ion conductivity of not less than 5.0×10−9 S/cm and not more than 5.0×10−8 S/cm at 25° C. in a vitreous state:
(1) a crystallization temperature (Te) is equal to or higher than 400° C. and equal to or lower than 460° C.;
(2) a glass transition point (Tg) is equal to or higher than 330° C. and equal to or lower than 365° C.; and
(3) a melt initiation temperature (mp) is equal to or higher than 560° C. and equal to or lower than 590° C.

### Claim 3 (depends on 1)

The lithium ion conductive glass material according to claim 1, which is a sintering auxiliary used for mixing and sintering with a lithium ion conductive material comprising a crystal phase with a rhombohedral NASICON structure, a crystal phase of Li1+xAlxTi2−xP3O12 (0.7>x≥0.05), or a crystal phase of Li1+x+yAlxTi2−xSiyP3−yO12 (0.7>x≥0.05, 0.5>y≥0), and is a powder with a maximum particle size of 200 μm or less and an average particle size (D50) of 100 μm or less.

### Claim 4 (depends on 1)

A solid electrolyte material formed by mixing the lithium ion conductive glass material according to claim 1 and a lithium ion conductive material comprising a crystal phase with a rhombohedral NASICON structure, a crystal phase of Li1+xAlxTi2−xP3O12 (0.7>x≥0.05), or a crystal phase of Li1+x+yAlxTi2−zSiyP3−yO12 (0.7>x≥0.05, 0.5>y≥0).

### Claim 5 (depends on 4)

An all-solid-state secondary battery, comprising a member integrally molded by sintering materials including the solid electrolyte material according to claim 4, and a positive electrode material or negative electrode material.

### Claim 6 (depends on 1)

An electrode active material comprising a covering glass layer formed by performing a covering treatment with the lithium ion conductive glass material according to claim 1 on a surface, wherein a coverage ratio of the covering glass layer on this surface is 18% or more.

### Claim 7 (depends on 6)

A lithium ion secondary battery comprising the electrode active material according to claim 6.

### Claim 8 (depends on 2)

The lithium ion conductive glass material according to claim 2, which is a sintering auxiliary used for mixing and sintering with a lithium ion conductive material comprising a crystal phase with a rhombohedral NASICON structure, a crystal phase of Li1+xAlxTi2−xP3O12 (0.7>x≥0.05), or a crystal phase of Li1+x+yAlxTi2−xSiyP3−yO12 (0.7>x≥0.05, 0.5>y≥0), and is a powder with a maximum particle size of 200 μm or less and an average particle size (D50) of 100 μm or less.

### Claim 9 (depends on 2)

A solid electrolyte material formed by mixing the lithium ion conductive glass material according to claim 2 and a lithium ion conductive material comprising a crystal phase with a rhombohedral NASICON structure, a crystal phase of Li1+xAlxTi2−xP3O12 (0.7>x≥0.05), or a crystal phase of Li1+x+yAlxTi2−xSiyP3−yO12 (0.7>x≥0.05, 0.5>y≥0).

### Claim 10 (depends on 9)

An all-solid-state secondary battery, comprising a member integrally molded by sintering materials including the solid electrolyte material according to claim 9, and a positive electrode material or negative electrode material.

### Claim 11 (depends on 2)

An electrode active material comprising a covering glass layer formed by performing a covering treatment with the lithium ion conductive glass material according to claim 2 on a surface, wherein a coverage ratio of the covering glass layer on this surface is 18% or more.

### Claim 12 (depends on 11)

A lithium ion secondary battery comprising the electrode active material according to claim 11.